JPS6238426B2 - - Google Patents
Info
- Publication number
- JPS6238426B2 JPS6238426B2 JP10910879A JP10910879A JPS6238426B2 JP S6238426 B2 JPS6238426 B2 JP S6238426B2 JP 10910879 A JP10910879 A JP 10910879A JP 10910879 A JP10910879 A JP 10910879A JP S6238426 B2 JPS6238426 B2 JP S6238426B2
- Authority
- JP
- Japan
- Prior art keywords
- temperature
- less
- equivalent
- steel
- low
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Turbine Rotor Nozzle Sealing (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10910879A JPS5635754A (en) | 1979-08-29 | 1979-08-29 | Low temperature turbine blade steel and its heat treatment |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10910879A JPS5635754A (en) | 1979-08-29 | 1979-08-29 | Low temperature turbine blade steel and its heat treatment |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5635754A JPS5635754A (en) | 1981-04-08 |
JPS6238426B2 true JPS6238426B2 (enrdf_load_stackoverflow) | 1987-08-18 |
Family
ID=14501767
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP10910879A Granted JPS5635754A (en) | 1979-08-29 | 1979-08-29 | Low temperature turbine blade steel and its heat treatment |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5635754A (enrdf_load_stackoverflow) |
Families Citing this family (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS602380B2 (ja) * | 1981-05-30 | 1985-01-21 | 川崎製鉄株式会社 | 低炭素マルテンサイト系ステンレス鋼オ−トバイデイスクブレ−キ用材料 |
DE3789776T2 (de) * | 1986-02-05 | 1994-08-18 | Hitachi Ltd | Hitzebeständiger Stahl und daraus hergestellte Gasturbinenteile. |
JPS63171856A (ja) * | 1987-01-09 | 1988-07-15 | Hitachi Ltd | 耐熱鋼 |
CN105463327A (zh) * | 2015-12-12 | 2016-04-06 | 郭策 | 大型水电站混流式水轮机涡壳 |
CN105603319B (zh) * | 2016-01-01 | 2017-11-14 | 衢州市联橙环保科技有限公司 | 一种厨余垃圾破碎装置 |
CN110205539B (zh) * | 2019-07-05 | 2020-11-20 | 浙江朋诚科技有限公司 | 一种飞剪用高强合金刀片及其制备方法 |
-
1979
- 1979-08-29 JP JP10910879A patent/JPS5635754A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS5635754A (en) | 1981-04-08 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
KR100222302B1 (ko) | 저항복비를 가지는 저온인성이 우수한 고강도 라인파이프강재 | |
US5496421A (en) | High-strength martensitic stainless steel and method for making the same | |
JP5439973B2 (ja) | 優れた生産性と溶接性を兼ね備えた、pwht後の落重特性に優れた高強度厚鋼板およびその製造方法 | |
JP2013104070A (ja) | 耐遅れ破壊特性に優れた高強度鋼および高強度ボルト | |
JPH10503809A (ja) | 熱間加工性に優れた耐硫化物応力割れ性を有するマルテンサイト系ステンレス鋼 | |
CA2621014C (en) | Low alloy steel | |
WO2022181164A1 (ja) | 油井用高強度ステンレス継目無鋼管およびその製造方法 | |
JPS616257A (ja) | 12%Cr耐熱鋼 | |
JPS6238426B2 (enrdf_load_stackoverflow) | ||
JP3539250B2 (ja) | 高耐応力腐食割れ性を有する655Nmm−2級低C高Cr合金油井管およびその製造方法 | |
JP2024138419A (ja) | 冷間鍛造性及び、耐水素脆化特性に優れるステンレス鋼 | |
JP2000319726A (ja) | 溶接性に優れた高強度鋼板の製造方法 | |
JP2000160300A (ja) | 高耐食性を有する655Nmm−2級低C高Cr合金油井管およびその製造方法 | |
JPS616256A (ja) | 12%Cr耐熱鋼 | |
JP3485034B2 (ja) | 高耐食性を有する862N/mm2級低C高Cr合金油井管およびその製造方法 | |
CN114258435B (zh) | 具有优异的蠕变强度和高温延性的铬钢板及其制造方法 | |
JP2004250766A (ja) | 強度・低温靭性に優れたNi含有鋼の製造方法 | |
JPH07110970B2 (ja) | 耐応力腐食割れ性の優れた針状フェライトステンレス鋼の製造方法 | |
US4882124A (en) | Alloys having excellent erosion resistance | |
JPH0450364B2 (enrdf_load_stackoverflow) | ||
JPH04120249A (ja) | マルテンサイト系ステンレス鋼とその製造法 | |
JPS6013060B2 (ja) | フエライト系耐熱鋼 | |
JPS62278251A (ja) | 耐応力腐食割れ性に優れた低合金鋼 | |
JP3250263B2 (ja) | 靭性および耐応力腐食割れ性に優れたマルテンサイト系ステンレス鋼継目無鋼管の製造法 | |
JP2672429B2 (ja) | 耐食性に優れたマルテンサイト系ステンレス鋼継目無鋼管の製造法 |