SU881050A1 - Method of water activation for tightening concrete mix - Google Patents

Method of water activation for tightening concrete mix Download PDF

Info

Publication number
SU881050A1
SU881050A1 SU792760982A SU2760982A SU881050A1 SU 881050 A1 SU881050 A1 SU 881050A1 SU 792760982 A SU792760982 A SU 792760982A SU 2760982 A SU2760982 A SU 2760982A SU 881050 A1 SU881050 A1 SU 881050A1
Authority
SU
USSR - Soviet Union
Prior art keywords
water
strength
magnetic
concrete mix
concrete
Prior art date
Application number
SU792760982A
Other languages
Russian (ru)
Inventor
Генрих Михайлович Короткевич
Original Assignee
За витель
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by За витель filed Critical За витель
Priority to SU792760982A priority Critical patent/SU881050A1/en
Application granted granted Critical
Publication of SU881050A1 publication Critical patent/SU881050A1/en

Description

Изобретение относитс  к промьшшен- ности строительных материалов и может быть использовано в различных отрасл  промышленности и гражданского строительства . Известен способ активации воды затворвни  бетонной смеси путем обработ ки ее ультразвуком 1. Наиболее близким к изобретению  вл етс  способ активации воды затворени  бетонной смеси путем обработки ее магнитным полем, напр женностью 1750 Э 2. Недостатком известного способа обработки воды затвс енн  бетонной снеси  вл етс  низка  прочность бетона . Цель изобретени  - повышение прочности бетона. Поставленна  цепь достигаетс  тем что согласно способу активации воды затрорени  бетонной смеси путем магни ной обработки, магнитную обработку осуществл ют при напр женности магнитного пол  2,0-2,5 Э и дополнительно воду затворени  обрабатывают ультразвуком интенсивностью 15-25 вт/см и частотой 15-30 кГц. П р и м ер. Готов т бетонные смеси из портландцемента старооскольского н Воскресенского заводов М 400, гранитого щебн  крупностью 5-20 мм и речного песка с модулем крупности 2,1 следуницего состава: Цемент 375-390 кг/м Крупный заполнитель до 950 кг/м Вода170-220 л/м Воду затворени  предварительно подвергают активации магнитным полем, ультразвуком и совместным одновременным воздействием магнитного пол  и ультразвука. Продолжительность активахщн во всех трех случа х одинакова. Бетонную смесь сразу после перемешивани  с активированной водой укладываютThe invention relates to the construction materials industry and can be used in various industries and civil engineering. The known method of activating the water of mixing concrete mix by treating it with ultrasound 1. The closest to the invention is the method of activating the mixing water of the concrete mix by treating it with a magnetic field of 1750 Oe 2. The disadvantage of the known method of treating water of the concrete condensate is low concrete strength. The purpose of the invention is to increase the strength of concrete. The delivered chain is achieved by the fact that according to the method of activating the water of splashing the concrete mixture by means of magnesium treatment, the magnetic treatment is carried out at a magnetic field strength of 2.0-2.5 Oe and additionally the mixing water is treated with an ultrasound intensity of 15-25 W / cm and a frequency of 15 -30 kHz. P r and m er. Concrete mixes are prepared from Portland cement of the Star of Oskol n Voskresensky mills M 400, crushed granite with a particle size of 5–20 mm and river sand with a modulus of particle size 2.1 of the following composition: Cement 375–390 kg / m Large aggregate up to 950 kg / m Water 170–220 L / m. The mixing water is preliminarily subjected to activation by a magnetic field, ultrasound, and simultaneous simultaneous exposure to a magnetic field and ultrasound. The duration of the activity is the same in all three cases. Concrete mixture immediately after mixing with activated water is placed

в форму и подвергают уплотнению ударным способом при амплитуде 3,5 мм и частоте соударений 250 уд/мин 4 мин, после чего через нейлоновую тканьinto the mold and subjected to compaction by the impact method with an amplitude of 3.5 mm and a frequency of collisions of 250 beats / min for 4 minutes, then through a nylon fabric

производ т вакуумирование при давлении 0,75-0,9 4-5 мин.vacuuming is performed at a pressure of 0.75-0.9 4-5 minutes.

Результаты испытаний прочности образцов приведены в таблице.The results of testing the strength of the samples are given in the table.

Примечание Водоотделение содержани  (в Note Water separation content (in

Экономический эффект от внедрени  способа по изобретению составл ет 1 руб. на 1 м бетона. Совместна  магнитна  и ультразвукова  обработка воды затворени  позвол ет повысить прочность бетона.The economic effect from the implementation of the method according to the invention is 1 rub. on 1 m of concrete. The combined magnetic and ultrasonic treatment of the mixing water increases the strength of the concrete.

Claims (2)

Формула изобретени Invention Formula Способ активации воды затворени  бетонной смеси путем магнитной обработки , отличающийс  тем, что, с целью повьшени  прочности бедостигает 40% первоначального водоI 1Г-ей серии опытов).The method of activating the mixing water of the concrete mixture by magnetic treatment, characterized in that, in order to increase the strength, it suffers from 40% of the initial water (1 st series of experiments). 5 88105065 8810506 тона, магнитную обработку осуществл -1. Авторское свидетельство СССРtone, magnetic processing carried out -1. USSR author's certificate ют при напр женности магнитного пол № 302940, кл. С 04 В 15/00, 1968.at magnetic field strength No. 302940, cl. From 04 To 15/00, 1968. 2,0-2,5 Э и дополнительно воду затво-2.0-2.5 Oe and additionally water shutter 2. Ctesse Hans-Peter. Elgnung def2. Ctesse Hans-Peter. Elgnung def рени  обрабатывают ультразвуком ий-Hektromagnetisiorung von Anmachlvasтенсивностью 15-25 вт/см и частотойs ser for die Erhohung der Betont,15-30 кГц. SchriftenrBauforeh R, Baustoffe ,Renee is treated with ultrasound i-Hektromagnetisiorung von Anmachlvas with an intensity of 15-25 W / cm and a frequency of ser for die Erhohung der Betont, 15-30 kHz. SchriftenrBauforeh R, Baustoffe, Источники информации,1970, № 12, 80-81, 15, 19, 25 (протоприн тые во внимание при экспертизетип) .Sources of information, 1970, No. 12, 80-81, 15, 19, 25 (protoprintye taken into account during the examination of the type).
SU792760982A 1979-05-03 1979-05-03 Method of water activation for tightening concrete mix SU881050A1 (en)