JPS60105173A - アルカリ蓄電池用ペースト式負極板の製造法 - Google Patents

アルカリ蓄電池用ペースト式負極板の製造法

Info

Publication number
JPS60105173A
JPS60105173A JP58212211A JP21221183A JPS60105173A JP S60105173 A JPS60105173 A JP S60105173A JP 58212211 A JP58212211 A JP 58212211A JP 21221183 A JP21221183 A JP 21221183A JP S60105173 A JPS60105173 A JP S60105173A
Authority
JP
Japan
Prior art keywords
cadmium
sintered
nickel
negative plate
active material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP58212211A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0318305B2 (enrdf_load_stackoverflow
Inventor
Masahiko Oshitani
政彦 押谷
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yuasa Corp
Original Assignee
Yuasa Corp
Yuasa Battery Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yuasa Corp, Yuasa Battery Corp filed Critical Yuasa Corp
Priority to JP58212211A priority Critical patent/JPS60105173A/ja
Publication of JPS60105173A publication Critical patent/JPS60105173A/ja
Publication of JPH0318305B2 publication Critical patent/JPH0318305B2/ja
Granted legal-status Critical Current

Links

Classifications

    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00Electrodes
    • H01M4/02Electrodes composed of, or comprising, active material
    • H01M4/64Carriers or collectors
    • H01M4/70Carriers or collectors characterised by shape or form
    • H01M4/80Porous plates, e.g. sintered carriers
    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00Electrodes
    • H01M4/02Electrodes composed of, or comprising, active material
    • H01M4/24Electrodes for alkaline accumulators
    • H01M4/26Processes of manufacture
    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02EREDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10Energy storage using batteries

Landscapes

  • Chemical & Material Sciences (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Electrochemistry (AREA)
  • General Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Manufacturing & Machinery (AREA)
  • Cell Electrode Carriers And Collectors (AREA)
  • Battery Electrode And Active Subsutance (AREA)
JP58212211A 1983-11-10 1983-11-10 アルカリ蓄電池用ペースト式負極板の製造法 Granted JPS60105173A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP58212211A JPS60105173A (ja) 1983-11-10 1983-11-10 アルカリ蓄電池用ペースト式負極板の製造法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP58212211A JPS60105173A (ja) 1983-11-10 1983-11-10 アルカリ蓄電池用ペースト式負極板の製造法

Publications (2)

Publication Number Publication Date
JPS60105173A true JPS60105173A (ja) 1985-06-10
JPH0318305B2 JPH0318305B2 (enrdf_load_stackoverflow) 1991-03-12

Family

ID=16618766

Family Applications (1)

Application Number Title Priority Date Filing Date
JP58212211A Granted JPS60105173A (ja) 1983-11-10 1983-11-10 アルカリ蓄電池用ペースト式負極板の製造法

Country Status (1)

Country Link
JP (1) JPS60105173A (enrdf_load_stackoverflow)

Also Published As

Publication number Publication date
JPH0318305B2 (enrdf_load_stackoverflow) 1991-03-12

Similar Documents

Publication Publication Date Title
JP5361712B2 (ja) 新規なアルカリ蓄電池用銀正極
EP0803922B1 (en) Method of producing an alkaline battery using spongy metal substrate
JPS60105173A (ja) アルカリ蓄電池用ペースト式負極板の製造法
JPS5819866A (ja) 二次電池用カドミウム電極の製造法
JP2615538B2 (ja) アルカリ蓄電池用ニツケル正極
JP2926732B2 (ja) アルカリ二次電池
JP3156485B2 (ja) アルカリ蓄電池用ニッケル極
JP2981538B2 (ja) アルカリ電池用電極
JP3454606B2 (ja) アルカリ蓄電池用正極活物質の製造方法
JPS58198856A (ja) アルカリ蓄電池用カドミウム負極板の製造方法
JP2981537B2 (ja) アルカリ電池用負極
JP3182228B2 (ja) アルカリ蓄電池用非焼結式正極板の製造方法
JP3397216B2 (ja) ニッケル極板とその製造方法およびこれを用いたアルカリ蓄電池
JPH0318304B2 (enrdf_load_stackoverflow)
JPS60216448A (ja) アルカリ蓄電池用ペ−スト式負極板
JP2564172B2 (ja) カドミウム負極板およびその負極板を用いたアルカリ二次電池
JPS60211766A (ja) アルカリ蓄電池用ペ−スト式負極板
JPS61124060A (ja) アルカリ蓄電池用ペ−スト式正極板
JPH04181656A (ja) アルカリ蓄電池用ニッケル極の製造法
JPS61124068A (ja) ニツケルカドミウムアルカリ蓄電池
JPS603859A (ja) 二次電池用カドミウム電極の製造法
JP2001325955A (ja) ニッケル正極板とアルカリ蓄電池
JPH05198312A (ja) 密閉形アルカリ蓄電池の製造法
JP2001028261A (ja) 電池用セパレータおよびアルカリ蓄電池
JPS5931830B2 (ja) 円柱状電極の製造法