SU494377A1 - The method of processing nepheline sludge - Google Patents
The method of processing nepheline sludgeInfo
- Publication number
- SU494377A1 SU494377A1 SU2007912A SU2007912A SU494377A1 SU 494377 A1 SU494377 A1 SU 494377A1 SU 2007912 A SU2007912 A SU 2007912A SU 2007912 A SU2007912 A SU 2007912A SU 494377 A1 SU494377 A1 SU 494377A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- sludge
- heat treatment
- carried out
- nepheline sludge
- processing nepheline
- Prior art date
Description
1one
Изобретение огносигс к промышденнооги сгроигедьных материалов к ыожез быть использовано при изготовпеиии теплоизол ционных засыпок из неорганических ыахериалов.The invention of fire retardants to industrial grade materials should be used in the manufacture of heat insulating backfill from inorganic materials.
Иавесген способ обработки нефелинового шлаыа, включающий его мокрый помол.Iavegen method of processing nepheline slag, including its wet grinding.
Недостатком такого способа вл етс изменение свойств материала при последующей службе в услови х переменной влажности.The disadvantage of this method is the change in material properties during subsequent service under conditions of variable humidity.
С целью получени стабильной теплоизол ционной засыпки из шпама и увеличени полноты его гицротации по предлагаемому способу помол шлама осущесгвл юзе в гор чей воде с последующей термообработкой и сушкой при I20-I30°C. L Дп термообработки можно испоньзовать пропаривание и автокпавирование. Нефелиновый шлам измельчают в шаровой мельнице мокрого помола при соотношении между водой и твердой фазой 1:1 до полного прохождени через сито OU8 мм. дл интенсификации гидратации нефелинового шлама испоньзуюЕ гор чую воду с температурой 7U-90 С. После помила в мепьнице дл углублени процесса грдратации полученную водную суспензию нефелинового шлама заливают 2- -кратиым избытком воды с температурой 70-УО°С и выдерживают в течение времени,достаточного дл образовани после высушивани при 120-300°С порошка с объемной массой 200-400 кг/м.In order to obtain a stable heat insulating backfill from spam and increase the completeness of its gitsrotation according to the proposed method, the grinding of sludge was carried out in hot water, followed by heat treatment and drying at I20-I30 ° C. L DP heat treatment can be used for steaming and autocompleting. Nepheline sludge is ground in a wet grinding ball mill at a ratio between water and solid phase of 1: 1 until the OU8 mm passes through the sieve. To intensify the hydration of nepheline sludge, use hot water with a temperature of 7U-90 ° C. After pomming in the field to deepen the grading process, the resulting aqueous suspension of nepheline sludge is poured with 2- steep excess water with a temperature of 70 ° C and hold for sufficient time to form, after drying at 120-300 ° C, a powder with a bulk weight of 200-400 kg / m.
Вместо выдержки молотого шлама в гор чей воде можно использовать пропаривание или автоклавирование сусдензии .Instead of holding ground sludge in hot water, steaming or autoclaving suspensions can be used.
Порошок с низкш объемный веооы попучаез с благодар способыосхи шпаыа к набуханию и глубокой гидратации, т.е. к присоединению большого количества воды. При водонасыщении шлаиа частицы его твердой фазы ирисоедин ют воду различного вида; химическую, адсорбционную, капилл рную. Несмотр на высокую степень набухани , шлам обладает кинетической устойчивостью и не склонен к оседанию.Powder with a low volumetric wave of populations with a means of swelling and deep hydration, i.e. to attach a large amount of water. At the water saturation of the slag particles of its solid phase, various types of water are attached; chemical, adsorption, capillary. Despite the high degree of swelling, the sludge has kinetic stability and is not prone to sedimentation.
Полученна из глубоко гидрагированного щлаыа засыпка имеет коэффициент теппопроводности окопо 0,08 ккал/и час град, несгораема и биологически стойка.The resulting deeply hydrated bedding has a thermal conductivity coefficient of around 0.08 kcal / hour and hail, non-combustible and biologically resistant.
Преддагаемый способ обработки нефепинового шлама позвол ет подучатьA predagdae method of processing nephepinovoy sludge allows you to pick up
гепдоизолнционную засыпку, по своим свойствам отвечаощую требовани м, предъ ввнемым к теплоизол ционным засыпк&м.anti-radiation backfilling, according to its properties, meets the requirements of thermal insulating backfills & m.
ФОРМУЛА ИЗОБРЕТЕНИЯCLAIM
Claims (3)