JPS62263903A - 金属の超微粒子製造法 - Google Patents
金属の超微粒子製造法Info
- Publication number
- JPS62263903A JPS62263903A JP10786486A JP10786486A JPS62263903A JP S62263903 A JPS62263903 A JP S62263903A JP 10786486 A JP10786486 A JP 10786486A JP 10786486 A JP10786486 A JP 10786486A JP S62263903 A JPS62263903 A JP S62263903A
- Authority
- JP
- Japan
- Prior art keywords
- metallic particles
- bubbles
- soln
- evaporate
- ultrafine
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。
め要約のデータは記録されません。
Description
【発明の詳細な説明】
従来の製造法は、真空容器のなかに不活性ガスを封入し
、そのなかで、超微粒子にする金属を高温に加熱して蒸
発させ、それを回収して金属微粒子を得る方法である。
、そのなかで、超微粒子にする金属を高温に加熱して蒸
発させ、それを回収して金属微粒子を得る方法である。
これは、高温加熱の燃料費の割りに金属微粒子を得る
量が少量で効率が悪い。
量が少量で効率が悪い。
本発明は、効率を高めるために、界面活性剤を含む溶液
に細かい金属粒子を入れて混合液(1)をつくり、その
容器(4)の底部から、水素と酸素の混合気体(2)を
噴射させて混合液(1)内に気泡(3)をつくる。
に細かい金属粒子を入れて混合液(1)をつくり、その
容器(4)の底部から、水素と酸素の混合気体(2)を
噴射させて混合液(1)内に気泡(3)をつくる。
このとき、気泡膜には金属粒子が含まれている。
この気泡(3)が上昇して混合液面(5)上に出たとき
、その混合液面(5)上にある熱線(6)に触れて燃焼
蒸発する。これにより気泡膜に含まれていた金属粒子は
融解し蒸発する。 この蒸気を導き磁気回転ドラム(ワ
)に付着させ冷却させて金属の超微粒子を得る製造方法
である。
、その混合液面(5)上にある熱線(6)に触れて燃焼
蒸発する。これにより気泡膜に含まれていた金属粒子は
融解し蒸発する。 この蒸気を導き磁気回転ドラム(ワ
)に付着させ冷却させて金属の超微粒子を得る製造方法
である。
図は、本発明の正面の一部断面図。
1は、混合液、2は、混合気体、3は、気泡。
4は、容器、5は、混合液面、6は、熱線、7は磁気回
転ドラム、8は、冷却水。
転ドラム、8は、冷却水。
Claims (1)
- 細かい金属粒子を含む混合液(1)に水素と酸素の混合
気体(2)を噴射して、気泡膜に金属粒子を含む気泡(
3)をつくり、この気泡(3)を燃焼蒸発させて、金属
の超微粒子を得る製造法。