JPS6231517B2 - - Google Patents

Info

Publication number
JPS6231517B2
JPS6231517B2 JP2392478A JP2392478A JPS6231517B2 JP S6231517 B2 JPS6231517 B2 JP S6231517B2 JP 2392478 A JP2392478 A JP 2392478A JP 2392478 A JP2392478 A JP 2392478A JP S6231517 B2 JPS6231517 B2 JP S6231517B2
Authority
JP
Japan
Prior art keywords
powder
oxide
metal
tape
radio wave
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP2392478A
Other languages
English (en)
Japanese (ja)
Other versions
JPS54116801A (en
Inventor
Tadaaki Sato
Tetsuji Ozaki
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kansai Paint Co Ltd
Original Assignee
Kansai Paint Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kansai Paint Co Ltd filed Critical Kansai Paint Co Ltd
Priority to JP2392478A priority Critical patent/JPS54116801A/ja
Publication of JPS54116801A publication Critical patent/JPS54116801A/ja
Publication of JPS6231517B2 publication Critical patent/JPS6231517B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Laminated Bodies (AREA)
  • Preventing Corrosion Or Incrustation Of Metals (AREA)
  • Shielding Devices Or Components To Electric Or Magnetic Fields (AREA)
  • Aerials With Secondary Devices (AREA)
  • Noise Elimination (AREA)
JP2392478A 1978-03-02 1978-03-02 Radio wave absorbing corrosionnproof tape Granted JPS54116801A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2392478A JPS54116801A (en) 1978-03-02 1978-03-02 Radio wave absorbing corrosionnproof tape

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2392478A JPS54116801A (en) 1978-03-02 1978-03-02 Radio wave absorbing corrosionnproof tape

Publications (2)

Publication Number Publication Date
JPS54116801A JPS54116801A (en) 1979-09-11
JPS6231517B2 true JPS6231517B2 (enExample) 1987-07-08

Family

ID=12124061

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2392478A Granted JPS54116801A (en) 1978-03-02 1978-03-02 Radio wave absorbing corrosionnproof tape

Country Status (1)

Country Link
JP (1) JPS54116801A (enExample)

Families Citing this family (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4538151A (en) * 1982-03-31 1985-08-27 Nippon Electric Co., Ltd. Electro-magnetic wave absorbing material
JPS58173898A (ja) * 1982-04-05 1983-10-12 日本電気株式会社 電波吸収体
JPS6013524A (ja) * 1983-07-04 1985-01-24 Fujikura Ltd 磁気シ−ルド用熱収縮性プラスチツクパイプの製造方法
JPS61170587A (ja) * 1985-01-25 1986-08-01 Bridgestone Corp 防食テ−プ
US20070148439A1 (en) * 2004-02-13 2007-06-28 Takuma Sato Communication state activation material, communication state activation sheet and communication state activation apparatus
CN102352215A (zh) * 2011-07-28 2012-02-15 西北工业大学 一种电磁双复纳米微波吸收剂Fe3O4/NanoG的制备方法
CN105009225B (zh) * 2013-02-21 2019-08-16 3M创新有限公司 具有电磁干扰减轻特性的聚合物复合物
CN111607796A (zh) * 2019-02-25 2020-09-01 天津大学 一种可控释放的磁性锌铝铈水滑石负载2-巯基苯并噻唑缓蚀剂及其制备方法
CN114801381A (zh) * 2022-03-29 2022-07-29 四川盈乐威科技有限公司 一种多层吸波材料及其制备方法

Also Published As

Publication number Publication date
JPS54116801A (en) 1979-09-11

Similar Documents

Publication Publication Date Title
Bhanvase et al. Kinetic properties of layer-by-layer assembled cerium zinc molybdate nanocontainers during corrosion inhibition
CN102473519A (zh) 磁性薄膜的制造方法、磁性薄膜及磁性体
JPS6231517B2 (enExample)
JP6661445B2 (ja) 高周波アンテナ素子、及び高周波アンテナモジュール
US3904421A (en) Anticorrosive paint
CN101280144A (zh) 高弹性吸波重防腐纳米涂料
CN108949103A (zh) 一种粉煤灰玻璃微珠-铁氧体的复合吸波材料及其制备方法
Mohamed et al. Novel water-based coatings of acrylic-polyurethane reinforced with mixed metal pigment for oil and gas pipelines protection
JPH0225279B2 (enExample)
JPH08302270A (ja) 顔料調合物
KR102011343B1 (ko) GHz 대역의 전자파 차폐능을 가진 금속산화물/고분자 복합체 및 이를 이용하여 제조한 전자파 차폐재
Ziganshina et al. Complex oxides–non-toxic pigments for anticorrosive coatings
Kapole et al. Intensification of corrosion resistance of 2 K epoxy coating by encapsulation of liquid inhibitor in nanocontainer core of sodium zinc molybdate and iron oxide
CN110317477A (zh) 一种减少电磁波干扰的高表面粗糙度金属防腐涂层及其涂覆方法
RU2502766C1 (ru) Радиопоглощающий материал и способ получения радиопоглощающего покрытия
Kapole et al. Investigation of corrosion inhibition performance of ultrasonically prepared sodium zinc molybdate nanopigment in two-pack epoxy-polyamide coating
JP3359606B2 (ja) 導電配向性フレーク状酸化亜鉛およびその製法
Mohamed et al. Influence of anticorrosive coatings integrated with novel core–shell pigment on the corrosion protection of pipelines in CO2 environment
CN111154259B (zh) 一种埃洛石-铈掺杂锰锌铁氧体复合吸波材料及制备方法
JPH107867A (ja) 電磁波吸収性樹脂組成物
JPS6060168A (ja) 導電性塗料
JP2005330163A (ja) 導電性酸化錫粉末、その製造方法、導電性ペースト及び導電性塗料
JP2613268B2 (ja) 鋼材の水素脆性防止方法及びこの方法によつて得られる鋼材
CN111378302A (zh) 一种高性能抗电磁波干扰的常温固化磷酸盐防腐涂层及其制备方法
Ahmed et al. New out-performing structured pigments for anticorrosive practical applications