SU1054415A1 - Способ ведени доменной плавки - Google Patents
Способ ведени доменной плавки Download PDFInfo
- Publication number
- SU1054415A1 SU1054415A1 SU823451141A SU3451141A SU1054415A1 SU 1054415 A1 SU1054415 A1 SU 1054415A1 SU 823451141 A SU823451141 A SU 823451141A SU 3451141 A SU3451141 A SU 3451141A SU 1054415 A1 SU1054415 A1 SU 1054415A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- natural gas
- oxygen
- consumption
- ratio
- gas
- Prior art date
Abstract
Изобретение относитс к черной металлургии и может быть использовано в доменной- плавке с применением природного газа и кислорода, вводимых в технологическое дутье. Цель изобретени - снижение расхода кокса и увеличение производительности. Технологический кислород и природный газ перед вводом в дутье смешиваютс перед подачей в фурмы в соотношении О,7...1,4 по объему и ввод тс в гор чее дутье через фурму. Снижение расхода кокса и повышение производительности достигаетс полным сгоранием природного газа-в фурменной зоне. 1 з.п. ф-лы.
Description
§
(Л
О1
Claims (1)
- 4 4; 110 Изобретение относитс к черной металлургии, в частности, к доменной плавке с добавками природного газа и кислорода в дутье. Цель изобретени - снижение расхода кокса и увеличение производительности путем обеспечени полного перемешивани и сгорани природного газа в потоке дуть . Пример. На доменной печи объемом 3000 м при нагреве дуть 1200 С через газоподвод щие трубки в воздушную полость фурм подают смесь природного газа и кислорода в соотношении 0,7 по объему. Общие расходы природного газа и кислорода составл ют при этом соответственно 300 и 450 . После выхода печи на устойчивый режим работы продолжают увеличение обогащени дуть кислородом и расхода природного газа, довед соотношение природного газа и кислорода До 1,4. Суммарные расходы природного газа 11 кислорода при этом составл ют соответственно 670 и 950 . За счет оптимального соотношени кислорода и природного газа в газокислородной смеси улучшилось использование природного газа, что дало снижение расхода кокса на 3,0-3,5% и увеличение производительности на 3,552 3,8%. При использовании смеси с соотношением природного газа к кислороду менее 0,7 наблюдались нарушени нормального схода шихтовых материалов вследствие чрезмерного увеличени температуры горени , а при превьш ении соотношени 1,4 увеличивалс расход кокса и снижалась производительность печи на 0,5-0,8% вследствие неполного сгорани природного газа. I Использование изобретени позвол ет повысить производительность и снизить расход кокса за счет более полного сгорани природного газа в фурменной зоне. Формула изобретени Способ ведени доменной плавки, включающий смешение природного газа и кислорода с последующим вводом газокислородной смеси через фурмы в поток гор чего дуть , отличающийс , тем, что, с целью снижени расхода кокса и увеличени производительности путем обеспечени полного перемешивани и сгорани природного газа в потоке дуть , соотношение природного газа и кислЬрода в газокислородной смеси поддерживают в пределах О,7...1,4 по объему.