SU1645026A1 - Способ получени изол ционных покрытий - Google Patents
Способ получени изол ционных покрытий Download PDFInfo
- Publication number
- SU1645026A1 SU1645026A1 SU884446846A SU4446846A SU1645026A1 SU 1645026 A1 SU1645026 A1 SU 1645026A1 SU 884446846 A SU884446846 A SU 884446846A SU 4446846 A SU4446846 A SU 4446846A SU 1645026 A1 SU1645026 A1 SU 1645026A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- coatings
- isocyanates
- filler
- distance
- mixture
- Prior art date
Abstract
Изобретение относитс к производству строительных материалов и мо жет быть использовано при изготовлении изол ционных покрытий. Изобретение позвол ет повысить механическую прочность покрытий, снизить их стои- . мость и упростить технологию за счет того, что в способе получени изол ционных покрытий вначале нанос т на металлическую поверхность отверди- тель, а затем через 0,5-1,0 с смесь изоцианатов с наполнителем и через 2-3 мин полученное покрытие обрабатывают водой путем распылени на рассто нии 0,5-0,6 м под давлением 0,05-0,08 Ша. 4 табл.
Description
Изобретение относитс к производству строительных материалов и может быть использовано при изготовлении из ол ционных покрытий.
Целью изобретени вл етс повышение механической прочности покрытий, .снижение стоимости и упрощение технологии .
Дл производства изол ционных работ используют композицию на осно- ве изоцианатов и отвердител - ди- этиленгликол в соотношении 100 и 20-30 мае.ч.соответственно. Пульверизацией раздельно на металлическую поверхность непрерывно нанос т сначала диэтиленгликоль,затемс интерва лом 0,5-1 с изоцианаты с наполнителем (например алюминиевую пудру - 2 мае.ч. на 100 мае.ч. изоцианатов) Следом с интервалом в 2-3 мин (с начала полимеризации композиции) осуществл ют уплотнение вод ным распылением на рассто нии 0,6-0,5 м от
объекта покрыти под давлением 0,05-0,08 МПа„
Составы дл осуществлени способа приведены в табл.1.
Таблица 1
Толщина покрыти 200-300 мк. Свойства изол ционного покрыти на их основе - в табл,2.3 и 4.
Таблица2
ТаблицаЗ Вли ние давлени воды на прочность покрыти .
Свойства изол ционных
изделий
Способ нанесени
при давлении | без давле- воды I ни воды
гВли ние рассто ни от источника распылени на структуру покрыти
0,5 м
Не выра- Слабо -.Четко вы- Четко Четко вы- Четко Четко вы- Размыта женавыра- ражена выра- раженавыра- ражена с
жена
0,6 м
Не выра- Слабо Не очень Четко Четко вы- Четко Четко вы- Размыта женавыра- четко вы- выра- ражена выраже-ражена с
жена
ражена
Формула изобретени
Способ получени изол ционных пок- 25 рытий путем нанесени на металлическую поверхность композиций на основе смеси изоцианатов, наполнител и от- ;вердител , отличающийс тем, что, с целью повышени механичес-зо кой прочности покрытий, снижени стоиТаблица
жена
жена
участками размыва
жена
на
участками размыва
мости и упрощени технологии, на поверхность вначале нанос т отвердн- тель, а затем через 0,5-1 с смесь изоцианатов с наполнителем и через 2- 3 мин полученное покрытие обрабатывают водой путем распылени на рас- ,сто нии 0.5-0,6 м под давлением |0,05-0,08 МПа.
Claims (1)
- Формула 'Изобретения Способ получения изоляционных покрытий путем нанесения на металлическую поверхность композиций на основе смеси изоцианатов, наполнителя и отвердителя, отличающийся тем, что, с целью повышения механической прочности покрытий, снижения стоимости и упрощения технологии, на по25 верхность вначале наносят отвердитель, а затем через 0,5-1 с смесь изо цианатов с наполнителем и через 23 мин полученное покрытие обрабатывают водой путем распыления на рас30 .стоянии 0.5-0,6 м под давлением0,05-0,08 МПа.