KR20230133018A - Damage restoration method of floor board - Google Patents

Damage restoration method of floor board Download PDF

Info

Publication number
KR20230133018A
KR20230133018A KR1020220030008A KR20220030008A KR20230133018A KR 20230133018 A KR20230133018 A KR 20230133018A KR 1020220030008 A KR1020220030008 A KR 1020220030008A KR 20220030008 A KR20220030008 A KR 20220030008A KR 20230133018 A KR20230133018 A KR 20230133018A
Authority
KR
South Korea
Prior art keywords
flooring
quick
damage
restoring
agent
Prior art date
Application number
KR1020220030008A
Other languages
Korean (ko)
Inventor
이일건
김태조
Original Assignee
이일건
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이일건 filed Critical 이일건
Priority to KR1020220030008A priority Critical patent/KR20230133018A/en
Publication of KR20230133018A publication Critical patent/KR20230133018A/en

Abstract

본 발명은 석재로 제작된 바닥재의 추가적인 파손을 방지할 수 있는 보강을 실현하면서 파손 부분을 저비용으로 신속히 복원시킬 수 있도록 한 바닥재의 파손 복원 방법을 제공한다.
본 발명의 적절한 실시 형태에 따른 바닥재의 파손 복원 방법은, 석재로 제작되어 바닥에 시공된 바닥재에서 발생된 들뜸, 균열, 파손 부분을 철거하는 단계와; 철거부분이 있는 일정 영역의 둘레를 따라 바닥재에 커팅 작업을 하여 급결제 주입홈통을 형성시켜 주는 단계와; 바닥재의 추가 파손을 방지하기 위해 급결제 주입홈통으로 급결제를 주입하여 파손부분을 갖는 바닥재의 하부 빈공간에 충진·경화시켜 해당 바닥재의 하면에 급결보강층을 형성시키는 단계; 복원제를 바닥재의 철거 부분에 메워 복원하는 단계와; 복원 부분에 광택이 이루어지도록 연마하는 단계;를 포함환 것을 특징으로 한다.
The present invention provides a method of restoring damage to flooring made of stone, which allows quick restoration of damaged parts at low cost while providing reinforcement to prevent further damage to flooring made of stone.
A method of restoring damage to a flooring material according to a suitable embodiment of the present invention includes the steps of removing the lifting, cracking, and damaged portions generated in the flooring material made of stone and installed on the floor; A step of cutting the flooring material along the circumference of a certain area where the demolition part is located to form an accelerator injection trough; In order to prevent further damage to the flooring, injecting a quick-setting agent into the quick-setting agent injection trough to fill and harden the empty space at the bottom of the flooring having the damaged portion to form a quick-setting reinforcement layer on the lower surface of the flooring; Restoring the removed part of the flooring by filling it with a restoration agent; It is characterized in that it includes a step of polishing the restored part to achieve gloss.

Description

바닥재의 파손 복원 방법{Damage restoration method of floor board}Damage restoration method of floor board}

본 발명은 바닥재의 파손 복원 방법에 관한 것으로, 특히 석재로 제작된 바닥재의 추가적인 파손을 방지할 수 있는 보강을 실현하면서 파손 부분을 저비용으로 신속히 복원시킬 수 있도록 한 바닥재의 파손 복원 방법에 관한 것이다.The present invention relates to a method for restoring damage to flooring, and in particular, to a method for restoring damage to flooring made of stone, which allows quick restoration of damaged parts at low cost while providing reinforcement to prevent further damage to flooring made of stone.

바닥재는 주거 공간의 바탕이자 많은 면적을 차지하는 스타일을 결정 짓는 주요한 인테리어 자재이다. 일반적으로 바닥재는 마루와 시트, 타일, 석재, 인조석재 등이 알려져 있다. 이 중 석재로 제작된 바닥대리석은 보통 가격이 고가이기 때문에 파손이 발생되는 경우, 교체를 하게 되면 교체비용이 상당히 증가하게 된다. 물론 교체하는데 소요되는 공사 기간도 길어지게 된다. 따라서 파손을 복구하는데 비용을 줄이면서 공기를 단축할 수 있는 기술적방안이 요구된다.Flooring is a major interior material that determines the style of a residential space and occupies a large area. Generally, flooring materials such as flooring, sheets, tiles, stone, and artificial stone are known. Among these, floor marble made of stone is usually expensive, so if it is damaged, the replacement cost increases significantly. Of course, the construction period required for replacement will also be longer. Therefore, a technical solution is required to reduce the cost and shorten the period for repairing damage.

본 발명의 배경이 되는 기술로는 한국 등록특허 등록번호 제10-1475316호(특허문헌 1)로서, '바닥재 시공방법'이 알려져 있다. 이는 우레탄 탄성층과 세라믹층이 함께 형성되어서 탄성력이 증대될 수 있고, 최상층에 고경질의 탑코팅층을 형성하여 햇빛에 의한 자외선을 차단하여 고분자를 보호하면서 외부의 충격로부터 탄성층과 세라믹층의 파손을 방지할 수 있도록 한 것이다. 그러나 이 배경기술은 세라믹층이 파손될 경우, 이에 대한 복원 방안이 없다.As the technology behind the present invention, the 'flooring construction method' is known as Korean Patent Registration No. 10-1475316 (Patent Document 1). This is because the urethane elastic layer and the ceramic layer are formed together to increase elasticity, and by forming a high-hardness top coating layer on the top layer, it protects the polymer by blocking ultraviolet rays from sunlight and prevents damage to the elastic layer and ceramic layer from external impact. This was done to prevent. However, this background technology has no restoration plan if the ceramic layer is damaged.

본 발명의 배경이 되는 다른 기술로는 한국 등록특허 등록번호 제10-1255329호(특허문헌 2)로서, '콘크리트 구조물의 벽체 및 바닥 보수공법'가 제안되어 있다. 이는 콘크리트 구조물의 벽체 또는 바닥면이 갖는 균열 및 파손 부위 측 보수 시공에 있어 콘크리트와의 부착성과 수밀성을 향상시킬 수 있도록 하고 다양한 외부 환경요인에도 저항력을 높여 고점착성을 유지할 수 있도록 한 것이다. 그러나 이 배경기술은 보수재료를 도포한 후 도막층을 형성하여 균열 및 파손 부위를 보수할 수 있으나 바닥면 자체를 보강할 수 있는 방법이 없어 추가적인 바닥의 파손을 방지할 수 없다.Another technology that forms the background of the present invention is Korean Patent Registration No. 10-1255329 (Patent Document 2), which proposes a 'wall and floor repair method for concrete structures'. This is to improve adhesion to concrete and watertightness in repair work on cracks and damaged areas of the wall or floor of a concrete structure, and to maintain high adhesion by increasing resistance to various external environmental factors. However, this background technology can repair cracks and damaged areas by forming a coating layer after applying repair materials, but there is no way to reinforce the floor itself, so it cannot prevent additional damage to the floor.

한국 등록특허 등록번호 제10-1475316호Korean Patent Registration No. 10-1475316 한국 등록특허 등록번호 제10-1255329호Korean Patent Registration No. 10-1255329

본 발명은 석재로 제작된 바닥재의 추가적인 파손을 방지할 수 있는 보강을 실현하면서 파손 부분을 저비용으로 신속히 복원시킬 수 있도록 한 바닥재의 파손 복원 방법을 제공함에 그 목적이 있다.The purpose of the present invention is to provide a method for restoring damage to flooring made of stone, which allows quick restoration of damaged parts at low cost while providing reinforcement to prevent further damage to flooring made of stone.

본 발명의 적절한 실시 형태에 따른 바닥재의 파손 복원 방법은, 석재로 제작되어 바닥에 시공된 바닥재에서 발생된 들뜸, 균열, 파손 부분을 철거하는 단계와; 철거부분이 있는 일정 영역의 둘레를 따라 바닥재에 커팅 작업을 하여 급결제 주입홈통을 형성시켜 주는 단계와; 바닥재의 추가 파손을 방지하기 위해 급결제 주입홈통으로 급결제를 주입하여 파손부분을 갖는 바닥재의 하부 빈공간에 충진·경화시켜 해당 바닥재의 하면에 급결보강층을 형성시키는 단계; 복원제를 바닥재의 철거 부분에 메워 복원하는 단계와; 복원 부분에 광택이 이루어지도록 연마하는 단계;를 포함환 것을 특징으로 한다.A method of restoring damage to a flooring material according to a suitable embodiment of the present invention includes the steps of removing the lifting, cracking, and damaged portions generated in the flooring material made of stone and installed on the floor; A step of cutting the flooring material along the circumference of a certain area where the demolition part is located to form an accelerator injection trough; In order to prevent further damage to the flooring, injecting a quick-setting agent into the quick-setting agent injection trough to fill and harden the empty space at the bottom of the flooring having the damaged portion to form a quick-setting reinforcement layer on the lower surface of the flooring; Restoring the removed part of the flooring by filling it with a restoration agent; It is characterized in that it includes a step of polishing the restored part to achieve gloss.

또한, 급결제는 접착성 수지와 경화제 및 조색제를 혼합하여 제조되고, 조색제는 바닥재의 색상과 일치하는 것을 특징으로 한다.In addition, the quick setting agent is manufactured by mixing an adhesive resin, a hardener, and a coloring agent, and the coloring agent is characterized in that it matches the color of the flooring material.

또한, 급결제는 급결제 주입홈통까지 도달하도록 충진하여 경화시키는 것을 특징으로 한다.In addition, the accelerator is filled and hardened so that it reaches the accelerator injection trough.

또한, 복원제는 접착성 수지와 경화제 및 조색제를 혼합하여 제조되고, 조색제는 바닥재의 색상과 일치하는 것을 특징으로 한다.In addition, the restoration agent is manufactured by mixing an adhesive resin, a hardener, and a coloring agent, and the coloring agent is characterized in that it matches the color of the flooring material.

본 발명에 따른 바닥재의 파손 복원 방법은, 바닥재와 동일한 조색제가 함유된 복원제를 사용하여 파손 부분을 흔적없이 원상태로 복원시킬 수 있다. 또한 복원 준비 과정에서 바닥재의 하부에 급결제를 충진시키는 공정으로 인해 해당 바닥재는 보강이 이루어져 추가적인 파손을 방지할 수 있다. 또한 파손된 바닥대리석을 교체하는 것이 아니라 파손 부분만을 복원시키는 방법이기 때문에 상대적으로 보수 비용이 저렴하여 사용자의 경제적 부담을 줄일 수 있다.The method of restoring damage to flooring according to the present invention can restore damaged parts to their original state without traces by using a restoration agent containing the same coloring agent as that of the flooring. In addition, during the restoration preparation process, the process of filling the lower part of the floor with a quick-setting agent strengthens the floor and prevents further damage. In addition, since it is a method of restoring only the damaged part rather than replacing the damaged floor marble, the repair cost is relatively low, reducing the financial burden on the user.

본 명세서에서 첨부되는 다음의 도면들은 본 발명의 바람직한 실시 예를 예시하는 것이며, 발명의 상세한 설명과 함께 본 발명의 기술사상을 더욱 이해시키는 역할을 하는 것이므로, 본 발명은 첨부한 도면에 기재된 사항에만 한정되어서 해석되어서는 아니 된다.
도 1은 본 발명의 실시 예에 따른 바닥재의 파손 복원 과정의 흐름도.
도 2는 본 발명의 실시 예에 따른 바닥재의 파손 복원 과정에서의 각 단면도.
도 3 내지 도 6은 본 발명의 실시 예에 따른 바닥재의 파손 복원 과정에서 나타나는 바닥재의 상태를 나타내는 사진.
The following drawings attached to this specification illustrate preferred embodiments of the present invention, and serve to further understand the technical idea of the present invention along with the detailed description of the invention. Therefore, the present invention is limited to the matters described in the attached drawings. It should not be interpreted as limited.
1 is a flowchart of a process for restoring damage to flooring according to an embodiment of the present invention.
Figure 2 is a cross-sectional view of each section in the process of restoring damage to flooring according to an embodiment of the present invention.
3 to 6 are photographs showing the state of the flooring that appears during the restoration process of damage to the flooring according to an embodiment of the present invention.

아래에서 본 발명은 첨부된 도면에 제시된 실시 예를 참조하여 상세하게 설명이 되지만 제시된 실시 예는 본 발명의 명확한 이해를 위한 예시적인 것으로 본 발명은 이에 제한되지 않는다.Below, the present invention will be described in detail with reference to embodiments shown in the attached drawings, but the presented embodiments are illustrative for a clear understanding of the present invention, and the present invention is not limited thereto.

본 실시 예에 따른 바닥재(10)의 파손 복원 방법을 순차적으로 설명한다.A method of restoring damage to the flooring material 10 according to this embodiment will be sequentially described.

먼저, 도 1과 같이 바닥에 시공된 바닥재(10)에서 발생된 들뜸 부분이나 균열 부분 또는 파손 부분을 철거(제거)하는 단계(S11)를 갖는다.(도 2의 (가) 참조) 철거는 전동공구에 장착시킨 각종 절삭공구를 이용하여 이루어질 수 있다.First, there is a step (S11) of demolishing (removing) the lifted part, cracked part, or damaged part that occurred in the flooring material 10 installed on the floor as shown in FIG. 1 (see (a) of FIG. 2). The demolition is performed by electric power. This can be done using various cutting tools mounted on the tool.

여기서, 바닥재(10)는 석재로 제작된 것으로 대리석, 점판암, 규암, 사문암, 인조석 등등이 될 수 있다. 본 실시 예에서 바닥재(10)는 바닥대리석으로 사각 형태로 제작되어 있으나 이러한 형태에 본 발명이 제한되는 것은 아니다.Here, the flooring material 10 is made of stone and may be marble, slate, quartzite, serpentine, artificial stone, etc. In this embodiment, the flooring material 10 is made of floor marble and has a square shape, but the present invention is not limited to this shape.

그 다음, 파손 부분(철거 부분)(101)이 있는 일정 영역의 둘레를 따라 바닥재(10)에 커팅 작업을 하여 급결제 주입홈통(12)을 형성시켜 주는 단계(S12)를 갖는다.(도 2의 (나) 및 도 3 참조) 급결제 주입홈통(12)은 새롭게 형성되거나 기존의 줄눈을 따라 형성될 수 있다. 커팅 작업은 전동공구에 장착시킨 커팅휠 또는 드릴을 이용할 수 있다.Next, there is a step (S12) in which the quick-setting agent injection trough 12 is formed by cutting the flooring material 10 along the circumference of a certain area where the damaged part (removed part) 101 is located (FIG. 2). (b) and FIG. 3) The quick-setting agent injection trough 12 may be newly formed or may be formed along an existing joint. Cutting work can be done using a cutting wheel or drill mounted on a power tool.

그 다음, 바닥재(10)의 추가 파손을 방지하기 위해 급결제 주입홈통(12)으로 급결제(14)를 주입하는 단계(S13)를 갖는다.(도 2의 (다) 및 도 4 참조) 급결제(14)의 주입은 중력식 또는 압력식 방법을 적용할 수 있다.Next, in order to prevent further damage to the flooring 10, there is a step (S13) of injecting the quick-setting agent 14 into the quick-setting agent injection trough 12 (see Figure 2 (C) and Figure 4). Injection of payment 14 can be done by gravity or pressure method.

이같이 급결제(14)가 급결제 주입홈통(12)을 통해 주입되면, 바닥재(10)의 하부 빈공간에 급결제(14)가 충진된다. 이 급결제(14)가 경화되면 해당 바닥재(10)의 하면에 급결보강층(11)이 형성·접합되어 바닥재(10)의 보강이 이루어진다. 이때 도 5와 같이 급결제 주입홈통(12)에도 급결제(14)가 메워지도록 한다. 이같이 보수 대상인 바닥재(10)의 하부에 급결제(14)가 채워져 신속히 보강됨으로써 추가적인 바닥재(10)의 파손을 효과적으로 방지할 수 있다. 급결제(14)는 접착성 수지와 경화제 및 조색제를 혼합하여 제조된다. 이때 경화제의 함량을 조절하여 급결제(14)의 경화시간을 조절할 수 있다. 급결제 주입홈통(12)의 형성 흔적을 없애기 위해 급결제에 사용된 조색제는 바닥재(10)의 색상과 일치하는 것이 좋다.When the accelerator 14 is injected through the accelerator injection trough 12 in this way, the empty space in the lower part of the flooring material 10 is filled with the accelerator 14. When this quick-setting agent 14 hardens, a quick-setting reinforcement layer 11 is formed and bonded to the lower surface of the flooring material 10, thereby reinforcing the flooring material 10. At this time, as shown in FIG. 5, the quick-setting agent injection trough 12 is also filled with the quick-setting agent 14. In this way, the lower part of the flooring material 10 to be repaired is filled with the quick-setting agent 14 and is quickly reinforced, thereby effectively preventing further damage to the flooring material 10. The quick setting agent 14 is manufactured by mixing an adhesive resin, a hardener, and a coloring agent. At this time, the curing time of the quick setting agent 14 can be adjusted by adjusting the content of the curing agent. In order to eliminate traces of formation of the quick-setting agent injection trough 12, the coloring agent used in the quick-setting agent should match the color of the flooring material 10.

이와 같이 본 발명은 파손된 바닥재(10)의 하부에 급결제(14)를 통해 해당 바닥재(10)를 보강하기 때문에 복원 중 또는 복원 후에 해당하는 바닥재(10)의 추가적인 파손을 방지할 수 있다.In this way, since the present invention reinforces the damaged flooring 10 through the quick-setting agent 14 at the bottom of the damaged flooring 10, additional damage to the flooring 10 during or after restoration can be prevented.

그 다음, 복원제(16)를 바닥재(10)의 철거 부분에 메워 복원하는 단계(S14)를 갖는다.(도 2의 (라) 및 도 5 참조) 복원제(16)는 접착성 수지와 경화제 및 조색제를 혼합하여 제조되고, 조색제는 바닥재(10)의 색상과 일치하는 것이 바람직하다.Next, there is a step (S14) of restoring the removed part of the flooring 10 by filling it with the restoration agent 16 (see FIGS. 2(D) and 5). The restoration agent 16 is composed of an adhesive resin and a hardener. and a coloring agent, and the coloring agent preferably matches the color of the flooring (10).

급결제(14)와 복원제(16)에 사용된 접착성 수지는 본 실시 예에서 폴리에스테르 수지를 사용하였으나 본 발명은 이러한 접착성 수지에 한정되는 것은 아니다.The adhesive resin used in the quick-setting agent 14 and the restoration agent 16 is polyester resin in this example, but the present invention is not limited to this adhesive resin.

이같이 복원제(16)는 접착성 수지에 의해 파손 부분이 메워지게 되며, 경화제에 의해 경화되어 파손 부분이 바닥재(10)와 동일한 색상을 갖고 도 7과 같이 일체되어 복원됨으로써 우수한 내구성을 갖게 된다.In this way, the restoration agent 16 fills the damaged part with an adhesive resin, and is hardened with a curing agent, so that the damaged part has the same color as the flooring material 10 and is restored as one as shown in FIG. 7, thereby providing excellent durability.

그 다음, 도 6과 같이 바닥재(10)의 복원 부분에 광택이 이루어지도록 주지의 연마기를 통해 연마하는 단계(S15)를 갖는다. 이같이 연마를 통해 바닥재(10)가 가지고 있던 광택이 복원 부분에도 나타나 파손의 흔적을 찾아볼 수 없는 전체적으로 일체된 마감을 얻을 수 있다.Next, as shown in FIG. 6, there is a step (S15) of polishing the restored portion of the flooring 10 using a known polishing machine so that it becomes glossy. Through this polishing, the gloss of the flooring material 10 appears in the restored portion, making it possible to obtain an overall integrated finish with no traces of damage.

지금까지 본 발명은 제시된 실시 예를 참조하여 상세하게 설명이 되었지만 이 분야에서 통상의 지식을 가진 자는 제시된 실시 예를 참조하여 본 발명의 기술적 사상을 벗어나지 않는 범위에서 다양한 변형 및 수정 발명을 만들 수 있을 것이다. 본 발명은 이와 같은 변형 및 수정 발명에 의하여 제한되지 않으며 다만 아래에 첨부된 청구범위에 의하여 제한된다. So far, the present invention has been described in detail with reference to the presented embodiments, but those skilled in the art can make various variations and modifications without departing from the technical spirit of the present invention with reference to the presented embodiments. will be. The present invention is not limited by such variations and modifications, but is limited by the claims appended below.

10: 바닥재
11: 급결보강층
12: 급결제 주입홈통
14: 급결제
16: 복원제
10: Flooring
11: Rapid reinforcement layer
12: Quick-setting agent injection trough
14: Urgent payment
16: Restorer

Claims (4)

석재로 제작되어 바닥에 시공된 바닥재(10)에서 발생된 들뜸, 균열, 파손 부분(101)을 철거하는 단계(S11)와;
철거부분이 있는 일정 영역의 둘레를 따라 바닥재(10)에 커팅 작업을 하여 급결제 주입홈통(12)을 형성시켜 주는 단계(S12)와;
바닥재(10)의 추가 파손을 방지하기 위해 급결제 주입홈통(12)으로 급결제(14)를 주입하여 파손부분을 갖는 바닥재(10)의 하부 빈공간에 충진·경화시켜 해당 바닥재(10)의 하면에 급결보강층(11)을 형성시키는 단계(S13)와;
복원제(16)를 바닥재(10)의 철거 부분에 메워 복원하는 단계(S14)와;
복원 부분에 광택이 이루어지도록 연마하는 단계(S15);를 포함환 것을 특징으로 하는 바닥재의 파손 복원 방법.
A step (S11) of removing the lifted, cracked, or damaged portion 101 that occurred in the flooring material 10 made of stone and installed on the floor;
A step (S12) of forming an accelerator injection trough 12 by cutting the flooring material 10 along the perimeter of a certain area where the demolition part is located;
In order to prevent further damage to the flooring material (10), the quick-setting agent (14) is injected into the quick-setting agent injection trough (12) to fill and harden the empty space at the bottom of the flooring material (10) with the damaged part, thereby restoring the flooring material (10). Forming a rapid reinforcement layer 11 on the lower surface (S13);
A step (S14) of restoring the removed part of the flooring 10 by filling it with a restoration agent 16;
A method of restoring damage to flooring, comprising the step of polishing the restored portion to a shine (S15).
제 1항에 있어서,
급결제(14)는 접착성 수지와 경화제 및 조색제를 혼합하여 제조되고, 조색제는 바닥재(10)의 색상과 일치하는 것을 특징으로 하는 바닥재의 파손 복원 방법.
According to clause 1,
A method of restoring damage to flooring, wherein the quick-setting agent (14) is manufactured by mixing an adhesive resin, a hardener, and a coloring agent, and the coloring agent matches the color of the flooring (10).
제 2항에 있어서,
급결제(14)는 급결제 주입홈통(12)까지 도달하도록 충진하여 경화시키는 것을 특징으로 하는 바닥재의 파손 복원 방법.
According to clause 2,
A method of restoring damage to flooring, characterized in that the quick-setting agent (14) is filled and hardened so that it reaches the quick-setting agent injection trough (12).
제 1항에 있어서,
복원제(16)는 접착성 수지와 경화제 및 조색제를 혼합하여 제조되고, 조색제는 바닥재(10)의 색상과 일치하는 것을 특징으로 하는 바닥재의 파손 복원 방법.
According to clause 1,
A method of restoring damage to flooring, wherein the restoration agent (16) is manufactured by mixing an adhesive resin, a hardener, and a coloring agent, and the coloring agent matches the color of the flooring (10).
KR1020220030008A 2022-03-10 2022-03-10 Damage restoration method of floor board KR20230133018A (en)