JPS6211482B2 - - Google Patents
Info
- Publication number
- JPS6211482B2 JPS6211482B2 JP52152661A JP15266177A JPS6211482B2 JP S6211482 B2 JPS6211482 B2 JP S6211482B2 JP 52152661 A JP52152661 A JP 52152661A JP 15266177 A JP15266177 A JP 15266177A JP S6211482 B2 JPS6211482 B2 JP S6211482B2
- Authority
- JP
- Japan
- Prior art keywords
- cobalt
- magnetic powder
- iron oxide
- powder
- oxide magnetic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Compounds Of Iron (AREA)
- Paints Or Removers (AREA)
- Magnetic Record Carriers (AREA)
- Hard Magnetic Materials (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15266177A JPS5484299A (en) | 1977-12-19 | 1977-12-19 | Method of producing ferromagnetic powder |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15266177A JPS5484299A (en) | 1977-12-19 | 1977-12-19 | Method of producing ferromagnetic powder |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5484299A JPS5484299A (en) | 1979-07-05 |
JPS6211482B2 true JPS6211482B2 (enrdf_load_stackoverflow) | 1987-03-12 |
Family
ID=15545311
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP15266177A Granted JPS5484299A (en) | 1977-12-19 | 1977-12-19 | Method of producing ferromagnetic powder |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5484299A (enrdf_load_stackoverflow) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0464380A (ja) * | 1990-07-04 | 1992-02-28 | San Denshi Kk | 遊技機の自動開放装置 |
-
1977
- 1977-12-19 JP JP15266177A patent/JPS5484299A/ja active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0464380A (ja) * | 1990-07-04 | 1992-02-28 | San Denshi Kk | 遊技機の自動開放装置 |
Also Published As
Publication number | Publication date |
---|---|
JPS5484299A (en) | 1979-07-05 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Kishimoto et al. | Coercivity of γ‐Fe2O3 particles growing iron‐cobalt ferrite | |
EP0164251B1 (en) | Barium ferrite particles for magnetic recording media | |
JP2017201672A (ja) | 磁性粉末の製造方法 | |
EP0279626B1 (en) | Plate-like magnetite particles, plate-like maghemite particles and process for producing the same | |
JPS6311763B2 (enrdf_load_stackoverflow) | ||
GB1559145A (en) | Acicular ferromagnetic metal particles and method for preparation of the same | |
JPS6211482B2 (enrdf_load_stackoverflow) | ||
JPS60245704A (ja) | 高保磁性六方晶系針状結晶フエライト粉末の製造方法 | |
EP0340689A2 (en) | Iron carbide fine particles and process for preparing the same | |
JPH0346409B2 (enrdf_load_stackoverflow) | ||
US3039963A (en) | Method of preparing ferrimagnetic materials | |
KR890000702B1 (ko) | 코발트-함유 자성 산화철 분말의 제조방법 | |
US4272285A (en) | Process for producing magnetic metal powders | |
JPS6135135B2 (enrdf_load_stackoverflow) | ||
JPH0633116A (ja) | 磁気記録媒体用強磁性金属粉末及びその製造方法 | |
EP0326165A2 (en) | Iron Carbide fine particles and a process for preparing the same | |
JPH0366255B2 (enrdf_load_stackoverflow) | ||
JPH0471012B2 (enrdf_load_stackoverflow) | ||
JPS6151401B2 (enrdf_load_stackoverflow) | ||
KR870001378B1 (ko) | 코발트 함유 자기 산화철 분말의 제조방법 | |
JPS6090829A (ja) | バリウムフエライトの処理法 | |
EP0179489B1 (en) | A process for producing acicular particles containing an iron carbide | |
JPS58161710A (ja) | 強磁性粉末の製造方法 | |
JPS5853495B2 (ja) | 磁気記録媒体 | |
JPS6251898B2 (enrdf_load_stackoverflow) |