Prior art keywords
epoxy
layer
leveling
construction method
abrasive
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202011346553.4A
Other languages
Chinese (zh)
Inventor
崔佳宇
袁后鹏
陈骏
李西夏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Baoye Architectural Decoration Co ltd
Shanghai Baoye Group Corp Ltd
Original Assignee
Shanghai Baoye Architectural Decoration Co ltd
Shanghai Baoye Group Corp Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Baoye Architectural Decoration Co ltd, Shanghai Baoye Group Corp Ltd filed Critical Shanghai Baoye Architectural Decoration Co ltd
Priority to CN202011346553.4A priority Critical patent/CN112502436A/en
Publication of CN112502436A publication Critical patent/CN112502436A/en
Pending legal-status Critical Current

Links

Images

Classifications

    • EFIXED CONSTRUCTIONS
    • E04BUILDING
    • E04GSCAFFOLDING; FORMS; SHUTTERING; BUILDING IMPLEMENTS OR AIDS, OR THEIR USE; HANDLING BUILDING MATERIALS ON THE SITE; REPAIRING, BREAKING-UP OR OTHER WORK ON EXISTING BUILDINGS
    • E04G21/00Preparing, conveying, or working-up building materials or building elements in situ; Other devices or measures for constructional work
    • EFIXED CONSTRUCTIONS
    • E04BUILDING
    • E04FFINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS
    • E04F15/00Flooring
    • E04F15/12Flooring or floor layers made of masses in situ, e.g. seamless magnesite floors, terrazzo gypsum floors
    • EFIXED CONSTRUCTIONS
    • E04BUILDING
    • E04FFINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS
    • E04F15/00Flooring
    • E04F15/12Flooring or floor layers made of masses in situ, e.g. seamless magnesite floors, terrazzo gypsum floors
    • E04F15/14Construction of joints, e.g. dividing strips

Landscapes

  • Engineering & Computer Science (AREA)
  • Architecture (AREA)
  • Civil Engineering (AREA)
  • Structural Engineering (AREA)
  • Mechanical Engineering (AREA)
  • Road Repair (AREA)

Abstract

The application discloses a construction method of an epoxy millstone indoor ground, which comprises the following steps: prefabricating, namely prefabricating a plurality of epoxy millstone slabs by adopting raw materials for manufacturing the epoxy millstone terrace. And cleaning the structural layer. And a leveling step, namely paving a leveling layer on the cleaned structural layer. And paving, namely adhering the epoxy abrasive plates on the leveling layer, and filling expansion joints among the epoxy abrasive plates adhered on the leveling layer to obtain the epoxy abrasive layer. And a decoration step, coating the raw materials on the epoxy abrasive layer to obtain the decoration layer. The repairing method of the terrace manufactured by the construction method is simple, the terrace is cut along the expansion joint, the epoxy abrasive plate where the part needing to be repaired is located is directly taken out, the epoxy abrasive plate with the same specification is replaced, and then after a series of treatments such as expansion joint treatment, epoxy resin coating, polishing and curing agent coating are carried out, traces are invisible.

Description

Construction method of epoxy millstone indoor ground
Technical Field
The application relates to the field of architectural decoration and finishing engineering, in particular to a construction method of epoxy millstone indoor ground.
Background
The damage caused by different reasons in the using process of the epoxy grindstone needs the later repair, and the common repair method of the epoxy grindstone is a point repair method and an integral covering repair method. The later stage of the point repairing method can cause repairing traces, and the overall covering and repairing cost is too high.
Content of application
The application provides a construction method of epoxy millstone indoor ground, which can shorten the construction period and avoid the problem of difficulty in later-stage repair.
In a first aspect, an embodiment of the present application provides a construction method for an epoxy grindstone indoor floor, including the following steps: prefabricating, namely prefabricating a plurality of epoxy millstone slabs by adopting raw materials for manufacturing the epoxy millstone terrace. And cleaning the structural layer. And a leveling step, namely paving a leveling layer on the cleaned structural layer. And paving, namely adhering the epoxy abrasive plates on the leveling layer, and filling expansion joints among the epoxy abrasive plates adhered on the leveling layer to obtain the epoxy abrasive layer. And a decoration step, coating the raw materials on the epoxy abrasive layer to obtain the decoration layer.
In some embodiments, in the leveling step, the expansion joint is disposed on the leveling layer, and the expansion joint is filled.
In some embodiments, in the leveling step, the interface agent is applied to the leveling layer filled with the expansion joint.
In some of these embodiments, the step of laying down includes applying an interfacial agent to the epoxy abrasive layer.
In some embodiments, the construction method further comprises the following steps: and finishing, namely grinding and polishing the decorative layer.
In some embodiments, the construction method further comprises the following steps: and curing, namely coating a curing agent on the polished decorative layer.
In some of these embodiments, the laying step involves applying an adhesive to each epoxy stone slab and then adhering each epoxy stone slab to the screed.
In some embodiments, in the laying step, the epoxy abrasive slabs adhered to the leveling layer are hammered and then the expansion joints between the epoxy abrasive slabs adhered to the leveling layer are filled.
In some of these embodiments, the laying step uses a rubber hammer to hammer the individual epoxy millstone plates adhered to the screed.
In some embodiments, in the laying step, the adjacent hammered epoxy abrasive plates are fixed by using clips, after a preset time, the clips are detached, and then the expansion joints between the epoxy abrasive plates glued on the leveling layer are filled.
According to the construction method of the indoor ground of the epoxy millstone provided by the embodiment of the application, the construction method comprises the following steps: prefabricating, namely prefabricating a plurality of epoxy millstone slabs by adopting raw materials for manufacturing the epoxy millstone terrace. And cleaning the structural layer. And a leveling step, namely paving a leveling layer on the cleaned structural layer. And paving, namely adhering the epoxy abrasive plates on the leveling layer, and filling expansion joints among the epoxy abrasive plates adhered on the leveling layer to obtain the epoxy abrasive layer. And a decoration step, coating the raw materials on the epoxy abrasive layer to obtain the decoration layer. The repairing method of the terrace manufactured by the construction method is simple, the terrace is cut along the expansion joint, the epoxy abrasive plate where the part needing to be repaired is located is directly taken out, the epoxy abrasive plate with the same specification is replaced, and then after a series of treatments such as expansion joint treatment, epoxy resin coating, polishing and curing agent coating are carried out, traces are invisible.
Drawings
In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings used in the description of the embodiments or the prior art will be briefly described below, it is obvious that the drawings in the following description are only some embodiments of the present application, and other drawings can be obtained by those skilled in the art without creative efforts.
Fig. 1 is a schematic flow chart of a construction method in an embodiment of the present application.
Detailed Description
In order to make the objects, technical solutions and advantages of the present application more apparent, the present application is described in further detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the present application and are not intended to limit the present application.
Referring to fig. 1, an embodiment of the present application provides a construction method of an epoxy millstone indoor floor, including the following steps: prefabricating, namely prefabricating a plurality of epoxy millstone slabs by adopting raw materials for manufacturing the epoxy millstone terrace. And cleaning the structural layer. And a leveling step, namely paving a leveling layer on the cleaned structural layer. And paving, namely adhering the epoxy abrasive plates on the leveling layer, and filling expansion joints among the epoxy abrasive plates adhered on the leveling layer to obtain the epoxy abrasive layer. And a decoration step, coating the raw materials on the epoxy abrasive layer to obtain the decoration layer.
The raw materials can be epoxy resin and crystal sand to increase the surface adhesion.
The cleaning step may specifically be: and cleaning the ash layer of the structural layer to prevent the leveling layer from cracking and hollowing.
The leveling layer is arranged for the purpose that: prevent cracking and is moisture-proof. The screed-coat can specifically be the mortar bed course of making level that contains the admixture, need not the maintenance way of old-fashioned such as watering after the construction, nevertheless need to avoid sunshine to penetrate directly and cross the hall wind, if sunshine and cross the hall wind inevitable, then can lay the appropriate maintenance of PE anti-light film when the surface course construction process links up not last to rationally make constructor carry out next process construction.
In the leveling step, an expansion joint is arranged on the leveling layer and is filled. Because the whole surface layer area is too big, the expansion and contraction causes the leveling layer to crack, arch and hollow, therefore, in order to avoid the above problems, the expansion joint is arranged.
In the leveling step, the interface agent is smeared on the leveling layer filled with the expansion joint. The arrangement enables the epoxy abrasive plate to be bonded with the leveling layer better. Before laying the epoxy grindstone, the leveling layer must be comprehensively detected and various professional treatments are performed, so that the epoxy grindstone layer can be laid.
In the laying step, each epoxy abrasive plate may have a size of 800 × 800. The gluing of the epoxy abrasive plates is carried out according to construction drawings.
In the laying step, the adhesive is coated on each epoxy abrasive plate, and then each epoxy abrasive plate is adhered on the leveling layer. The coating area of the adhesive is the same as that of the epoxy abrasive plate. Before smearing, the epoxy millstone plate must be cleaned to ensure the surface, the side surface and the paved surface to be clean and pollution-free. In the gluing process, the high elastic line is calibrated, a standard block/similar standard sample must be placed, the standard block/similar standard sample is placed at the intersection of the cross lines, the cross lines are installed diagonally, and the flatness is guaranteed to be within 2m +/-3 mm.
In the laying step, the epoxy abrasive plates adhered to the leveling layer are hammered into solid, and then expansion joints among the epoxy abrasive plates adhered to the leveling layer are filled.
In the laying step, a rubber hammer is used for hammering each epoxy abrasive plate adhered on the leveling layer.
In the laying step, the adjacent hammered epoxy abrasive plates are fixed by the clips, after the preset time (72 h can be used), the clips are detached, and then expansion joints among the epoxy abrasive plates adhered to the leveling layer are filled. Before the clamp is disassembled, a shovel is used for scratching out the excessive ash in the ash gap. After the whole gluing process is finished, pedestrians cannot step on the adhesive in 24h, and the adhesive can walk after 72h to fill the expansion joint and the like.
In the laying step, the interface agent is smeared on the epoxy abrasive layer. The interface agent in the paving step and the interface agent in the leveling step are the same interface agent.
The construction method also comprises the following steps: and finishing, namely grinding and polishing the decorative layer. The finishing step may specifically be: and checking the flatness of the site, properly polishing the workpiece which does not meet the requirement, and assembling a hexagonal grinding head (diamond grinding head) with a vacuum low-speed grinding machine for trial grinding before polishing to ensure that the ground dust has no roll adhered to the grinding head and has no blackening phenomenon. The resin grinding head can be assembled with a vacuum grinder for polishing, the polishing is used for eliminating slight grinding marks left during grinding/scratching in the previous process, and the ground floor surface and the aggregate texture of the stone are more uniform, fine, smooth and clean and have reflection.
The construction method also comprises the following steps: and curing, namely coating a curing agent on the polished decorative layer. The curing step may specifically be: adopt and seal the curing agent, carry out the decorative layer and seal the curing agent and handle, seal the maintenance to the decorative layer, prevent that other relevant professionals from getting into the terrace maintenance region when the terrace surface curing agent is not completely solidified, avoid polluting the decorative layer, influence the terrace after the completion and look and feel the effect.
The arrangement of the expansion joint in the leveling step or the arrangement of the expansion joint in the laying step is carried out according to the construction drawing. And regardless of the filling expansion joint in the step of making level, the filling expansion joint in still the step of laying can all specifically be: firstly, the expansion joint is straightly paid off to cut an inclined plane, the depth is about 1-3cm, if the expansion joint is not reserved on site and needs to be kept, the depth of 3-5cm is needed to be cut, then mortar or epoxy millstone slabs on an insecure leveling layer on the joint edge are removed, then dust absorption bottoming repair is carried out, after the repair is finished, the inclined plane is paid off to cut, masking paper is pasted on the two sides of the expansion joint, a caulking agent is filled along the expansion joint by a glue gun, finally a scraping blade is used for uniformly smearing along the expansion joint downwards by 45 degrees, and meanwhile, expansion joint marks are made on construction drawings. Wherein, according to the construction specification, an expansion joint is reserved generally at 6X 6 m.
The joint mixture of the leveling layer and the joint mixture of the epoxy abrasive layer are respectively corresponding special joint mixtures. After the surface of the leveling layer is cleaned, the adhesive force of the epoxy grindstone terrace is determined by solid, non-laitance, solid and clear textures.
The same or similar reference numerals in the drawings of the present embodiment correspond to the same or similar components; in the description of the present application, it is to be understood that if there is an orientation or positional relationship indicated by the terms "upper", "lower", "left", "right", etc. based on the orientation or positional relationship shown in the drawings, it is only for convenience of description and simplification of description, but it is not intended to indicate or imply that the referred device or element must have a specific orientation, be constructed in a specific orientation, and be operated, and therefore, the terms describing the positional relationship in the drawings are only for illustrative purposes and are not to be construed as limitations of the present patent, and specific meanings of the above terms may be understood by those skilled in the art according to specific situations.
The above description is only exemplary of the present application and should not be taken as limiting the present application, as any modification, equivalent replacement, or improvement made within the spirit and principle of the present application should be included in the protection scope of the present application.

Claims (10)

1. The construction method of the epoxy millstone indoor ground is characterized by comprising the following steps:
prefabricating, namely prefabricating a plurality of epoxy millstone slabs by adopting raw materials for manufacturing the epoxy millstone terrace;
cleaning, namely cleaning the structural layer;
a leveling step, namely paving a leveling layer on the cleaned structural layer;
paving, namely gluing the epoxy abrasive plates on the leveling layer, and filling expansion joints among the epoxy abrasive plates glued on the leveling layer with glue to obtain an epoxy abrasive layer;
and a decoration step, coating the raw materials on the epoxy abrasive layer to obtain the decoration layer.
2. The construction method according to claim 1,
and in the leveling step, an expansion joint is arranged on the leveling layer and is filled.
3. The construction method according to claim 2,
in the leveling step, an interface agent is smeared on the leveling layer filled with the expansion joint.
4. The construction method according to claim 1,
in the laying step, an interface agent is smeared on the epoxy abrasive layer.
5. The construction method according to claim 1, further comprising the steps of:
and finishing, namely grinding and polishing the decorative layer.
6. The construction method according to claim 5, further comprising the steps of:
and curing, namely coating a curing agent on the polished decorative layer.
7. The construction method according to claim 1,
in the laying step, the adhesive is smeared on each epoxy abrasive plate, and then each epoxy abrasive plate is adhered on the leveling layer.
8. The construction method according to claim 1,
in the laying step, the epoxy abrasive plates adhered to the leveling layer are hammered with glue, and then expansion joints among the epoxy abrasive plates adhered to the leveling layer are filled with glue.
9. The construction method according to claim 8,
in the laying step, a rubber hammer is adopted to hammer the epoxy millstone plates adhered to the leveling layer.
10. The construction method according to claim 8,
in the laying step, clamps are adopted to fix the adjacent hammered epoxy abrasive slabs, after the preset time, the clamps are disassembled, and then expansion joints among the epoxy abrasive slabs adhered to the leveling layer are filled with glue.
CN202011346553.4A 2020-11-26 2020-11-26 Construction method of epoxy millstone indoor ground Pending CN112502436A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN202011346553.4A CN112502436A (en) 2020-11-26 2020-11-26 Construction method of epoxy millstone indoor ground

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN202011346553.4A CN112502436A (en) 2020-11-26 2020-11-26 Construction method of epoxy millstone indoor ground

Publications (1)

Publication Number Publication Date
CN112502436A true CN112502436A (en) 2021-03-16

Family

ID=74966129

Family Applications (1)

Application Number Title Priority Date Filing Date
CN202011346553.4A Pending CN112502436A (en) 2020-11-26 2020-11-26 Construction method of epoxy millstone indoor ground

Country Status (1)

Country Link
CN (1) CN112502436A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN113356374A (en) * 2021-06-23 2021-09-07 上海典跃建材科技有限公司 Structural deformation joint of gold grindstone

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110565899A (en) * 2019-09-17 2019-12-13 苏州金螳螂建筑装饰股份有限公司 leveling structure and leveling method for epoxy gold grindstone terrace base layer
CN110821117A (en) * 2019-11-11 2020-02-21 湖南梅克雷薇新材料科技有限公司 Tile leveling structure and tile leveling structure construction process
CN210508238U (en) * 2019-08-15 2020-05-12 四川天宜石油化工工程有限公司 Seepage-proofing floor expansion joint filling structure and expansion joint structure

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN210508238U (en) * 2019-08-15 2020-05-12 四川天宜石油化工工程有限公司 Seepage-proofing floor expansion joint filling structure and expansion joint structure
CN110565899A (en) * 2019-09-17 2019-12-13 苏州金螳螂建筑装饰股份有限公司 leveling structure and leveling method for epoxy gold grindstone terrace base layer
CN110821117A (en) * 2019-11-11 2020-02-21 湖南梅克雷薇新材料科技有限公司 Tile leveling structure and tile leveling structure construction process

Non-Patent Citations (4)

* Cited by examiner, † Cited by third party
Title
北京市第四建筑工程公司: "铺设预制水磨石板块地面施工工艺", 《建筑技术》 *
施国璋: "改进铺贴予制水磨石板地坪施工工艺的尝试", 《建筑施工》 *
林木发: "预制水磨石地面的技术创新", 《建筑施工》 *
汝宗林: "现制环氧基水磨石地坪施工工艺", 《石材》 *

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN113356374A (en) * 2021-06-23 2021-09-07 上海典跃建材科技有限公司 Structural deformation joint of gold grindstone

Similar Documents

Publication Publication Date Title
CN111997303B (en) Cast-in-place inorganic artificial terrazzo terrace and construction method thereof
US7591967B2 (en) Method for the aesthetic surface treatment of a monolithic concrete floor and product of the method
CN110284724B (en) GRC plate repairing method
US20100005743A1 (en) Flexible Cement Veneer
CN106884536A (en) A kind of construction method of compound terrace
CN107152145A (en) A kind of stone material flooring construction method
CN108343213A (en) A kind of underground parking garage epoxy resin mortar abrasion-proof terrace and construction method
CN112502436A (en) Construction method of epoxy millstone indoor ground
CN111962349A (en) Wear-resistant concrete ground construction process
CN104831926A (en) Paving method of joggle type block-shaped surface building floor
CN111962348A (en) Concrete floor construction process
CN216921186U (en) Ground structure of golden millstone
US20070044685A1 (en) Mosaic marble flooring and driveway system
CN111255191A (en) Semi-pre-pasted ceramic tile and paving method thereof
CN112554501B (en) Special seam beautifying strip for building material and construction method thereof
KR100858347B1 (en) Method for carrying out floor board of structure andfloor board of structure carried out by its method
CN211949245U (en) Roof stone flashing structure
CN214169786U (en) Terrazzo floor used in shopping center
CN114575552A (en) Ceramic tile close joint paving method
US8920067B2 (en) Concrete decorative inlay process
CN114704047B (en) Integral ground construction process for inorganic grinding stone
CN220686599U (en) Facing material paving structure
CN221321607U (en) Factory building ground coating structure
JP4395126B2 (en) Paving method
JPH084265A (en) Executing method of non-skid pavement of concrete or mortar bed surface

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
SE01 Entry into force of request for substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication

Application publication date: 20210316

RJ01 Rejection of invention patent application after publication