JPS6141248B2 - - Google Patents

Info

Publication number
JPS6141248B2
JPS6141248B2 JP57042425A JP4242582A JPS6141248B2 JP S6141248 B2 JPS6141248 B2 JP S6141248B2 JP 57042425 A JP57042425 A JP 57042425A JP 4242582 A JP4242582 A JP 4242582A JP S6141248 B2 JPS6141248 B2 JP S6141248B2
Authority
JP
Japan
Prior art keywords
slurry
water
coal ash
viscosity
kneading
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP57042425A
Other languages
English (en)
Japanese (ja)
Other versions
JPS58159885A (ja
Inventor
Sumio Horiuchi
Katsuyuki Tamaoki
Atsuo Onoe
Shigeru Goto
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shimizu Construction Co Ltd
Original Assignee
Shimizu Construction Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shimizu Construction Co Ltd filed Critical Shimizu Construction Co Ltd
Priority to JP57042425A priority Critical patent/JPS58159885A/ja
Publication of JPS58159885A publication Critical patent/JPS58159885A/ja
Publication of JPS6141248B2 publication Critical patent/JPS6141248B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Consolidation Of Soil By Introduction Of Solidifying Substances Into Soil (AREA)
  • Processing Of Solid Wastes (AREA)
  • Soil Conditioners And Soil-Stabilizing Materials (AREA)
JP57042425A 1982-03-17 1982-03-17 石炭灰スラリ−の製法 Granted JPS58159885A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP57042425A JPS58159885A (ja) 1982-03-17 1982-03-17 石炭灰スラリ−の製法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP57042425A JPS58159885A (ja) 1982-03-17 1982-03-17 石炭灰スラリ−の製法

Publications (2)

Publication Number Publication Date
JPS58159885A JPS58159885A (ja) 1983-09-22
JPS6141248B2 true JPS6141248B2 (enExample) 1986-09-13

Family

ID=12635703

Family Applications (1)

Application Number Title Priority Date Filing Date
JP57042425A Granted JPS58159885A (ja) 1982-03-17 1982-03-17 石炭灰スラリ−の製法

Country Status (1)

Country Link
JP (1) JPS58159885A (enExample)

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6291284A (ja) * 1985-10-15 1987-04-25 Shimizu Constr Co Ltd 石炭灰の埋立方法
JP2001106557A (ja) * 1999-10-07 2001-04-17 Taiheiyo Cement Corp 凝結性ダストの貯留方法
JP5024608B2 (ja) * 2007-05-24 2012-09-12 清水建設株式会社 石炭灰の地盤材料化方法
JP7199190B2 (ja) * 2018-10-04 2023-01-05 日本基礎技術株式会社 液状化対策工法

Also Published As

Publication number Publication date
JPS58159885A (ja) 1983-09-22

Similar Documents

Publication Publication Date Title
JP3172932B2 (ja) 発生土を用いた水硬性組成物の製造方法
JPS6141248B2 (enExample)
US9725369B2 (en) Method of processing unhardened concrete
CN114602931A (zh) 一种用于焚烧飞灰减容稳定化处置的方法
JPS58139775A (ja) フライアツシユの廃棄方法
JPH04193749A (ja) 砕石スラッジ造粒物の製造方法
JP2750407B2 (ja) モルタル系空洞充填材
JPS5826061A (ja) セメント混練物の作業性低下防止方法
JPH09263438A (ja) セメント系グラウト材組成物
JPH0912348A (ja) 微粉体の硬化体製造方法
JPH07246397A (ja) 浚渫スラリーの処理方法
CN107673722A (zh) 一种水泥基复合固化剂
JP2881353B2 (ja) 地盤改良方法
JP5744393B2 (ja) 裏込め注入材
JP4229083B2 (ja) 飛灰のスラリー化方法および貯蔵ないし輸送方法
JPS629155B2 (enExample)
JP3101949B2 (ja) 地盤注入工法
JP3217777B1 (ja) 土壌改良方法
JP2001241032A (ja) 地盤改良材および地盤改良工法
JP2002220827A (ja) 軟弱土のヤシ殻繊維による固化処理方法
JP2832689B2 (ja) 地盤改良工法
JP2906307B2 (ja) ごみ燃料焼却灰を使用したエアミルクの製造法
JPS60133115A (ja) 地盤造成工法
JP4743403B2 (ja) 石炭灰からのホウ素溶出抑制方法
JPS57192493A (en) Granulation of aqueous slurry of coal powder