JPS63171201A - 高い塗装艶消し性を有する塗装用金属板とその製造方法及び艶消し塗装金属板 - Google Patents
高い塗装艶消し性を有する塗装用金属板とその製造方法及び艶消し塗装金属板Info
- Publication number
- JPS63171201A JPS63171201A JP62001133A JP113387A JPS63171201A JP S63171201 A JPS63171201 A JP S63171201A JP 62001133 A JP62001133 A JP 62001133A JP 113387 A JP113387 A JP 113387A JP S63171201 A JPS63171201 A JP S63171201A
- Authority
- JP
- Japan
- Prior art keywords
- metal plate
- parts
- roll
- peak
- painting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Reduction Rolling/Reduction Stand/Operation Of Reduction Machine (AREA)
- Laser Beam Processing (AREA)
- Application Of Or Painting With Fluid Materials (AREA)
- Metal Rolling (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP62001133A JPS63171201A (ja) | 1987-01-08 | 1987-01-08 | 高い塗装艶消し性を有する塗装用金属板とその製造方法及び艶消し塗装金属板 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP62001133A JPS63171201A (ja) | 1987-01-08 | 1987-01-08 | 高い塗装艶消し性を有する塗装用金属板とその製造方法及び艶消し塗装金属板 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63171201A true JPS63171201A (ja) | 1988-07-15 |
| JPH0341241B2 JPH0341241B2 (enrdf_load_stackoverflow) | 1991-06-21 |
Family
ID=11492944
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP62001133A Granted JPS63171201A (ja) | 1987-01-08 | 1987-01-08 | 高い塗装艶消し性を有する塗装用金属板とその製造方法及び艶消し塗装金属板 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63171201A (enrdf_load_stackoverflow) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH05177210A (ja) * | 1992-01-08 | 1993-07-20 | Kawasaki Steel Corp | 耐プレスしわ性の良好なほうろう用薄鋼板 |
| JP2016010811A (ja) * | 2014-06-30 | 2016-01-21 | ミネベア株式会社 | 金属材料の表面処理方法及びこの方法を用いたフォースセンサ |
| JP2016114304A (ja) * | 2014-12-16 | 2016-06-23 | 昭和電工株式会社 | 沸騰伝熱部材およびこれを用いた沸騰冷却装置 |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS591636A (ja) * | 1982-06-26 | 1984-01-07 | Nisshin Steel Co Ltd | 鮮映性塗装めつき鋼板の製造方法 |
| JPS602156A (ja) * | 1983-06-13 | 1985-01-08 | Shuzo Nakazono | 豆乳の製造方法 |
-
1987
- 1987-01-08 JP JP62001133A patent/JPS63171201A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS591636A (ja) * | 1982-06-26 | 1984-01-07 | Nisshin Steel Co Ltd | 鮮映性塗装めつき鋼板の製造方法 |
| JPS602156A (ja) * | 1983-06-13 | 1985-01-08 | Shuzo Nakazono | 豆乳の製造方法 |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH05177210A (ja) * | 1992-01-08 | 1993-07-20 | Kawasaki Steel Corp | 耐プレスしわ性の良好なほうろう用薄鋼板 |
| JP2016010811A (ja) * | 2014-06-30 | 2016-01-21 | ミネベア株式会社 | 金属材料の表面処理方法及びこの方法を用いたフォースセンサ |
| US9649721B2 (en) | 2014-06-30 | 2017-05-16 | Minebea Co., Ltd. | Surface treatment method for metal material and force sensor |
| JP2016114304A (ja) * | 2014-12-16 | 2016-06-23 | 昭和電工株式会社 | 沸騰伝熱部材およびこれを用いた沸騰冷却装置 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0341241B2 (enrdf_load_stackoverflow) | 1991-06-21 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4798772A (en) | Steel sheets for painting and a method of producing the same | |
| US4795681A (en) | Steel sheets for painting and a method of producing the same | |
| JP6334536B2 (ja) | 金属材料、特に鋼材からなる平板製品、このような平板製品の使用、およびこのような平板製品を製造するためのロールと方法。 | |
| JPH0342961B2 (enrdf_load_stackoverflow) | ||
| JPH0338923B2 (enrdf_load_stackoverflow) | ||
| JPS63171201A (ja) | 高い塗装艶消し性を有する塗装用金属板とその製造方法及び艶消し塗装金属板 | |
| JPS6350488A (ja) | 塗装後鮮映性に優れた鋼板およびその製造方法 | |
| JPS63112086A (ja) | 鋼板圧延用ダルロ−ルの製造方法 | |
| JPH0339761B2 (enrdf_load_stackoverflow) | ||
| JPH044044B2 (enrdf_load_stackoverflow) | ||
| JPS6333593A (ja) | プレス成形性および塗装後鮮映性に優れるめつき鋼板 | |
| JPH10235414A (ja) | ダル仕上げ用ワークロールとその表面加工方法、ならびにつや消し性に優れたステンレス鋼板の製造方法 | |
| JPS63165011A (ja) | 模様鋼板及びその製造方法 | |
| JPS63256207A (ja) | 圧延用ロ−ル | |
| JPS63256203A (ja) | 艶消塗装用鋼板とその製造方法 | |
| JPH0448523B2 (enrdf_load_stackoverflow) | ||
| JP2019155474A (ja) | 圧延用ロール、表面処理鋼板、冷延鋼板およびそれらの製造方法 | |
| JP2724213B2 (ja) | 耐パウダリング性および塗装鮮映性の優れた合金化溶融亜鉛めっき鋼板 | |
| JPH02274853A (ja) | 成形性と塗装後鮮映性に優れた合金化溶融亜鉛めっき鋼板 | |
| JP2530970B2 (ja) | 塗装鮮映性及びプレス成形性の優れた鋼帯 | |
| JPH04333309A (ja) | 塗装鮮映性に優れた塗装用鋼板 | |
| JP2514692B2 (ja) | 塗装鮮映性の優れた鋼板及びその製造方法 | |
| JPH02274860A (ja) | 高機能表面粗度調整合金化溶融めっき鋼板の製造法 | |
| JPH02274857A (ja) | 高機能表面粗度調整合金化溶融めっき鋼板の製造法 | |
| JP2530968B2 (ja) | 塗装鮮映性及びプレス成形性の優れた鋼帯 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| S531 | Written request for registration of change of domicile |
Free format text: JAPANESE INTERMEDIATE CODE: R313531 |
|
| S533 | Written request for registration of change of name |
Free format text: JAPANESE INTERMEDIATE CODE: R313533 |
|
| R350 | Written notification of registration of transfer |
Free format text: JAPANESE INTERMEDIATE CODE: R350 |
|
| LAPS | Cancellation because of no payment of annual fees |