KR960039465A - 알칼리축전지용 수소흡장합금의 제조방법 및 수소흡장합금전극의 제조방법 - Google Patents
알칼리축전지용 수소흡장합금의 제조방법 및 수소흡장합금전극의 제조방법 Download PDFInfo
- Publication number
- KR960039465A KR960039465A KR1019960010115A KR19960010115A KR960039465A KR 960039465 A KR960039465 A KR 960039465A KR 1019960010115 A KR1019960010115 A KR 1019960010115A KR 19960010115 A KR19960010115 A KR 19960010115A KR 960039465 A KR960039465 A KR 960039465A
- Authority
- KR
- South Korea
- Prior art keywords
- hydrogen
- absorbing alloy
- alloy
- oxalate
- aqueous solution
- Prior art date
Abstract
1. 청구범위에 기재된 발명이 속한 기술분야
본 발명은 수소흡장합금전극의 제조 방법.에 관한 것이며 상세하게는 수소흡장합금전극의 구성재료인 수소흡장합금분말의 처리방법에 관한 것이다.
2. 발명이 해결하려고, 하는 기술적 과,제
본 발명은 작업성이 좋고, 더구나 산처리 효과의 높은 수소흡장합금분말의 처리방법을 제공하고, 충전초기의 전지내압이 작고, 또한 우수한 고,율방전 특성 및 사이클특성을 갖는 알칼리축전지용수소흡장합금전극을 제공하는 것이다.
3. 발명의 해결방법의 요지
본 발명은 수소흡장합금분말을 이용하여 이루어지는 수소흡장합금전극의 제조 방법.에 있어서, 항기 제조 방법.이 수소흡장합금분말을 강산성용액으로 세정한 후 상기 강산성용액보다 pH값이 큰 약산성으로 세정처리하는 2단계 처리공정으로 구성되는 것을 특징으로 한다.
4. 발명의 중요한 용도
수소흡장합금분말을 2단계로 산처리하는 본 발명의 수소흡장합금전극의 제조 방법.에 의하면, 전극의 초기 충전시의 전지내압을 저감시키고, 또한 고,율방전특성, 사이클특성을 현저하게 향상시킬 수 있다.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 산처리제수소흡장합금에 대한 표면처리에 있어서, 표면처리액의 NA2HPO4농도가 전지초기내압과,의 관계를 나타내는 그래프다.제2도는 산처리제수소흡장합금에대한 표면처리에 있어서, 표면처리액의 NA2HPO4농도와, 고,율방전특성치와,의 관계를 나타낸 그래프이다. 제3도는 산처리제수소흡장합금에 대한 표면처리에 있어서, 표면처리액의 NA2HPO4농도와, 사이클수명과,의 관계를 나타낸 그래프이다.
Claims (14)
- 수소흡장합금분말을 이용하여 구성된 수소흡장합금전극의 제조 방법에 있어서, 상기 제조 방법이 수소흡장합금분말을 강산성액으로 세정한 후, 상기 강산성액보다 pH값이 큰 약산성액에서 세정처리하는 2단계 산처리공정을 거치는 것을 특징으로 하는 수소흡장합금전극의 제조방법.
- 제1항에 있어서, 상기 강산성용액이 pH0.5 이상에서 2.0 이하의 강산성수용액이며, 상기 약산성용액이 PH2.2.이상 5.0이하의 약산성수용액인 것을 특징으로 하는 수소흡장합금전극의 제조 방법.
- 제2항에 있어서, 상기 약산성수용액이 pH2.2 이상 5.0 이하의 완충수용액인 것을 특징으로 하는 수소흡장합금전극의 제조 방법.
- 수소흡장합금을 산성수용액에 침적처리하는 산처리공정과, 상기 산처리한 수소흡장합금에 대하여 0.6 ∼ 10중량% 농도의 옥소산염수용액으로 표면처리하는 옥소산염 표면처리공정을 포함하는 것을 특징으로 하는 알칼리축전지용수소흡장합금의 제조 방법.
- 제4항에 있어서, 상기 옥소산염표면처리공정으로 처리한 수소흡장합금을 다시 순수에 침적 보존하는 순수침적보존공정을 부가하는 것을 특징으로 하는 알칼리축전지용수소흡장합금의 제조 방법.
- 제4항에 있어서, 상기 옥소산염표면처리공정으로 처리한 수소흡장장합금을 다시 순수에서 교반세정하는 순수교반교정을 부가하는 것을 특징으로 하는 알칼리축전지용수소흡장합금의 제조 방법.
- 수소흡장합금을 산성수용액에 침적처리하는 산처리공정과 상기 산처리한 수소흡장합금에 대하여 고농도의 옥수산염수용액으로 표면처리하는 고농도옥소산염표면처리공정과, 상기 고농도옥소산염수용액으로 표면처리한 수소흡장합금을 상기 고농도 옥소산염수용액보다도 저농도의 옥소산염수용액으로 교반세정하는 저농도옥소산염교반세정공정을 거치는 것을 특징으로 하는 알칼리축전지용수소흡장합금의 제조 방법.
- 수소흡장합금을 산성수용액에 침적처리하는 산처리공정과, 상기 산처리한 수소흡장합금에대하여 고농도의 옥소산염수용액으로 표면처리하는 고농도옥소산염표면처리공정과, 상기 고농도옥소산염수용액으로 표면처리한 수소흡장합금을 상기 고농도옥소산염수용액보다도 저농도의 옥소산염수용액으로 침적보존하는 저농도옥소산염침적공정을 거치는 것을 특징으로 하는 알칼라축전지용수소흡장합금의 제조 방법.
- 제4항 또는 제5항에 있어서, 상기 고,농도옥소산염수용액의 농도가 0.6 ∼ 10중량%이며, 상기 저농도 옥소산염수용액의 농도가 0.1 ∼ 1중량%인 것을 특징으로 하는 알칼리축전지용수소흡장합금의 제조 방법.
- 수소흡장합금을 산성수용액으로 처리하는 산처리공정과, 상기 산처리공정에 의해 수소흡장합금에 유입된 음이온의 잔류량이 수소흡장합금에 대해 5 × 10∼6mol/g이하로 될 때까지 세정하는 공정을 갖춘 알칼리축전지용 수소흡장합금의 제조 방법.
- 제10항에 있어서, 상기 산성 수용액의 pH가 0.5이상, 3.5이하인것을 특징으로 하는 알칼리축전지용수소흡장합금의 제조 방법.
- 제10항 또는 제11항에 있어서, 상기 세정공정에서의 세정이 산화방지제함유수소액으로 행해지는 것을 특징으로 하는 알칼리축전지용수소흡장합금의 제조 방법.
- 제10항내지 제12항의 어느 한 항에 있어서, 상기 세정공정 후에 다시 상기 세정공정으로 세정된 수소흡장합금을 산화방지제함유 수용액중에 침적보존하는 보존세정공정을 갖는 것을 특징으로 하는 알칼리축전이용 수소흡장합금의 제조 방법.
- 제10항 내지 제13항의 어느 한 항에 있어서, 상기 수소흡장합금이 4.0 × 10∼3이하 불균일 왜곡을 갖고있는 것을 특징으로 하는 알칼리축전지용수소흡장합금의 제조 방법.※참고사항:최초출원 내용에 의하여 공개하는 것임.