JPS6210948B2 - - Google Patents

Info

Publication number
JPS6210948B2
JPS6210948B2 JP2947280A JP2947280A JPS6210948B2 JP S6210948 B2 JPS6210948 B2 JP S6210948B2 JP 2947280 A JP2947280 A JP 2947280A JP 2947280 A JP2947280 A JP 2947280A JP S6210948 B2 JPS6210948 B2 JP S6210948B2
Authority
JP
Japan
Prior art keywords
mortar
steel
concrete
aqueous solution
hydroxybenzotriazole
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP2947280A
Other languages
English (en)
Japanese (ja)
Other versions
JPS56125259A (en
Inventor
Keiichi Tanigawa
Hiroshi Sakurai
Haruo Shimada
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP2947280A priority Critical patent/JPS56125259A/ja
Publication of JPS56125259A publication Critical patent/JPS56125259A/ja
Publication of JPS6210948B2 publication Critical patent/JPS6210948B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Curing Cements, Concrete, And Artificial Stone (AREA)
JP2947280A 1980-03-08 1980-03-08 Rust prevention for steel material in concrete or mortar Granted JPS56125259A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2947280A JPS56125259A (en) 1980-03-08 1980-03-08 Rust prevention for steel material in concrete or mortar

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2947280A JPS56125259A (en) 1980-03-08 1980-03-08 Rust prevention for steel material in concrete or mortar

Publications (2)

Publication Number Publication Date
JPS56125259A JPS56125259A (en) 1981-10-01
JPS6210948B2 true JPS6210948B2 (da) 1987-03-09

Family

ID=12277033

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2947280A Granted JPS56125259A (en) 1980-03-08 1980-03-08 Rust prevention for steel material in concrete or mortar

Country Status (1)

Country Link
JP (1) JPS56125259A (da)

Also Published As

Publication number Publication date
JPS56125259A (en) 1981-10-01

Similar Documents

Publication Publication Date Title
DE69822605T2 (de) Verfahren zur Sanierung und/oder zum Schutz von Bewehrungsstahl in ausgehärtetem Beton durch Aufbringen von korrosionshemmenden Zusammensetzungen auf die Oberfläche
JPH0380754B2 (da)
JPH11500401A (ja) 亜硝酸カルシウムを用いた改良腐食防止配合物
JPS5883071A (ja) 建造物ユニツトに於ける鉄筋、緊張線材などの防蝕法
JPH0468272B2 (da)
US3433657A (en) Prevention of alkali-aggregate reactions in concrete
EP0305393A1 (en) INHIBITION OF CORROSION IN REINFORCED CONCRETE.
JP2939490B2 (ja) 鉄筋コンクリートの錆抑止方法
US4802923A (en) Benefaction of concrete and aggregate using calcium phosphate
JPS6210948B2 (da)
JP6697971B2 (ja) 塩害対策用フレッシュコンクリート
JPS621343B2 (da)
JPS62265189A (ja) セメント系材料の劣化防止施工方法
JPS6067681A (ja) プレストレスコンクリ−トの防食方法
EP0084951B1 (en) Preventing carbonation in concrete and the like
JP2007269562A (ja) 耐中性化性および耐塩害性に優れた鉄筋を有する水和硬化体
JPS61256952A (ja) 鋼材防食性のセメント混練物およびセメント硬化体の製造法
JP3196810B2 (ja) 塩化物イオン吸着剤添加防錆ぺーストとモルタルを用いる塩害の補修工法
JPS5852025B2 (ja) 防蜻性セメント又は石膏組成物
GB1578984A (en) Corrosion-protection of metal reinforcements for concrete
JP4827585B2 (ja) 耐中性化性および耐塩害性に優れた鉄筋を有する水和硬化体
JP4882258B2 (ja) 耐塩害性に優れた鉄筋を有する水和硬化体
JP4882257B2 (ja) 耐塩害性に優れた鉄筋を有する水和硬化体
JP2001072457A (ja) 塩化物イオン吸着剤添加防錆ぺーストとモルタル
JPH0733556A (ja) コンクリートの耐久性向上方法