JPS6167724A - 高融点活性金属及びその合金の真空ア−ク溶解方法 - Google Patents
高融点活性金属及びその合金の真空ア−ク溶解方法Info
- Publication number
- JPS6167724A JPS6167724A JP19005584A JP19005584A JPS6167724A JP S6167724 A JPS6167724 A JP S6167724A JP 19005584 A JP19005584 A JP 19005584A JP 19005584 A JP19005584 A JP 19005584A JP S6167724 A JPS6167724 A JP S6167724A
- Authority
- JP
- Japan
- Prior art keywords
- melting
- alloys
- active metals
- vacuum arc
- melting point
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Manufacture And Refinement Of Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19005584A JPS6167724A (ja) | 1984-09-10 | 1984-09-10 | 高融点活性金属及びその合金の真空ア−ク溶解方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19005584A JPS6167724A (ja) | 1984-09-10 | 1984-09-10 | 高融点活性金属及びその合金の真空ア−ク溶解方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6167724A true JPS6167724A (ja) | 1986-04-07 |
| JPH0429722B2 JPH0429722B2 (enExample) | 1992-05-19 |
Family
ID=16251589
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP19005584A Granted JPS6167724A (ja) | 1984-09-10 | 1984-09-10 | 高融点活性金属及びその合金の真空ア−ク溶解方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6167724A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2007291453A (ja) * | 2006-04-25 | 2007-11-08 | Kobe Steel Ltd | 消耗電極 |
| CN113462904A (zh) * | 2021-07-22 | 2021-10-01 | 西安汉唐分析检测有限公司 | 一种高Mo含量Ti-Mo合金真空自耗电极棒的压制方法 |
-
1984
- 1984-09-10 JP JP19005584A patent/JPS6167724A/ja active Granted
Non-Patent Citations (2)
| Title |
|---|
| TITANIUM 1980 SCIENCE AND TECHNOLOGY=1980 * |
| TITANIUM AND TITANIUM ALLOYS=1976 * |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2007291453A (ja) * | 2006-04-25 | 2007-11-08 | Kobe Steel Ltd | 消耗電極 |
| CN113462904A (zh) * | 2021-07-22 | 2021-10-01 | 西安汉唐分析检测有限公司 | 一种高Mo含量Ti-Mo合金真空自耗电极棒的压制方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0429722B2 (enExample) | 1992-05-19 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US8668760B2 (en) | Method for the production of a β-γ-TiAl base alloy | |
| US3649253A (en) | Deoxidation of aluminum-killed molten steel | |
| JPH05239584A (ja) | 高強度アルミニウム合金圧延板およびその製造方法 | |
| EP0202336B1 (en) | Process for producing a thin plate of a high ferrosilicon alloy | |
| US3737981A (en) | Process of manufacturing forged or rolled rod steel from ledeburitic tool steel | |
| JPS6167724A (ja) | 高融点活性金属及びその合金の真空ア−ク溶解方法 | |
| JPH05214458A (ja) | チタン合金インゴットのvar 法による溶解方法 | |
| JPH0559483A (ja) | 商用周波数帯トランス用非晶質合金薄帯の製造方法 | |
| US20200199711A1 (en) | Processes for producing superalloys and superalloys obtained by the processes | |
| CN116083700A (zh) | 一种弧形连铸连轧工艺制备W4Mo3Cr4VSi高速钢棒线材的方法 | |
| JPS63111172A (ja) | タ−ゲツト材の製造方法 | |
| JP3322806B2 (ja) | 鋼中の酸化物の微細分散法 | |
| JP4540516B2 (ja) | ワークロールの製造方法 | |
| JPS629746A (ja) | 鋳塊製造方法 | |
| DE69317489T2 (de) | Verfahren zur Herstellung von weich-magnetischen Legierungen hoher permeabilität und Legierungen | |
| JPH0971827A (ja) | 工業用純チタンインゴットの製造方法 | |
| CN112941393A (zh) | 一种五元中间合金材料及其制备方法和用途 | |
| US1975310A (en) | Process of making ferrous alloys | |
| JP2926169B2 (ja) | 連鋳片の加熱方法 | |
| JPS619554A (ja) | 冷間圧延用鍛鋼ロ−ル | |
| JPH07136740A (ja) | チタン合金の鋳造方法 | |
| JPH08120366A (ja) | チタン鋳塊の連続鋳造方法 | |
| JPS6137954A (ja) | モリブデン又はモリブデン合金の溶接方法 | |
| JPH06335750A (ja) | Al−Zr系合金の製造方法 | |
| US3387968A (en) | Free-cutting steels |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |