JPS6338841B2 - - Google Patents
Info
- Publication number
- JPS6338841B2 JPS6338841B2 JP57012670A JP1267082A JPS6338841B2 JP S6338841 B2 JPS6338841 B2 JP S6338841B2 JP 57012670 A JP57012670 A JP 57012670A JP 1267082 A JP1267082 A JP 1267082A JP S6338841 B2 JPS6338841 B2 JP S6338841B2
- Authority
- JP
- Japan
- Prior art keywords
- powder
- barium titanate
- metal
- temperature
- ptc
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Thermistors And Varistors (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1267082A JPS58130504A (ja) | 1982-01-29 | 1982-01-29 | 限流素子の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1267082A JPS58130504A (ja) | 1982-01-29 | 1982-01-29 | 限流素子の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58130504A JPS58130504A (ja) | 1983-08-04 |
| JPS6338841B2 true JPS6338841B2 (enExample) | 1988-08-02 |
Family
ID=11811802
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1267082A Granted JPS58130504A (ja) | 1982-01-29 | 1982-01-29 | 限流素子の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58130504A (enExample) |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS56169301A (en) * | 1980-06-02 | 1981-12-26 | Tohoku Metal Ind Ltd | Method of producing barium titanate semiconductor porcelain |
-
1982
- 1982-01-29 JP JP1267082A patent/JPS58130504A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS58130504A (ja) | 1983-08-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR101152453B1 (ko) | 반도체 자기 조성물 | |
| MacChesney et al. | Factors and mechanisms affecting the positive temperature coefficient of resistivity of barium titanate | |
| US3044968A (en) | Positive temperature coefficient thermistor materials | |
| US3373120A (en) | Semiconductive ceramic compositions with positive temperature coefficient of resistance | |
| JP5844507B2 (ja) | 半導体磁器組成物の製造方法及び半導体磁器組成物を用いたヒータ | |
| JPS6338841B2 (enExample) | ||
| JPH0230561B2 (enExample) | ||
| JPS6338842B2 (enExample) | ||
| JPH0590012A (ja) | 高電圧用バリスタ及びその製造方法 | |
| JP2623188B2 (ja) | バリスタ及びその製造方法 | |
| JP3286515B2 (ja) | 電圧非直線抵抗体 | |
| JP2872588B2 (ja) | 電圧非直線抵抗体の製造方法 | |
| JPS6338843B2 (enExample) | ||
| JPH0338802A (ja) | 正特性半導体磁器の製造方法 | |
| JP2000313661A (ja) | 放電プラズマ焼結体とその製造方法 | |
| Zhao et al. | The variable thermal sensitivity of strontium-lead titanate semiconducting ceramics | |
| JPH04265223A (ja) | 微粉体 | |
| JP2783559B2 (ja) | 酸化物系複合焼結体とその製造方法およびそれを用いた抵抗体 | |
| JPH08321404A (ja) | BaTiO3基サーミスター及びその製造方法 | |
| KR0147966B1 (ko) | 고온 ptc 써미스터용 세라믹 조성물 | |
| EP0444877A2 (en) | Electrical resistor element | |
| JPS59115503A (ja) | 限流素子の製造方法 | |
| JPS5827905A (ja) | 限流素子の製造方法 | |
| JPH02244602A (ja) | 限流素子の製造方法 | |
| JPS59101801A (ja) | 感温抵抗素子 |