SU1514732A1 - Способ обработки шлакового заполнителя - Google Patents

Способ обработки шлакового заполнителя Download PDF

Info

Publication number
SU1514732A1
SU1514732A1 SU874329941A SU4329941A SU1514732A1 SU 1514732 A1 SU1514732 A1 SU 1514732A1 SU 874329941 A SU874329941 A SU 874329941A SU 4329941 A SU4329941 A SU 4329941A SU 1514732 A1 SU1514732 A1 SU 1514732A1
Authority
SU
USSR - Soviet Union
Prior art keywords
asbestos
waste
cement production
lime milk
slag aggregate
Prior art date
Application number
SU874329941A
Other languages
English (en)
Inventor
Leonid I Dvorkin
Viktor N Marchuk
Original Assignee
Uk I Inzh Vodnogo Khoz
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Uk I Inzh Vodnogo Khoz filed Critical Uk I Inzh Vodnogo Khoz
Priority to SU874329941A priority Critical patent/SU1514732A1/ru
Application granted granted Critical
Publication of SU1514732A1 publication Critical patent/SU1514732A1/ru

Description

Изобретение относится к промышленности строительных материалов и
2
может быть использовано для изготовления бетонных и железобетонных конструкций и изделий. Целью изобретения является повышение прочности, водонепроницаемости и морозостойкости. Готовят суспензию, содержащую (мас.%) 30_35 известкового молока и 65“70 отходов асбестоцементного производства, и обрабатывают шлаковый заполнитель. Прочность на сжатие бетона после тепловлажностной обработки 40-43 МПа, водонепроницаемость 12-14 и морозостойкость 450-500. 1 табл.
Изобретение относится к промышленности строительных материалов и может быть использовано для изготовления бетонных и железобетонных конструкций и изделий.
Цель изобретения - повышение прочности, водонепроницаемости и морозостойкости .
Пример. Щебень из мартеновского шлака фракции 5“40 мм погружают в предварительно приготовленную суспензию, содержащую известковое молоко и отходы асбестоцементного производства перемешивают в течение 3“
4 мин, извлекают на сетку и выдерживают в течение 2-3 сут. Для обработки 1 кг шлакового щебня необходимо не менее 200 г суспензии.
Результаты испытаний представлены в таблице.

Claims (1)

  1. Формула изобретения
    Способ обработки шлакового заполнителя путем активации его известковым молоком, отличающийся тем, что, с целью повышения прочности, водонепроницаемости, морозостойкости, известковое молоко предварительно смешивают с отходами асбестоцементного производства при следующем соотношении компонентов, масД:
    Известковое молоко 30“35
    Отходы асбестоцементного производства 65_
    -8Ц 1514732
    3
    1514732
    4
    Способ обработки Состав суспензии, мас.% — Прочность бетона на сжатие, МПа Водонепроницаемость Морозостойкость, циклы Известковое молоко Отходы асбестоцементного производства после ТВО в возрасте 28 сут По изоб- 25 75 36,4 50,6 8 400 ретению 30 70 40,5 56,4 12 450 32,5 67,5 41,1 57,0 12 450 35 65 *»3,5 58,1 14 500 По прото- 40 60 38,9 53,0 11 450 типу - 38,8 50,1 10 450
SU874329941A 1987-09-30 1987-09-30 Способ обработки шлакового заполнителя SU1514732A1 (ru)