SU437807A1 - Способ получени низкоуглеродистой стали - Google Patents
Способ получени низкоуглеродистой сталиInfo
- Publication number
- SU437807A1 SU437807A1 SU1928150A SU1928150A SU437807A1 SU 437807 A1 SU437807 A1 SU 437807A1 SU 1928150 A SU1928150 A SU 1928150A SU 1928150 A SU1928150 A SU 1928150A SU 437807 A1 SU437807 A1 SU 437807A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- carbon steel
- low carbon
- producing low
- metal
- period
- Prior art date
Description
(54) СПОСОБ ПОЛУЧЕНИЯ НИЗКОУГЛЕРОДИСТОЙ СТАЛИ 3 Общее количество присаженных окатышей 6,5 т. Конечна температура металла 1640°С, содержание углерода 0,025%, содержание кислорода 0,085%., Предмет изобретени Способ получени низкоуглеродистон стали с содержанием углеродане более 0,03% и конверторе из шихты, содержаш,ей жидкий чугун и металлолом, в ключаюш ий продувку металла техническим кислородом в двапериода со скачиванием шлака и присадкой охладите4 л : в первом периоде - металлолома, а во втором - металлизованных окатышей по ходу продувки, отличающийс тем, что, с целью повыи1епи качества металла, ускорени про5цесса и увеличени выхода стали, в завалку 1 01вертор присаживают металлолом в количестве 28-33% от веса жндкого чугуна и продувают металла до 1570-1620°С к концу первого периода, а во втором периоде приса юживают металлизоваииые окатыши порци ми по 0,4-0,5 т через каждые 0,3-0,5 мин в количестве 4-10% от веса чугуна в течение всего времени продувки.