JPS6041588A - 産業廃棄物の固化方法 - Google Patents
産業廃棄物の固化方法Info
- Publication number
- JPS6041588A JPS6041588A JP58144146A JP14414683A JPS6041588A JP S6041588 A JPS6041588 A JP S6041588A JP 58144146 A JP58144146 A JP 58144146A JP 14414683 A JP14414683 A JP 14414683A JP S6041588 A JPS6041588 A JP S6041588A
- Authority
- JP
- Japan
- Prior art keywords
- cement
- industrial waste
- water
- resin
- particles
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Glanulating (AREA)
- Fire-Extinguishing Compositions (AREA)
- Processing Of Solid Wastes (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58144146A JPS6041588A (ja) | 1983-08-06 | 1983-08-06 | 産業廃棄物の固化方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58144146A JPS6041588A (ja) | 1983-08-06 | 1983-08-06 | 産業廃棄物の固化方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6041588A true JPS6041588A (ja) | 1985-03-05 |
| JPH0230751B2 JPH0230751B2 (enEXAMPLES) | 1990-07-09 |
Family
ID=15355284
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58144146A Granted JPS6041588A (ja) | 1983-08-06 | 1983-08-06 | 産業廃棄物の固化方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6041588A (enEXAMPLES) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6061086A (ja) * | 1983-09-13 | 1985-04-08 | Kikusui Kagaku Kogyo Kk | 産業廃棄物の固化方法 |
| GB2405154A (en) * | 2002-06-20 | 2005-02-23 | Asahi Glass Co Ltd | Lubricant solution and method of applying lubricant |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN114270798B (zh) | 2019-09-26 | 2023-10-24 | 索尼半导体解决方案公司 | 摄像装置 |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS51108671A (en) * | 1975-03-20 | 1976-09-27 | Japan Steel Works Ltd | Haikibutsuno mukogaishorihoho |
| JPS53113763A (en) * | 1977-03-17 | 1978-10-04 | Shizuki Tatematsu | Treatment of industrial waste |
-
1983
- 1983-08-06 JP JP58144146A patent/JPS6041588A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS51108671A (en) * | 1975-03-20 | 1976-09-27 | Japan Steel Works Ltd | Haikibutsuno mukogaishorihoho |
| JPS53113763A (en) * | 1977-03-17 | 1978-10-04 | Shizuki Tatematsu | Treatment of industrial waste |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6061086A (ja) * | 1983-09-13 | 1985-04-08 | Kikusui Kagaku Kogyo Kk | 産業廃棄物の固化方法 |
| GB2405154A (en) * | 2002-06-20 | 2005-02-23 | Asahi Glass Co Ltd | Lubricant solution and method of applying lubricant |
| GB2405154B (en) * | 2002-06-20 | 2005-10-26 | Asahi Glass Co Ltd | Lubricant solution and method of applying lubricant |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0230751B2 (enEXAMPLES) | 1990-07-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US5304709A (en) | Hazardous wast disposal method and composition | |
| JPS6412358B2 (enEXAMPLES) | ||
| JPS61182599A (ja) | 放射性廃液の処理処分方法 | |
| JPS6041588A (ja) | 産業廃棄物の固化方法 | |
| JPS6081051A (ja) | 石炭灰硬化体製ボードの製造方法 | |
| JP2013056980A (ja) | 泥土改良剤およびその製造方法、並びに泥土の安定固化処理方法 | |
| CN106495511B (zh) | 一种利用电镀污泥制备胶凝材料的工艺 | |
| JP2781566B2 (ja) | 放射性廃棄物のセメント固化方法及び固化体 | |
| JPS6061086A (ja) | 産業廃棄物の固化方法 | |
| KR850001519A (ko) | 속경성 시멘트용 고체 5산화인 함유물질의 제조방법 | |
| JPS6212187B2 (enEXAMPLES) | ||
| CN107382175A (zh) | 一种泥土固凝剂、其制备方法及应用 | |
| JPH1180728A (ja) | 発生土及び汚泥の改質処理方法並びに改良土 | |
| JPS59232947A (ja) | 固化剤およびその固化処理法 | |
| JPS58138778A (ja) | 土壌硬化剤 | |
| JPS62183896A (ja) | 石炭灰の安定化方法 | |
| SU967992A1 (ru) | Сырьева смесь дл изготовлени чеистого бетона | |
| JPS62201399A (ja) | リン酸塩廃液の固化処理方法 | |
| CN117229016A (zh) | 一种将渣土固化成生态路基的新型土壤外加剂、制备方法及其用途 | |
| JPH10153694A (ja) | 金属アルミニウム含有放射性固体廃棄物の処理方法 | |
| SU817213A1 (ru) | Тампонажный материал дл "холод-НыХ" СКВАжиН | |
| JPS59152250A (ja) | ポルトランドセメントの製造方法 | |
| JPS62267699A (ja) | 放射性廃棄物の固化処理方法 | |
| KR790001620B1 (ko) | 방수성 포트랜드 시멘트 제조방법 | |
| CN119371123A (zh) | 用于海上风电桩基础抗冲刷的碱激发固化土及制备方法 |