JPS60195024A - 水酸化コバルトの製造方法 - Google Patents
水酸化コバルトの製造方法Info
- Publication number
- JPS60195024A JPS60195024A JP5027984A JP5027984A JPS60195024A JP S60195024 A JPS60195024 A JP S60195024A JP 5027984 A JP5027984 A JP 5027984A JP 5027984 A JP5027984 A JP 5027984A JP S60195024 A JPS60195024 A JP S60195024A
- Authority
- JP
- Japan
- Prior art keywords
- aqueous solution
- cobalt
- alkali
- sulfate
- added
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Inorganic Compounds Of Heavy Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5027984A JPS60195024A (ja) | 1984-03-15 | 1984-03-15 | 水酸化コバルトの製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5027984A JPS60195024A (ja) | 1984-03-15 | 1984-03-15 | 水酸化コバルトの製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS60195024A true JPS60195024A (ja) | 1985-10-03 |
| JPH0353258B2 JPH0353258B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1991-08-14 |
Family
ID=12854489
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP5027984A Granted JPS60195024A (ja) | 1984-03-15 | 1984-03-15 | 水酸化コバルトの製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS60195024A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Cited By (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH03153524A (ja) * | 1989-11-13 | 1991-07-01 | Sakai Chem Ind Co Ltd | 金属水酸化物ゾルの製造方法 |
| EP0819771A1 (en) * | 1996-07-17 | 1998-01-21 | Nanodyne Incorporated | Reclamation process for tungsten carbide/cobalt using oxidation and acid digestion |
| EP0789408A3 (en) * | 1996-02-07 | 1998-09-16 | SANYO ELECTRIC Co., Ltd. | Conductive agent and non-sintered nickel electrode for alkaline storage batteries |
| CN101921001A (zh) * | 2010-09-17 | 2010-12-22 | 浙江华友钴业股份有限公司 | 一种从硫酸钴溶液中制备氢氧化钴的工艺 |
| CN107804878A (zh) * | 2017-11-24 | 2018-03-16 | 广东佳纳能源科技有限公司 | 一种粗制氢氧化钴的制备方法 |
-
1984
- 1984-03-15 JP JP5027984A patent/JPS60195024A/ja active Granted
Cited By (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH03153524A (ja) * | 1989-11-13 | 1991-07-01 | Sakai Chem Ind Co Ltd | 金属水酸化物ゾルの製造方法 |
| EP0789408A3 (en) * | 1996-02-07 | 1998-09-16 | SANYO ELECTRIC Co., Ltd. | Conductive agent and non-sintered nickel electrode for alkaline storage batteries |
| US6057057A (en) * | 1996-02-07 | 2000-05-02 | Sanyo Electric Co., Ltd. | Conductive agent and non-sintered nickel electrode for alkaline storage batteries |
| EP0819771A1 (en) * | 1996-07-17 | 1998-01-21 | Nanodyne Incorporated | Reclamation process for tungsten carbide/cobalt using oxidation and acid digestion |
| CN101921001A (zh) * | 2010-09-17 | 2010-12-22 | 浙江华友钴业股份有限公司 | 一种从硫酸钴溶液中制备氢氧化钴的工艺 |
| CN107804878A (zh) * | 2017-11-24 | 2018-03-16 | 广东佳纳能源科技有限公司 | 一种粗制氢氧化钴的制备方法 |
| CN107804878B (zh) * | 2017-11-24 | 2019-11-19 | 广东佳纳能源科技有限公司 | 一种粗制氢氧化钴的制备方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0353258B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1991-08-14 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH11310415A (ja) | 高純度酸化錫とその製造方法 | |
| US4053568A (en) | Process for the preparation of antacid aluminum hydroxycarbonate hydrate | |
| JPS60195024A (ja) | 水酸化コバルトの製造方法 | |
| CA1046241A (en) | Preparation of nickel black | |
| JPS63503535A (ja) | ジルコニアの生成方法 | |
| JP3194176B2 (ja) | 硫酸根含有高塩基性塩化アルミニウム溶液の製造方法 | |
| JPH0362651B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
| JPS585174B2 (ja) | 塩基性乳酸アルミニウムの製造方法 | |
| FR2564084A1 (fr) | Procede pour la preparation de carbonate de cuivre basique | |
| JPS61106422A (ja) | 高純度塩基性炭酸ニツケルの製造方法 | |
| RU2154029C2 (ru) | Способ получения карбоната кобальта из раствора хлорида | |
| CN110468275A (zh) | 除去稀土沉淀物中硫酸根的方法及由该方法得到的产品 | |
| JP2002503620A (ja) | 純粋な二酸化チタン水和物及びその製造方法 | |
| CN1041193C (zh) | 由元素镍制备氢氧化镍的方法 | |
| KR20000035098A (ko) | 불순 황산 제2철 용액으로부터 유용한 생성물의 제조방법 | |
| JPS6345131A (ja) | 高純度硫酸コバルトの製造方法 | |
| US4073877A (en) | Manufacture of titanium dioxide pigment seed from a titanium sulfate solution | |
| RU2019511C1 (ru) | Способ получения оксида цинка из цинксодержащих продуктов | |
| JP2910493B2 (ja) | 次亜塩素酸ナトリウム溶液の安定化方法 | |
| CN1271728A (zh) | 尿囊素的合成工艺 | |
| JPH0812328A (ja) | 水酸化第二銅の製造法 | |
| JPS6222929B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
| EP2319803B1 (en) | Aluminum hydroxide gel particles and process for production of same | |
| CN113149084A (zh) | 一种超细氧化钴的制备方法 | |
| JP4635310B2 (ja) | 中性硫酸ナトリウム組成物およびその製造方法 |