KR880009410A - 관구용(管球用) 유리 발브의 제조방법 - Google Patents
관구용(管球用) 유리 발브의 제조방법 Download PDFInfo
- Publication number
- KR880009410A KR880009410A KR1019880000758A KR880000758A KR880009410A KR 880009410 A KR880009410 A KR 880009410A KR 1019880000758 A KR1019880000758 A KR 1019880000758A KR 880000758 A KR880000758 A KR 880000758A KR 880009410 A KR880009410 A KR 880009410A
- Authority
- KR
- South Korea
- Prior art keywords
- glass tube
- molding
- axis
- pair
- cross
- Prior art date
Abstract
내용 없음.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제 4, 5는 각각 공정을 순서대로 나타낸 설명도.
제 6 도는 본 발명에 관계되는 제조방법에 의해 제조된 발브를 나타낸 사시도.
제 7 도는 제 6 도의 I-I선에 따른 단면도.
제 8 도는 제 6 도의 II-II선에 따른 단면도.
제 9 도는 본 발명에 의한 제조방법에 의해 제조된 발브의 변형예로서, 제 7 도에 나타낸 발브의 단면형상에 대응하는 부분의 단면 형상이 나타나 있다.
Claims (10)
- 개구된 양단부를 가지는 곧은 유리관을 준비하고, 곧은 유리관을 그 축선이 거의 동일한 면내에 포함하여 소정의 만곡형상에 따르게 하여 꾸부리고, 꾸부려진 유리관을 그 축선과 직각으로 교차하는 방향에 대한 단면형상이 전술한 면과 거의 직각으로 교차하는 방향으로 압축된 소정의 형상이 되도록 변형하는 단계로 이루어진 것을 특징으로 하는 관구형 발브의 제조방법.
- 제1항에 있어서, 꾸부려진 유리관은 양단부를 남기고 변형되는 것을 특징으로 하는 제조방법.
- 제2항에 있어서, 변형 공정은 꾸부려진 유리관을 발브에 모울드 성형하는 공정을 포함하며, 전술한 모울드 성형 공정은, 꾸부려진 유리관을 가열 연화하고, 가열연화된 유리관을 대향하는 한쌍의 모울딩대 사이에서 위치를 정하고, 한쌍의 모울딩 대는 각각 소정의 만곡형상 및 소정의 단면형상에 대응하는 성형면을 가지고 있고, 전술한 유리관을 한쌍의 모울딩대에서 꺾어서 전술한 발브를 성형하는 것으로 구성되어 있는 것을 특징으로 하는 방법.
- 제3항에 있어서, 모울딩의 단계는 전술한 가열 연화된 유리관을 한쌍의 모울딩대로 꺽어서, 개구단부에서 유리관 내로 가압된 가스를 주입하여 유리관을 모울딩대의 각각의 성형면에 밀착시키는 것을 포함하는 것을 특징으로 하는 방법.
- 제3항에 있어서, 가열 연화된 유리관은 양단부로 지지되어 걸려 있는 것을 특징으로 하는 방법.
- 제2항에 있어서, 양단부를 잘라내는 단계로 구성되어 있는 것을 특징으로 하는 방법.
- 제1항에 있어서, 곧은 유리관은 양단부가 서로 근접되어, 그 축선이 원주형상에 따르게 하여 꾸부려진 것을 특징으로 하는 방법.
- 제1항에 있어서, 곧은 유리관은 양단부가 서로 근접되어, 그 축선이 거의 U자 형상으로 꾸부려진 것을 특징으로 하는 방법.
- 제3항에 있어서, 단면 현상은, 전술한 면에 포함되어 있는 대칭축선을 가지고 있는 편평한 원환형상을 포함하고 있는 것을 특징으로 하는 방법.
- 제9항에 있어서, 모울딩의 단계에서, 전술한 단면 형상의 대칭축선 약각 만곡되어 있는 것을 특징으로 하는 방법.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.