JPS6021853A - リン酸ジルコニウム低膨張磁器 - Google Patents
リン酸ジルコニウム低膨張磁器Info
- Publication number
- JPS6021853A JPS6021853A JP58130617A JP13061783A JPS6021853A JP S6021853 A JPS6021853 A JP S6021853A JP 58130617 A JP58130617 A JP 58130617A JP 13061783 A JP13061783 A JP 13061783A JP S6021853 A JPS6021853 A JP S6021853A
- Authority
- JP
- Japan
- Prior art keywords
- zirconium phosphate
- low expansion
- expansion ceramic
- porcelain
- phosphate low
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Compositions Of Oxide Ceramics (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58130617A JPS6021853A (ja) | 1983-07-18 | 1983-07-18 | リン酸ジルコニウム低膨張磁器 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58130617A JPS6021853A (ja) | 1983-07-18 | 1983-07-18 | リン酸ジルコニウム低膨張磁器 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6021853A true JPS6021853A (ja) | 1985-02-04 |
| JPS6362468B2 JPS6362468B2 (esLanguage) | 1988-12-02 |
Family
ID=15038503
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58130617A Granted JPS6021853A (ja) | 1983-07-18 | 1983-07-18 | リン酸ジルコニウム低膨張磁器 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6021853A (esLanguage) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02503772A (ja) * | 1987-04-22 | 1990-11-08 | カレドニア コンポジッツ リミテッド | インライン芯材埋込み引抜き成形装置 |
| JPH0321433A (ja) * | 1989-06-20 | 1991-01-30 | Mitsui Toatsu Chem Inc | 繊維強化プラスチック‐レジンコンクリート複合材の製造方法 |
| CN110937889A (zh) * | 2019-12-10 | 2020-03-31 | 武汉科技大学 | 一种磷酸锆陶瓷材料及其制备方法 |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0294061U (esLanguage) * | 1989-01-13 | 1990-07-26 |
-
1983
- 1983-07-18 JP JP58130617A patent/JPS6021853A/ja active Granted
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02503772A (ja) * | 1987-04-22 | 1990-11-08 | カレドニア コンポジッツ リミテッド | インライン芯材埋込み引抜き成形装置 |
| JPH0321433A (ja) * | 1989-06-20 | 1991-01-30 | Mitsui Toatsu Chem Inc | 繊維強化プラスチック‐レジンコンクリート複合材の製造方法 |
| CN110937889A (zh) * | 2019-12-10 | 2020-03-31 | 武汉科技大学 | 一种磷酸锆陶瓷材料及其制备方法 |
| CN110937889B (zh) * | 2019-12-10 | 2022-03-04 | 武汉科技大学 | 一种磷酸锆陶瓷材料及其制备方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6362468B2 (esLanguage) | 1988-12-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Agrawal et al. | Synthesis and sintering of Ca0. 5Zr2P3O12-a low thermal expansion material | |
| JPH0244787B2 (esLanguage) | ||
| US6197248B1 (en) | Process for preparing aluminum titanate powder and sintered body | |
| US4189327A (en) | Semi-cordierite and method of making the same | |
| US3948670A (en) | Alumina-chrome refractory | |
| JPS6021853A (ja) | リン酸ジルコニウム低膨張磁器 | |
| US2876122A (en) | Calcium oxide articles and method of making the same | |
| JPS6065726A (ja) | 部分安定化ジルコニア体 | |
| US3244539A (en) | Bonded alumina refractory | |
| US4435514A (en) | Chromia magnesia refractory | |
| US2935411A (en) | High dielectric constant ceramics | |
| JPS6217071A (ja) | 安定化ジルコニア焼結体 | |
| US3131073A (en) | Ceramic material and method of preparation | |
| US3979214A (en) | Sintered alumina body | |
| JPS6031795B2 (ja) | ジルコニア焼結体 | |
| JP3108493B2 (ja) | 熱交換器用部材 | |
| JPS6259572A (ja) | 窒化けい素質焼結体およびその製造方法 | |
| JPH09227223A (ja) | 快削性複合セラミックスの製造法 | |
| JP2997539B2 (ja) | アルミナ多孔体の製造方法 | |
| US2160923A (en) | Refractory material | |
| JPH11322409A (ja) | βスポジューメンセラミックス及びその製造方法 | |
| JPS59107968A (ja) | ジルコニア磁器の製造方法 | |
| US4990473A (en) | Zirconyl phosphate ceramics, a process for their production and their use | |
| JPS6340771A (ja) | 六方晶窒化硼素の常圧高密度複合焼結体およびその製造方法 | |
| JPH01270581A (ja) | Bi−Ca−Sr−Cu−O系超電導膜形成用ターゲット材の製造法 |