MD3753F1 - Electrode for hydrogen electrolytic obtaining and process for manufacturing thereof - Google Patents

Electrode for hydrogen electrolytic obtaining and process for manufacturing thereof Download PDF

Info

Publication number
MD3753F1
MD3753F1 MDA20070010A MD20070010A MD3753F1 MD 3753 F1 MD3753 F1 MD 3753F1 MD A20070010 A MDA20070010 A MD A20070010A MD 20070010 A MD20070010 A MD 20070010A MD 3753 F1 MD3753 F1 MD 3753F1
Authority
MD
Moldova
Prior art keywords
nickel
cobalt
solution
palladium
alloy
Prior art date
Application number
MDA20070010A
Other languages
Romanian (ro)
Other versions
MD3753G2 (en
Inventor
Olga Covaliova
Victor Covaliov
Original Assignee
Universitatea De Stat Din Moldova
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Universitatea De Stat Din Moldova filed Critical Universitatea De Stat Din Moldova
Priority to MDA20070010A priority Critical patent/MD3753G2/en
Publication of MD3753F1 publication Critical patent/MD3753F1/en
Publication of MD3753G2 publication Critical patent/MD3753G2/en

Abstract

Inventia se refera la electrochimia tehnica, si anume la electrodul pentru obtinerea electroliticaa hidrogenului si la procedeul de confectionare aacestuia. Electrodul, conform inventiei, consta dintr-un suport conducator de curent din material fibrocarbonic poros si dintr-un strat activ din aliaj poros de cobalt-nichel-bor-paladiu. Procedeul de confectionare a electrodului include depunerea pe suportul conducator de curent a aliajului poros de cobalt-nichel dintr-o solutie, care contine saruri de cobalt, de nichel si dimetilaminoboran, cu dizolvarea ulterioara a componentului nemetalic. Se efectueaza activarea catalitica cu paladiu a suprafetei poroase a materialului fibrocarbonic si depunerea chimico-catalitica a aliajului de cobalt-nichel-paladiu-bor din solutie, care suplimentar contine sare de paladiu, pirofosfat de potasiu, trietanolamina si 2-mercaptobenzotiazol, in urmatorulraport al componentelor, g/L: clorura de nichel 30…35sulfat de cobalt 15…20clorura de paladiu 3…5pirofosfat de potasiu 60…80solutie apoasa de 25% de trietanolamina, mL 60…100dimetilaminoboran 1…32-mercaptobenzotiazol 0,01…0,02.Depunerea aliajului se efectueaza la temperatura de 50…70°C si pH 6,5…10,0, iar dizolvarea se efectueaza prin prelucrarea in fluxul unei solutii incalzite pana la 40…50°C, timp de 3…5 min, solutia avand urmatorul raport al componentelor, g/L:persulfat de amoniu 20…50acid sulfuric, densitatea 1,84 10…15apa restul. The invention relates to the technical electrochemistry, namely to the electrode for obtaining electrolytic hydrogen and to the process of making it. The electrode, according to the invention, consists of a current conducting support of porous fibrocarbon material and an active layer of porous cobalt-nickel-boron-palladium alloy. The process of making the electrode includes the deposition on the current conducting support of the cobalt-nickel porous alloy in a solution, which contains cobalt, nickel and dimethylaminoboran salts, with the subsequent dissolution of the non-metallic component. Palladium catalytic activation of the porous surface of the fibrocarbon material and the chemical-catalytic deposition of cobalt-nickel-palladium-boron alloy in the solution is carried out, which additionally contains palladium salt, potassium pyrophosphate, triethanolamine and 2-mercaptobenzothiazole, in the following report of components, g / L: nickel chloride 30 ... 35 cobalt sulphate 15 ... 20 palladium chloride 3 ... 5 potassium pyrophosphate 60 ... 80 25% aqueous triethanolamine solution, mL 60 ... 100 dimethylaminoborane 1 ... 32-mercaptobenzothiazole 0.01 ... 0.02 . The alloy is deposited at 50 ... 70 ° C and pH 6.5 ... 10.0, and the dissolution is carried out by processing in the flow of a heated solution up to 40 ... 50 ° C, for 3 ... 5 minutes, the solution having the following component ratio, g / L: ammonium persulfate 20 ... 50 sulfuric acid, density 1.84 10 ... 15 after the remainder.

MDA20070010A 2007-01-17 2007-01-17 Electrode for hydrogen electrolytic obtaining and process for manufacturing thereof MD3753G2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
MDA20070010A MD3753G2 (en) 2007-01-17 2007-01-17 Electrode for hydrogen electrolytic obtaining and process for manufacturing thereof

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
MDA20070010A MD3753G2 (en) 2007-01-17 2007-01-17 Electrode for hydrogen electrolytic obtaining and process for manufacturing thereof

Publications (2)

Publication Number Publication Date
MD3753F1 true MD3753F1 (en) 2008-11-28
MD3753G2 MD3753G2 (en) 2009-06-30

Family

ID=40097504

Family Applications (1)

Application Number Title Priority Date Filing Date
MDA20070010A MD3753G2 (en) 2007-01-17 2007-01-17 Electrode for hydrogen electrolytic obtaining and process for manufacturing thereof

Country Status (1)

Country Link
MD (1) MD3753G2 (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
MD4207C1 (en) * 2011-10-10 2013-09-30 Государственный Университет Молд0 Process for manufacturing a combined volume-porous flow-through electrode and process for electrolytic production of hydrogen
CN115386899A (en) * 2022-10-08 2022-11-25 山东昭文新能源科技有限公司 A kind of cobalt-nickel alloy/porous carbon oxygen evolution catalyst and its preparation method and application

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
MD244Z (en) * 2009-09-04 2011-02-28 Государственный Университет Молд0 Electrode for electrolytic production of hydrogen and process for manufacturing thereof

Family Cites Families (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
SU537125A1 (en) * 1974-04-25 1976-11-30 Институт электрохимии Академии наук СССР Electrode for electrolysis of an alkali aqueous solution and method for its manufacture
MD3151G2 (en) * 2005-12-05 2007-04-30 Государственный Университет Молд0 Electrode and process for obtaining thereof for electrolysis of the alkaline aqueous solutions
MD3383G2 (en) * 2006-02-17 2008-03-31 Государственный Университет Молд0 Electrode and process for electroflotation separation of disperse systems and process for electrode obtaining
MD3488G2 (en) * 2007-01-17 2008-08-31 Государственный Университет Молд0 Process for hydrogen electrolytic obtaining

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
MD4207C1 (en) * 2011-10-10 2013-09-30 Государственный Университет Молд0 Process for manufacturing a combined volume-porous flow-through electrode and process for electrolytic production of hydrogen
CN115386899A (en) * 2022-10-08 2022-11-25 山东昭文新能源科技有限公司 A kind of cobalt-nickel alloy/porous carbon oxygen evolution catalyst and its preparation method and application

Also Published As

Publication number Publication date
MD3753G2 (en) 2009-06-30

Similar Documents

Publication Publication Date Title
AU2018335218B2 (en) Method of producing an electrocatalyst
CN102719846A (en) Alkaline water electrolysis Ni-based three-dimensional network gradient alloy hydrogen evolution cathode
JP2015524024A5 (en)
CN102560571B (en) Non-cyanide silver coating stable electrical plating solution, preparation method and silver-plated method thereof
CN102691081A (en) A kind of electroplating silver solution and electroplating method
Mech et al. Electrodeposition of catalytically active Ni-Mo alloys
CN101387000A (en) Non-cyanogen strike copper plating technique
CN104562107A (en) Highly-corrosion-resistant environment-friendly black tin-cobalt alloy electroplating liquid and electroplating method thereof.
MD3753F1 (en) Electrode for hydrogen electrolytic obtaining and process for manufacturing thereof
US4152240A (en) Plated metallic cathode with porous copper subplating
CN108588768B (en) Steel and iron parts alkalinity deep hole nickel-plating additive, pre-plating solution and pre-plating process
CN102703840A (en) Block ternary nickel-tungsten-phosphorus amorphous alloy and preparation method thereof
Yan et al. Electrochemical reduction process of Co (II) in citrate solution
MD3488F1 (en) Process for hydrogen electrolytic obtaining
CN101260551A (en) Cyanide-free silver electroplating method
US4214954A (en) Plated metallic cathode with porous copper subplating
MD244Z (en) Electrode for electrolytic production of hydrogen and process for manufacturing thereof
MD3151F1 (en) Electrode and process for obtaining thereof for electrolysis of the alkaline aqueous solutions
CN103173818A (en) Environment-friendly silver electroplating technique
CN111115768A (en) Electrode for removing nitrate nitrogen and total nitrogen in water and preparation method thereof
JP2005290500A (en) Alloy electrode for hydrogen generation and method for producing the same
JP2004137587A (en) Alloy electrode for hydrogen generation and its production method
CN105401180A (en) Electroplating liquid of wear-resistant gold-plated film and electroplating method thereof
Dikici Nikel-Kobalt (Ni-Co) Alaşımlı Kaplamalarda Co Miktarının Mikroyapıya Etkisi
JP3161827U (en) Insoluble anode structure

Legal Events

Date Code Title Description
FG4A Patent for invention issued
KA4A Patent for invention lapsed due to non-payment of fees (with right of restoration)
MM4A Patent for invention definitely lapsed due to non-payment of fees