JPS6351051B2 - - Google Patents
Info
- Publication number
- JPS6351051B2 JPS6351051B2 JP59121910A JP12191084A JPS6351051B2 JP S6351051 B2 JPS6351051 B2 JP S6351051B2 JP 59121910 A JP59121910 A JP 59121910A JP 12191084 A JP12191084 A JP 12191084A JP S6351051 B2 JPS6351051 B2 JP S6351051B2
- Authority
- JP
- Japan
- Prior art keywords
- glass
- heat treatment
- skin layer
- temperature
- humidity
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Separation Using Semi-Permeable Membranes (AREA)
- Re-Forming, After-Treatment, Cutting And Transporting Of Glass Products (AREA)
- Glass Compositions (AREA)
- Catalysts (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59121910A JPS614513A (ja) | 1984-06-15 | 1984-06-15 | 多孔質ガラス膜の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59121910A JPS614513A (ja) | 1984-06-15 | 1984-06-15 | 多孔質ガラス膜の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS614513A JPS614513A (ja) | 1986-01-10 |
| JPS6351051B2 true JPS6351051B2 (enExample) | 1988-10-12 |
Family
ID=14822932
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP59121910A Granted JPS614513A (ja) | 1984-06-15 | 1984-06-15 | 多孔質ガラス膜の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS614513A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0347305U (enExample) * | 1989-09-08 | 1991-05-01 | ||
| JPH0347304U (enExample) * | 1989-09-08 | 1991-05-01 |
-
1984
- 1984-06-15 JP JP59121910A patent/JPS614513A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0347305U (enExample) * | 1989-09-08 | 1991-05-01 | ||
| JPH0347304U (enExample) * | 1989-09-08 | 1991-05-01 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS614513A (ja) | 1986-01-10 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CA1316311C (en) | Anisotropic membranes for gas separation | |
| JPH0529490B2 (enExample) | ||
| JPH0565211B2 (enExample) | ||
| FR2742071A1 (fr) | Procede d'elaboration de membranes de zeolithe supportee par du verre poreux | |
| US11766640B2 (en) | Method for preparing block copolymer hollow fiber membrane by melt spinning-stretching and selective swelling | |
| US4340408A (en) | High silica glass | |
| JPH02502354A (ja) | 透析膜の処理 | |
| US6187381B1 (en) | Process for preparing silica gel and process for producing dehumidifying element | |
| CN119746650B (zh) | 一种偶极非质子溶剂脱水用三层结构复合膜及其制备方法 | |
| JPS614513A (ja) | 多孔質ガラス膜の製造法 | |
| EP1682252A1 (en) | Titania composite membrane for water/alcohol separation, and preparation thereof | |
| KR102196707B1 (ko) | 에폭시 제조공정 부산물 회수용 투과증발 분리막의 제조방법 | |
| CN112569811A (zh) | 具有白酒催化过滤性能的聚间苯二甲酰间苯二胺混合基质膜及其制备与应用 | |
| JPS63100916A (ja) | ガス選択透過性膜の製造方法 | |
| JPH0139974B2 (enExample) | ||
| CN1068974A (zh) | 不对称聚酰亚胺气体分离膜的制备 | |
| JPS5849646A (ja) | 多孔質ガラスの耐アルカリ強化方法 | |
| CN109553636B (zh) | 一种有机硅氧烷混合环体除杂的方法 | |
| EP1151974B1 (de) | Oxidkeramischer Körper mit ultrafeinen Poren, Verfahren zu seiner Herstellung und Verwendung | |
| JPS644979B2 (enExample) | ||
| JPH0425226B2 (enExample) | ||
| RU1808346C (ru) | Способ получени полимерной мембраны | |
| JPS614519A (ja) | 無機ガス分離膜の製造方法 | |
| CN114835127A (zh) | 一种亲水型气凝胶的制备方法 | |
| JP2001205058A (ja) | 非対称性ポリイミド分離膜の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |