KR910012200A - 자기소결성을 갖는 탄소재 원료의 제조방법 - Google Patents
자기소결성을 갖는 탄소재 원료의 제조방법 Download PDFInfo
- Publication number
- KR910012200A KR910012200A KR1019890019994A KR890019994A KR910012200A KR 910012200 A KR910012200 A KR 910012200A KR 1019890019994 A KR1019890019994 A KR 1019890019994A KR 890019994 A KR890019994 A KR 890019994A KR 910012200 A KR910012200 A KR 910012200A
- Authority
- KR
- South Korea
- Prior art keywords
- self
- raw material
- sintering
- manufacturing
- temperature
- Prior art date
Abstract
내용 없음.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 본 발명에 의해 제조된 자기소결성 탄소재원료의 편광형미경사진.
Claims (1)
- 콜타르 또는 핏치를 원료로 하여 자기소결성을 갖는 탄소재(탄소성형체)원료를 제조하는 방법에 있어서, 콜타르 또는 핏치내부에 산소농도가 21wt% 함유된 혼합가스를 100ml/min·gr의 유속으로 취입하면서 1-3℃/min의 승온속도로 300-350℃까지 가열하여 이 온도에서 2-4시간 유지시킨 후 5-10℃/min의 승온속도로 400-450℃의 온도로 가열하고, 이 온도에서 5-10분간 유지한 후 공냉시키는 것을 특징으로 하는 자기소결성을 갖는 탄소재 원료의 제조방법.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.