JPS61217514A - 予備脱燐剤の製造方法 - Google Patents
予備脱燐剤の製造方法Info
- Publication number
- JPS61217514A JPS61217514A JP6032785A JP6032785A JPS61217514A JP S61217514 A JPS61217514 A JP S61217514A JP 6032785 A JP6032785 A JP 6032785A JP 6032785 A JP6032785 A JP 6032785A JP S61217514 A JPS61217514 A JP S61217514A
- Authority
- JP
- Japan
- Prior art keywords
- slag
- pipe
- suction
- soda ash
- refining
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21C—PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C21C1/00—Refining of pig-iron; Cast iron
- C21C1/02—Dephosphorising or desulfurising
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Refinement Of Pig-Iron, Manufacture Of Cast Iron, And Steel Manufacture Other Than In Revolving Furnaces (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6032785A JPS61217514A (ja) | 1985-03-25 | 1985-03-25 | 予備脱燐剤の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6032785A JPS61217514A (ja) | 1985-03-25 | 1985-03-25 | 予備脱燐剤の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61217514A true JPS61217514A (ja) | 1986-09-27 |
JPH0588283B2 JPH0588283B2 (enrdf_load_stackoverflow) | 1993-12-21 |
Family
ID=13138961
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6032785A Granted JPS61217514A (ja) | 1985-03-25 | 1985-03-25 | 予備脱燐剤の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61217514A (enrdf_load_stackoverflow) |
-
1985
- 1985-03-25 JP JP6032785A patent/JPS61217514A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPH0588283B2 (enrdf_load_stackoverflow) | 1993-12-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4861368A (en) | Method for producing iron | |
CZ20002097A3 (cs) | Nádoba pro přímou tavbu | |
JPS61217514A (ja) | 予備脱燐剤の製造方法 | |
JPH0475288B2 (enrdf_load_stackoverflow) | ||
JPH0332601B2 (enrdf_load_stackoverflow) | ||
JP3336167B2 (ja) | 電気炉ダストの処理方法 | |
CN116083663A (zh) | 风淬法钢渣处理系统 | |
EP3752650B1 (en) | Method for refining molten metal using a converter | |
KR20140053195A (ko) | 고로 용선 등의 액상 용금의 탈린 방법 및 장치 | |
CN113215350A (zh) | 一种利用转炉除尘灰制备的转炉用压渣剂 | |
CN221421149U (zh) | 一种利用除尘灰在线脱磷的上料装置 | |
JPH06145830A (ja) | ダスト中の亜鉛の回収方法 | |
JP6402062B2 (ja) | ダストリサイクル方法 | |
JPS5916921A (ja) | 付着スラグの除去方法 | |
JPH09194923A (ja) | 溶銑予備処理発生ダストの再利用方法 | |
CN219032226U (zh) | 风淬法钢渣处理系统 | |
CN222331956U (zh) | 一种钢渣分级利用及余热回收装置 | |
JPH046208A (ja) | 溶銑予備処理ダストの再利用方法および装置 | |
JPH0559417A (ja) | 溶銑予備処理ダストの再利用方法および装置 | |
JP2003155511A (ja) | 転炉スラグ製品の製造方法 | |
JP4599744B2 (ja) | 酸化鉄含有集塵ダストを利用した溶銑予備処理剤の製造方法 | |
JP3794048B2 (ja) | 溶銑の脱珪処理方法 | |
JP3787960B2 (ja) | 溶融還元製錬方法 | |
JPS63210007A (ja) | 溶銑からキツシユグラフアイトを採取する方法 | |
JPS61227116A (ja) | 溶銑予備処理方法および装置 |