JPS61217567A - ア−ク溶接用コンタクトチツプのセラミツク被覆方法 - Google Patents

ア−ク溶接用コンタクトチツプのセラミツク被覆方法

Info

Publication number
JPS61217567A
JPS61217567A JP60057222A JP5722285A JPS61217567A JP S61217567 A JPS61217567 A JP S61217567A JP 60057222 A JP60057222 A JP 60057222A JP 5722285 A JP5722285 A JP 5722285A JP S61217567 A JPS61217567 A JP S61217567A
Authority
JP
Japan
Prior art keywords
ceramic
arc welding
contact tip
layer
substrate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP60057222A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0140910B2 (enExample
Inventor
Tadao Amasaka
天坂 格郎
Misao Iwata
美佐男 岩田
Kazumi Fujikawa
藤川 和美
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Noritake Co Ltd
Toyota Motor Corp
Original Assignee
Noritake Co Ltd
Toyota Motor Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Noritake Co Ltd, Toyota Motor Corp filed Critical Noritake Co Ltd
Priority to JP60057222A priority Critical patent/JPS61217567A/ja
Publication of JPS61217567A publication Critical patent/JPS61217567A/ja
Publication of JPH0140910B2 publication Critical patent/JPH0140910B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Arc Welding In General (AREA)
  • Coating By Spraying Or Casting (AREA)
JP60057222A 1985-03-20 1985-03-20 ア−ク溶接用コンタクトチツプのセラミツク被覆方法 Granted JPS61217567A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP60057222A JPS61217567A (ja) 1985-03-20 1985-03-20 ア−ク溶接用コンタクトチツプのセラミツク被覆方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP60057222A JPS61217567A (ja) 1985-03-20 1985-03-20 ア−ク溶接用コンタクトチツプのセラミツク被覆方法

Publications (2)

Publication Number Publication Date
JPS61217567A true JPS61217567A (ja) 1986-09-27
JPH0140910B2 JPH0140910B2 (enExample) 1989-09-01

Family

ID=13049499

Family Applications (1)

Application Number Title Priority Date Filing Date
JP60057222A Granted JPS61217567A (ja) 1985-03-20 1985-03-20 ア−ク溶接用コンタクトチツプのセラミツク被覆方法

Country Status (1)

Country Link
JP (1) JPS61217567A (enExample)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2010018778A1 (ja) * 2008-08-13 2010-02-18 ミヤチテクノス株式会社 アーク溶接用トーチ

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2010018778A1 (ja) * 2008-08-13 2010-02-18 ミヤチテクノス株式会社 アーク溶接用トーチ
JPWO2010018778A1 (ja) * 2008-08-13 2012-01-26 ミヤチテクノス株式会社 アーク溶接用トーチ

Also Published As

Publication number Publication date
JPH0140910B2 (enExample) 1989-09-01

Similar Documents

Publication Publication Date Title
US6036995A (en) Method for removal of surface layers of metallic coatings
US3031330A (en) Method of bonding an outer coating of one metal to a base surface of aluminum or the like
US3868235A (en) Process for applying hard carbide particles upon a substrate
JPWO2016171273A1 (ja) 被覆金型およびその製造方法
JP2002275658A (ja) セラミック被覆形成用の改善された表面形成方法
WO1997032053A1 (fr) Procede de formation d'un depot par pulverisation
JPS6117912B2 (enExample)
JP3076768B2 (ja) 薄膜形成装置用部材の製造方法
JPS61217567A (ja) ア−ク溶接用コンタクトチツプのセラミツク被覆方法
CN104451671A (zh) 一种涡轮热端部件热障涂层的激光加工方法
CN117568767B (zh) 一种刀具涂层及其制备方法和应用
JP3403460B2 (ja) 非酸化物系セラミック溶射皮膜を有する炭素材料の製造方法
JPS61245978A (ja) セラミツク被覆ト−チノズルおよびその製造方法
JP2004314170A (ja) アルミニウム又はアルミニウム合金から成るストリップを鋳造するための鋳造ロール
JP2000345313A (ja) 繰り返し熱衝撃及び摺動摩耗を受けるロール胴部基材表面の耐熱性、耐食性、耐摩耗性を向上させた連続鋳造に用いるロール製造法
KR100439411B1 (ko) 허스롤의 용사코팅방법
JPH0413854A (ja) 耐摩耗・耐食性溶融亜鉛浴中ロール
JPS5861269A (ja) 局部的な塩浴窒化防止方法
JPS63118057A (ja) 溶融アルミニウムめつき鋼板の製造方法
JPS61296969A (ja) セラミツク被覆ア−ク溶接用コンタクトチツプ
RU2823409C1 (ru) Способ подготовки поверхности графитированного электрода к нанесению защитного покрытия
JPS59153506A (ja) 耐摩耗性および耐焼付性に優れたシ−ムレス管製造用ガイドシユ−の製造方法
JP2012026013A (ja) 成膜装置用部品および該成膜装置用部品に付着した付着膜の除去方法
JPH05271996A (ja) マグネシウム合金材料の表面処理方法
JPH0342024Y2 (enExample)

Legal Events

Date Code Title Description
LAPS Cancellation because of no payment of annual fees