JPS61158874A - 取鍋用セミジルコン質流し込み不定形耐火物 - Google Patents
取鍋用セミジルコン質流し込み不定形耐火物Info
- Publication number
- JPS61158874A JPS61158874A JP59280868A JP28086884A JPS61158874A JP S61158874 A JPS61158874 A JP S61158874A JP 59280868 A JP59280868 A JP 59280868A JP 28086884 A JP28086884 A JP 28086884A JP S61158874 A JPS61158874 A JP S61158874A
- Authority
- JP
- Japan
- Prior art keywords
- zircon
- weight
- particles
- ladle
- amount
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Ceramic Products (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59280868A JPS61158874A (ja) | 1984-12-29 | 1984-12-29 | 取鍋用セミジルコン質流し込み不定形耐火物 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59280868A JPS61158874A (ja) | 1984-12-29 | 1984-12-29 | 取鍋用セミジルコン質流し込み不定形耐火物 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61158874A true JPS61158874A (ja) | 1986-07-18 |
JPH0585510B2 JPH0585510B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1993-12-07 |
Family
ID=17631076
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP59280868A Granted JPS61158874A (ja) | 1984-12-29 | 1984-12-29 | 取鍋用セミジルコン質流し込み不定形耐火物 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61158874A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US7704905B2 (en) * | 2007-05-07 | 2010-04-27 | Corning Incorporated | Reduced strain refractory ceramic composite and method of making |
US9199870B2 (en) | 2012-05-22 | 2015-12-01 | Corning Incorporated | Electrostatic method and apparatus to form low-particulate defect thin glass sheets |
US9422187B1 (en) | 2015-08-21 | 2016-08-23 | Corning Incorporated | Laser sintering system and method for forming high purity, low roughness silica glass |
JP2024148501A (ja) * | 2023-04-05 | 2024-10-18 | 株式会社ヨータイ | ジルコン質鋳込み品の製造方法及びジルコン質鋳込み品 |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6051678A (ja) * | 1983-08-31 | 1985-03-23 | 昭和電工株式会社 | セラミツクス粒子のニツケル化学コ−ト方法 |
-
1984
- 1984-12-29 JP JP59280868A patent/JPS61158874A/ja active Granted
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6051678A (ja) * | 1983-08-31 | 1985-03-23 | 昭和電工株式会社 | セラミツクス粒子のニツケル化学コ−ト方法 |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US7704905B2 (en) * | 2007-05-07 | 2010-04-27 | Corning Incorporated | Reduced strain refractory ceramic composite and method of making |
US7932200B2 (en) | 2007-05-07 | 2011-04-26 | Corning Incorporated | Reduced strain refractory ceramic composite and method of making |
TWI382006B (zh) * | 2007-05-07 | 2013-01-11 | Corning Inc | 減小應變耐火性陶瓷複合物及其製造方法 |
US9199870B2 (en) | 2012-05-22 | 2015-12-01 | Corning Incorporated | Electrostatic method and apparatus to form low-particulate defect thin glass sheets |
US9422187B1 (en) | 2015-08-21 | 2016-08-23 | Corning Incorporated | Laser sintering system and method for forming high purity, low roughness silica glass |
JP2024148501A (ja) * | 2023-04-05 | 2024-10-18 | 株式会社ヨータイ | ジルコン質鋳込み品の製造方法及びジルコン質鋳込み品 |
Also Published As
Publication number | Publication date |
---|---|
JPH0585510B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1993-12-07 |