JPS62207548A - 連続鋳造法による硫黄系快削鋼の製造方法 - Google Patents
連続鋳造法による硫黄系快削鋼の製造方法Info
- Publication number
- JPS62207548A JPS62207548A JP4824386A JP4824386A JPS62207548A JP S62207548 A JPS62207548 A JP S62207548A JP 4824386 A JP4824386 A JP 4824386A JP 4824386 A JP4824386 A JP 4824386A JP S62207548 A JPS62207548 A JP S62207548A
- Authority
- JP
- Japan
- Prior art keywords
- continuous casting
- heating
- slab
- free
- mns
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Continuous Casting (AREA)
- Treatment Of Steel In Its Molten State (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4824386A JPS62207548A (ja) | 1986-03-07 | 1986-03-07 | 連続鋳造法による硫黄系快削鋼の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4824386A JPS62207548A (ja) | 1986-03-07 | 1986-03-07 | 連続鋳造法による硫黄系快削鋼の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62207548A true JPS62207548A (ja) | 1987-09-11 |
| JPH0346220B2 JPH0346220B2 (enExample) | 1991-07-15 |
Family
ID=12797997
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP4824386A Granted JPS62207548A (ja) | 1986-03-07 | 1986-03-07 | 連続鋳造法による硫黄系快削鋼の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62207548A (enExample) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN1302126C (zh) * | 2005-03-04 | 2007-02-28 | 宝钢集团上海五钢有限公司 | 低碳高硫(硫磷)易切削结构钢连铸坯的生产方法 |
| JP2017209684A (ja) * | 2016-05-23 | 2017-11-30 | 新日鐵住金株式会社 | 溶鋼の連続鋳造方法 |
| CN115852232A (zh) * | 2022-11-28 | 2023-03-28 | 阳春新钢铁有限责任公司 | 连铸全水冷却生产硫系易切削钢的方法 |
-
1986
- 1986-03-07 JP JP4824386A patent/JPS62207548A/ja active Granted
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN1302126C (zh) * | 2005-03-04 | 2007-02-28 | 宝钢集团上海五钢有限公司 | 低碳高硫(硫磷)易切削结构钢连铸坯的生产方法 |
| JP2017209684A (ja) * | 2016-05-23 | 2017-11-30 | 新日鐵住金株式会社 | 溶鋼の連続鋳造方法 |
| CN115852232A (zh) * | 2022-11-28 | 2023-03-28 | 阳春新钢铁有限责任公司 | 连铸全水冷却生产硫系易切削钢的方法 |
| CN115852232B (zh) * | 2022-11-28 | 2024-04-30 | 阳春新钢铁有限责任公司 | 连铸全水冷却生产硫系易切削钢的方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0346220B2 (enExample) | 1991-07-15 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP5041029B2 (ja) | 高マンガン含有鋼の製造方法 | |
| CN110000355B (zh) | 改善大方坯连铸坯框型偏析的方法 | |
| JP5360086B2 (ja) | 非磁性鋼の連続鋳造を用いた製造方法 | |
| Zuo et al. | Study on the sump and temperature field during low frequency electromagnetic casting a superhigh strength Al–Zn–Mg–Cu alloy | |
| CN102343424A (zh) | 一种水平连续铸造高导高强铜合金圆棒的装置及方法 | |
| JP2025520823A (ja) | 高炭素鋼線材の製造方法 | |
| CN113118398A (zh) | 一种消除高碳马氏体不锈钢连铸板坯大颗粒碳化物的生产方法 | |
| CN111375736B (zh) | 一种马氏体沉淀硬化不锈钢的浇铸方法 | |
| JPS62207548A (ja) | 連続鋳造法による硫黄系快削鋼の製造方法 | |
| Volkova et al. | Microstructure and cleanliness of rapidly solidified steels | |
| KR20190120303A (ko) | 강의 연속 주조 방법 | |
| JP4303578B2 (ja) | 鋼の連続鋳造鋳片の中心欠陥低減方法 | |
| JP7551793B2 (ja) | 鋳造スラブの品質を改善するためのスラブの冷却および圧下方法 | |
| JP3374761B2 (ja) | 連続鋳造鋳片、その連続鋳造方法および厚鋼板の製造方法 | |
| ITOH et al. | Refining of solidification structures of continuously cast type 430 stainless steel slabs by electromagnetic stirring | |
| JP2003181608A (ja) | 連続鋳造機外におけるブルームの冷却方法 | |
| JPS62207547A (ja) | 連続鋳造法による硫黄系快削鋼の製造方法 | |
| NL8000463A (nl) | Continu gegoten staalprodukt met verminderde microsegregatie. | |
| JPH0639505A (ja) | チタン含有ステンレス溶鋼の鋳造方法 | |
| JP6515291B2 (ja) | 鋼の連続鋳造方法 | |
| Dutta et al. | Continuous casting (concast) | |
| Kakkar | Controlling Cracks in Peritectic Steel through Casting Parameter Optimization | |
| SU823439A1 (ru) | Способ обработки отливок из высоко-МАРгАНцОВиСТОй СТАли | |
| JP2001240934A (ja) | 球状黒鉛鋳鉄の製造方法 | |
| JPS5852444B2 (ja) | 熱間圧延時の鋼片表面割れ抑制法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |