- Prior art keywords
- lead
- weight
- brass
- low
- alloy
- Prior art date
Links
Landscapes
- Domestic Plumbing Installations (AREA)
- Conductive Materials (AREA)
Priority Applications (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW098128163A TWI392752B (zh) | 2009-08-21 | 2009-08-21 | 低鉛銅合金 |
CA 2680214 CA2680214C (fr) | 2009-08-21 | 2009-09-29 | Alliage de cuivre a basse teneur en plomb |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW098128163A TWI392752B (zh) | 2009-08-21 | 2009-08-21 | 低鉛銅合金 |
Publications (2)
Publication Number | Publication Date |
---|---|
TW201107501A TW201107501A (en) | 2011-03-01 |
TWI392752B true TWI392752B (zh) | 2013-04-11 |
Family
ID=43618918
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW098128163A TWI392752B (zh) | 2009-08-21 | 2009-08-21 | 低鉛銅合金 |
Country Status (2)
Country | Link |
---|---|
CA (1) | CA2680214C (fr) |
TW (1) | TWI392752B (fr) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2013065830A1 (fr) | 2011-11-04 | 2013-05-10 | 三菱伸銅株式会社 | Article en alliage de cuivre forgé à chaud |
TWI740299B (zh) | 2019-06-25 | 2021-09-21 | 日商三菱綜合材料股份有限公司 | 快削性銅合金及快削性銅合金的製造方法 |
TWI751825B (zh) * | 2019-12-11 | 2022-01-01 | 日商三菱綜合材料股份有限公司 | 快削性銅合金及快削性銅合金的製造方法 |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
TWI577931B (zh) * | 2015-05-28 | 2017-04-11 | 建準電機工業股份有限公司 | 具有發光模組之吊扇馬達 |
-
2009
- 2009-08-21 TW TW098128163A patent/TWI392752B/zh not_active IP Right Cessation
- 2009-09-29 CA CA 2680214 patent/CA2680214C/fr not_active Expired - Fee Related
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
TWI577931B (zh) * | 2015-05-28 | 2017-04-11 | 建準電機工業股份有限公司 | 具有發光模組之吊扇馬達 |
Also Published As
Publication number | Publication date |
---|---|
TW201107501A (en) | 2011-03-01 |
CA2680214C (fr) | 2012-04-24 |
CA2680214A1 (fr) | 2011-02-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP6335194B2 (ja) | 良好な熱成形性を有する、無鉛の、切断が容易な、耐腐食性真鍮合金 | |
TWI550106B (zh) | Low lead free bismuth no silicon brass alloy | |
WO2019007309A1 (fr) | Alliage de laiton écologique pour coulage et son procédé de fabrication | |
US20110064602A1 (en) | Dezincification-resistant copper alloy | |
TWI392752B (zh) | 低鉛銅合金 | |
AU2014202540B2 (en) | Lead-free bismuth-free silicon-free brass | |
TWI387656B (zh) | Preparation of Low Lead Brass Alloy and Its | |
TWI390057B (zh) | 低鉛抗脫鋅銅合金 | |
TWI398531B (zh) | 抗脫鋅銅合金及其物件之製法 | |
US20110142715A1 (en) | Brass alloy | |
TWI398532B (zh) | Lead-free brass alloy | |
CA2687452C (fr) | Alliage de laiton | |
TWI392751B (zh) | 低鉛銅合金 | |
US20110081271A1 (en) | Low-lead copper alloy | |
US8349097B2 (en) | Dezincification-resistant copper alloy and method for producing product comprising the same | |
TWI485271B (zh) | Low shrinkage corrosion resistant brass alloy | |
CN103205597A (zh) | 无铅的锑镍黄铜合金 | |
CA2718613A1 (fr) | Alliage de bronze resistant a la dezincification | |
CA2675525C (fr) | Procede de fabrication d'alliage de cuivre et de faible titrage de plomb, et produit ainsi constitue | |
JP2005248303A (ja) | 無鉛快削青銅鋳物及び無鉛快削青銅物品の製造方法 | |
CN101994025A (zh) | 低铅的铜合金 | |
US20110081272A1 (en) | Low-lead copper alloy | |
TW201309816A (zh) | 環保黃銅合金 | |
TW201213563A (en) | Dezincification-resistant brass alloy |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MM4A | Annulment or lapse of patent due to non-payment of fees |