SU558855A1 - Способ получени двойной соли сульфата кали -кальци - Google Patents

Способ получени двойной соли сульфата кали -кальци

Info

Publication number
SU558855A1
SU558855A1 SU1974436A SU1974436A SU558855A1 SU 558855 A1 SU558855 A1 SU 558855A1 SU 1974436 A SU1974436 A SU 1974436A SU 1974436 A SU1974436 A SU 1974436A SU 558855 A1 SU558855 A1 SU 558855A1
Authority
SU
USSR - Soviet Union
Prior art keywords
calcium
double salt
obtaining
potassium sulfate
suspension
Prior art date
Application number
SU1974436A
Other languages
English (en)
Inventor
Наталья Власьевна Гаркунова
Юрий Сергеевич Плышевский
Зоя Ивановна Плюта
Константин Васильевич Ткачев
Виктор Афанасьевич Рябин
Original Assignee
Предприятие П/Я А-7125
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я А-7125 filed Critical Предприятие П/Я А-7125
Priority to SU1974436A priority Critical patent/SU558855A1/ru
Application granted granted Critical
Publication of SU558855A1 publication Critical patent/SU558855A1/ru

Description

ют без нагревани . Во врем  перемешивани  происходит загустение пульпы до плотности 1,6 г/см с повышением температуры пульпы до 48 С, при которой пульпу выдерживают в течение 10 мин. Пульпу перемедд1вают до однородной консистенции и фильтруют.
В результате получают 230,8 г раствора хлорвда железа, с концентрацией 13,7 % FeClj и 142,8 г влажного осадка, которьш после промывки и сушки пои 105°С содержит 24,6 %KjO. вес осадка
100 г. При этом переход Кз О в осадок составл ет
81,5%.

Claims (2)

1. Способ получени  двойной соли сульфата кали -кальци  путем взаимодействи  сульфатных
растворов с хлоридом кали  и гипсом с последующей фильгравдей Полученной суспензии, отмывкой и сушкой осадка, отличающийс  тем, что, с целью упрощени  процесса и возможности переработки отходов, содержащих сульфат железа, например , отходов производства двуокиси титана, последние используют с концентрацией железного купороса 10-30 вес.%.
2. Способ по п. I, о I   и ч а ю щ и и с   тем, что взаимодействие исходных реагентов осуществл ют при перемешивании суспензии до плотности 1,6-1,8 г/см, а затем выдерживают при температуре 40-60° С в течение 10-60 мин.
Источники инфор ации, прин тые во внимание при экспертизе:
1.Патент США № 3348913, кл. 23-121, опубл 24.10.67.
2.Позин М. Е. Технологи  минеральных солей. 1961,с. 111-112.
SU1974436A 1973-12-04 1973-12-04 Способ получени двойной соли сульфата кали -кальци SU558855A1 (ru)