JPS62226814A - 酸化チタン微粒子の製造方法 - Google Patents
酸化チタン微粒子の製造方法Info
- Publication number
- JPS62226814A JPS62226814A JP7005186A JP7005186A JPS62226814A JP S62226814 A JPS62226814 A JP S62226814A JP 7005186 A JP7005186 A JP 7005186A JP 7005186 A JP7005186 A JP 7005186A JP S62226814 A JPS62226814 A JP S62226814A
- Authority
- JP
- Japan
- Prior art keywords
- titanium oxide
- water
- fine particles
- titanium
- solution
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Inorganic Compounds Of Heavy Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7005186A JPS62226814A (ja) | 1986-03-28 | 1986-03-28 | 酸化チタン微粒子の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7005186A JPS62226814A (ja) | 1986-03-28 | 1986-03-28 | 酸化チタン微粒子の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62226814A true JPS62226814A (ja) | 1987-10-05 |
| JPH0524865B2 JPH0524865B2 (enrdf_load_stackoverflow) | 1993-04-09 |
Family
ID=13420375
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP7005186A Granted JPS62226814A (ja) | 1986-03-28 | 1986-03-28 | 酸化チタン微粒子の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62226814A (enrdf_load_stackoverflow) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0517153A (ja) * | 1991-07-09 | 1993-01-26 | Mitsubishi Heavy Ind Ltd | 光反応促進用チタン酸化物触媒の製造方法 |
| US5200167A (en) * | 1989-02-28 | 1993-04-06 | Nippon Soda Co., Ltd. | Method for the preparation of spherical, fine particle titanium oxide |
| WO2004087578A1 (en) * | 2003-04-03 | 2004-10-14 | Hoon Chung | Non-acidic, non-basic colloid solution containing dispersed titanium dioxide, method of manufacturing the same, and coating material comprising the colloid solution |
-
1986
- 1986-03-28 JP JP7005186A patent/JPS62226814A/ja active Granted
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5200167A (en) * | 1989-02-28 | 1993-04-06 | Nippon Soda Co., Ltd. | Method for the preparation of spherical, fine particle titanium oxide |
| JPH0517153A (ja) * | 1991-07-09 | 1993-01-26 | Mitsubishi Heavy Ind Ltd | 光反応促進用チタン酸化物触媒の製造方法 |
| WO2004087578A1 (en) * | 2003-04-03 | 2004-10-14 | Hoon Chung | Non-acidic, non-basic colloid solution containing dispersed titanium dioxide, method of manufacturing the same, and coating material comprising the colloid solution |
| AU2003240024B2 (en) * | 2003-04-03 | 2006-06-29 | Sunhanmnt Co., Ltd | Non-acidic, non-basic colloid solution containing dispersed titanium dioxide, method of manufacturing the same, and coating material comprising the colloid solution |
| CN1329305C (zh) * | 2003-04-03 | 2007-08-01 | (株)善韩M&T | 含有分散二氧化钛的非酸、非碱胶体溶液,其制备方法和含有该胶体溶液的涂布材料 |
| US7605186B2 (en) | 2003-04-03 | 2009-10-20 | Sunhanmnt Co., Ltd. | Non-acidic, non-basic colloid solution containing dispersed titanium dioxide method of manufacturing the same, and coating material comprising the colloid solution |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0524865B2 (enrdf_load_stackoverflow) | 1993-04-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6881393B2 (en) | Process for making nano-sized and sub-micron-sized lithium-transition metal oxides | |
| CN106848231B (zh) | 通过复合前驱体配制方法制备的化合物及包含其的电池 | |
| CN101973578A (zh) | 水基溶胶凝胶法制备高纯度单分散钛酸钡纳米粉体的方法 | |
| KR20120060856A (ko) | 산화 티타늄 졸, 그 제조 방법, 초미립자상 산화 티타늄, 그 제조 방법 및 용도 | |
| JPH0472774B2 (enrdf_load_stackoverflow) | ||
| Sugimoto et al. | Formation mechanism of uniform spindle-type titania particles in the gel-sol process | |
| JPH01133939A (ja) | 酸化チタン微粒子の製造方法 | |
| WO2024244086A1 (zh) | 一种四方相纳米钛酸钡粉体及其制备方法和应用 | |
| CN102093049B (zh) | 一种准立方形貌钛酸铋镧纳米颗粒及其制备方法 | |
| JP2010274142A (ja) | 光触媒粒子の分散液及びその製法 | |
| JPS62226814A (ja) | 酸化チタン微粒子の製造方法 | |
| JPS62278125A (ja) | 結晶質酸化チタン微粒子の製法 | |
| JP5574527B2 (ja) | 酸化セリウム微粒子の製造方法 | |
| JP2004131366A (ja) | 四塩化チタン及び塩酸水溶液、硝酸水溶液またはこれらの混合溶液を使用した実質的にブルッカイト相の二酸化チタンの超微細粒子の製造方法 | |
| JPH0791066B2 (ja) | 酸化チタン微粒子の製造方法 | |
| JPH04214031A (ja) | 複合酸化ジルコニウム及びイットリウムの製法 | |
| JPH0472776B2 (enrdf_load_stackoverflow) | ||
| JPS62158116A (ja) | 酸化アルミニウム微粒子の製造方法 | |
| JPH0524864B2 (enrdf_load_stackoverflow) | ||
| JPS62226816A (ja) | 酸化ジルコニウム微粒子の製造方法 | |
| JP2709206B2 (ja) | 球形多孔質アナターゼ型二酸化チタン微粒子及びその製造方法 | |
| CN109133161B (zh) | 一种钛酸锶纳米颗粒的制备方法 | |
| JPS58213633A (ja) | 酸化アルミニウムの製造方法 | |
| KR100503858B1 (ko) | 무기산으로 제조한 사염화티타늄 수용액과 스트론튬카보네이트 수용액으로부터 나노크기의 결정성 티탄산스트론튬 분말을 제조하는 방법 | |
| Gao et al. | Influence of some parameters on the synthesis of ZrO2 nanoparticles by heating of alcohol–aqueous salt solutions |