SU495359A1 - Способ плавки стали в кислородной конверторе - Google Patents
Способ плавки стали в кислородной конвертореInfo
- Publication number
- SU495359A1 SU495359A1 SU2045046A SU2045046A SU495359A1 SU 495359 A1 SU495359 A1 SU 495359A1 SU 2045046 A SU2045046 A SU 2045046A SU 2045046 A SU2045046 A SU 2045046A SU 495359 A1 SU495359 A1 SU 495359A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- oxygen converter
- smelting steel
- oxygen
- heat
- slag
- Prior art date
Description
1
Изобретение от иоюитс к области чор.иой металлур-гии.
Известен способ вьшлаеюи стали в кислородном кон-вертере, включающий продувку металла кислородом и при1садку в Ваину шла кообразующих .
Недостат1КОМ известного способа вл етс низка OKQpocTb шлакообразовани .
Цель изобретени - уюкорение шлакообразава1Ри и улучшение теплового баланса плааки.
Дл этого по предлагаемому юнособу перед продувкой в вавну ввод т сланец, имеюш,ий теплот|в0|рную способность 3500-4000 ккал/кг. Кроме того, сланец /ввод т соиместно с флюсующим материалом.
Предлагаемый спасоб осуществл ют следующим образом.
В .кон1вертер после завалии скрапа заливают чугун и ввод т сла1нец. Во В|рем продувки происходит сгорание слаеца, а выдел ющеес при ЭТ01М тепло способствует улучшению теплового баланса плавки. При сгорании сланца образуетс зола, соде)ржаща 52- 55% СаО, 20-25% SiOa, 4-6% MgO, 5-7%
Ре2Оз, 3-4% АЬОз, представл юща собой легкоплавкий шлак, имеющий температуру плавлени 1300-1400°С.
TaiKHM образом, использование в завалку сланца обе спечивает выделение дополлительного тепла в ванне и быстрое образование акТ1И1ВНОГО шлака.
Сланец может примен тьс также в смеси с известью или в виде брикетов из сланца и извести.
Формула и 3 о б р е т е 1Н и
1.Способ вы|нлав ки стали в кислородном KOHiBepTep-e, включающий продувку металла кислородом и присадку в ванну щлакообразуюш )их, отличающийс тем, что, с целью ускорени шлакообразовани и улучшени теплового баланса плавки, перед продувкой р ванну ввод т сланец, имеющий теплотворную способность 3500-4000 юкал/кг.
2.Способ по н. 1, отличающийс тем, что сланец ввод т совместно с флюсующим материалом.