TW201335092A - 在離子交換製程中於玻璃產生恆定壓縮應力之方法 - Google Patents
在離子交換製程中於玻璃產生恆定壓縮應力之方法 Download PDFInfo
- Publication number
- TW201335092A TW201335092A TW102103926A TW102103926A TW201335092A TW 201335092 A TW201335092 A TW 201335092A TW 102103926 A TW102103926 A TW 102103926A TW 102103926 A TW102103926 A TW 102103926A TW 201335092 A TW201335092 A TW 201335092A
- Authority
- TW
- Taiwan
- Prior art keywords
- glass
- bath
- temperature
- time
- compressive stress
- Prior art date
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C21/00—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
- C03C21/001—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface in liquid phase, e.g. molten salts, solutions
- C03C21/002—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface in liquid phase, e.g. molten salts, solutions to perform ion-exchange between alkali ions
Landscapes
- Chemical & Material Sciences (AREA)
- Life Sciences & Earth Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- General Chemical & Material Sciences (AREA)
- Geochemistry & Mineralogy (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Surface Treatment Of Glass (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US13/363,567 US20120216565A1 (en) | 2011-02-24 | 2012-02-01 | Method of producing constancy of compressive stress in glass in an ion exchange process |
Publications (1)
Publication Number | Publication Date |
---|---|
TW201335092A true TW201335092A (zh) | 2013-09-01 |
Family
ID=47714580
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW102103926A TW201335092A (zh) | 2012-02-01 | 2013-02-01 | 在離子交換製程中於玻璃產生恆定壓縮應力之方法 |
Country Status (2)
Country | Link |
---|---|
TW (1) | TW201335092A (fr) |
WO (1) | WO2013116420A1 (fr) |
Cited By (13)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US11021393B2 (en) | 2014-11-04 | 2021-06-01 | Corning Incorporated | Deep non-frangible stress profiles and methods of making |
US11079309B2 (en) | 2013-07-26 | 2021-08-03 | Corning Incorporated | Strengthened glass articles having improved survivability |
US11084756B2 (en) | 2014-10-31 | 2021-08-10 | Corning Incorporated | Strengthened glass with ultra deep depth of compression |
US11174197B2 (en) | 2016-04-08 | 2021-11-16 | Corning Incorporated | Glass-based articles including a metal oxide concentration gradient |
US11220456B2 (en) | 2014-10-08 | 2022-01-11 | Corning Incorporated | Glasses and glass ceramics including a metal oxide concentration gradient |
US11267228B2 (en) | 2015-07-21 | 2022-03-08 | Corning Incorporated | Glass articles exhibiting improved fracture performance |
US11472734B2 (en) | 2015-12-11 | 2022-10-18 | Corning Incorporated | Fusion-formable glass-based articles including a metal oxide concentration gradient |
US11492291B2 (en) | 2012-02-29 | 2022-11-08 | Corning Incorporated | Ion exchanged glasses via non-error function compressive stress profiles |
US11613103B2 (en) | 2015-07-21 | 2023-03-28 | Corning Incorporated | Glass articles exhibiting improved fracture performance |
US11634359B2 (en) | 2014-02-24 | 2023-04-25 | Corning Incorporated | Strengthened glass with deep depth of compression |
US11724965B2 (en) | 2018-01-24 | 2023-08-15 | Corning Incorporated | Glass-based articles having high stress magnitude at depth |
US11878941B2 (en) | 2014-06-19 | 2024-01-23 | Corning Incorporated | Glasses having non-frangible stress profiles |
US11963320B2 (en) | 2016-04-08 | 2024-04-16 | Corning Incorporated | Glass-based articles including a stress profile comprising two regions |
Families Citing this family (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US9302937B2 (en) | 2010-05-14 | 2016-04-05 | Corning Incorporated | Damage-resistant glass articles and method |
TWI572480B (zh) | 2011-07-25 | 2017-03-01 | 康寧公司 | 經層壓及離子交換之強化玻璃疊層 |
EP3204337B1 (fr) | 2014-10-07 | 2020-04-22 | Corning Incorporated | Article en verre à profil de contraintes déterminé et son procédé de production |
EP3362417A1 (fr) | 2015-10-14 | 2018-08-22 | Corning Incorporated | Article en verre stratifié à profil de contraintes déterminé et son procédé de production |
Family Cites Families (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3637453A (en) * | 1966-06-17 | 1972-01-25 | Owens Illinois Inc | Glass-ceramic articles having an integral compressive stress surface layer |
JPS5417765B1 (fr) | 1971-04-26 | 1979-07-03 | ||
US8341976B2 (en) * | 2009-02-19 | 2013-01-01 | Corning Incorporated | Method of separating strengthened glass |
US8802581B2 (en) * | 2009-08-21 | 2014-08-12 | Corning Incorporated | Zircon compatible glasses for down draw |
WO2011149694A1 (fr) * | 2010-05-26 | 2011-12-01 | Corning Incorporated | Échange d'ions de verre à revêtement antireflet ar et procédé associé |
-
2013
- 2013-01-31 WO PCT/US2013/023980 patent/WO2013116420A1/fr active Application Filing
- 2013-02-01 TW TW102103926A patent/TW201335092A/zh unknown
Cited By (20)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US11492291B2 (en) | 2012-02-29 | 2022-11-08 | Corning Incorporated | Ion exchanged glasses via non-error function compressive stress profiles |
US11079309B2 (en) | 2013-07-26 | 2021-08-03 | Corning Incorporated | Strengthened glass articles having improved survivability |
US11634359B2 (en) | 2014-02-24 | 2023-04-25 | Corning Incorporated | Strengthened glass with deep depth of compression |
US11878941B2 (en) | 2014-06-19 | 2024-01-23 | Corning Incorporated | Glasses having non-frangible stress profiles |
US11465937B2 (en) | 2014-10-08 | 2022-10-11 | Corning Incorporated | Glasses and glass ceramics including a metal oxide concentration gradient |
US11459270B2 (en) | 2014-10-08 | 2022-10-04 | Corning Incorporated | Glasses and glass ceramics including a metal oxide concentration gradient |
US11220456B2 (en) | 2014-10-08 | 2022-01-11 | Corning Incorporated | Glasses and glass ceramics including a metal oxide concentration gradient |
US11746046B2 (en) | 2014-10-31 | 2023-09-05 | Corning Incorporated | Strengthened glass with ultra deep depth of compression |
US11084756B2 (en) | 2014-10-31 | 2021-08-10 | Corning Incorporated | Strengthened glass with ultra deep depth of compression |
US11377388B2 (en) | 2014-11-04 | 2022-07-05 | Corning Incorporated | Deep non-frangible stress profiles and methods of making |
US11021393B2 (en) | 2014-11-04 | 2021-06-01 | Corning Incorporated | Deep non-frangible stress profiles and methods of making |
US11267228B2 (en) | 2015-07-21 | 2022-03-08 | Corning Incorporated | Glass articles exhibiting improved fracture performance |
US11613103B2 (en) | 2015-07-21 | 2023-03-28 | Corning Incorporated | Glass articles exhibiting improved fracture performance |
US11472734B2 (en) | 2015-12-11 | 2022-10-18 | Corning Incorporated | Fusion-formable glass-based articles including a metal oxide concentration gradient |
US11878936B2 (en) | 2015-12-11 | 2024-01-23 | Corning Incorporated | Fusion-formable glass-based articles including a metal oxide concentration gradient |
US11691913B2 (en) | 2016-04-08 | 2023-07-04 | Corning Incorporated | Glass-based articles including a metal oxide concentration gradient |
US11279652B2 (en) | 2016-04-08 | 2022-03-22 | Corning Incorporated | Glass-based articles including a metal oxide concentration gradient |
US11174197B2 (en) | 2016-04-08 | 2021-11-16 | Corning Incorporated | Glass-based articles including a metal oxide concentration gradient |
US11963320B2 (en) | 2016-04-08 | 2024-04-16 | Corning Incorporated | Glass-based articles including a stress profile comprising two regions |
US11724965B2 (en) | 2018-01-24 | 2023-08-15 | Corning Incorporated | Glass-based articles having high stress magnitude at depth |
Also Published As
Publication number | Publication date |
---|---|
WO2013116420A1 (fr) | 2013-08-08 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
TW201335092A (zh) | 在離子交換製程中於玻璃產生恆定壓縮應力之方法 | |
US20120216569A1 (en) | Method of producing constancy of compressive stress in glass in an ion-exchange process | |
US20120216565A1 (en) | Method of producing constancy of compressive stress in glass in an ion exchange process | |
JP7327533B2 (ja) | 化学強化用ガラス、化学強化ガラスおよび化学強化ガラスの製造方法 | |
EP3071526B1 (fr) | Verres échangeurs d'ions et à résistance élevée à l'endommagement | |
TWI820462B (zh) | 強化玻璃 | |
US10315949B2 (en) | Fast ion-exchangeable boron-free glasses with low softening point | |
US4042405A (en) | High strength ophthalmic lens | |
US20140345325A1 (en) | Double ion exchange process | |
JP7009593B2 (ja) | ガラス物品を熱処理する方法 | |
DE202017007020U1 (de) | Artikel auf Glasbasis mit einem Metalloxid-Konzentrationsgradienten | |
JP5229966B2 (ja) | 偏光ガラスの製造方法 | |
EP3330234B1 (fr) | Verres d'aluminosilicate contenant du lithium | |
DE1421842B2 (de) | Verfestigter glasgegenstand aus einem alkali aluminium silikatglas und verfahren zu seiner herstellung | |
US20070141350A1 (en) | Visible light optical polarizer made from stretched H2-treated glass and method of making same | |
WO2020092122A1 (fr) | Procédés et systèmes de renforcement chimique de verre contenant du lithium | |
JPH0676224B2 (ja) | 強化ガラスの製造法 | |
JP2021504291A (ja) | ガラス物品のイオン交換方法 | |
KR102562798B1 (ko) | 3-차원 형상을 위한 이온교환 가능한 연질 유리 | |
CN109987839A (zh) | 一种玻璃及玻璃制品 | |
CN114956602A (zh) | 化学强化玻璃及其制造方法 | |
CN114956601A (zh) | 化学强化玻璃的制造方法 | |
CN116161876B (zh) | 化学强化玻璃及其制造方法 | |
JP2017114718A (ja) | 化学強化用ガラス板及び化学強化ガラスの製造方法 | |
JP6435937B2 (ja) | 化学強化用ガラス板及び化学強化ガラス |