JPS59162496A - 酸化鉄皮膜の除去方法 - Google Patents
酸化鉄皮膜の除去方法Info
- Publication number
- JPS59162496A JPS59162496A JP3707883A JP3707883A JPS59162496A JP S59162496 A JPS59162496 A JP S59162496A JP 3707883 A JP3707883 A JP 3707883A JP 3707883 A JP3707883 A JP 3707883A JP S59162496 A JPS59162496 A JP S59162496A
- Authority
- JP
- Japan
- Prior art keywords
- iron oxide
- oxide film
- electrolytic
- ultrasonic vibration
- film according
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Solid-Sorbent Or Filter-Aiding Compositions (AREA)
- Cleaning And De-Greasing Of Metallic Materials By Chemical Methods (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3707883A JPS59162496A (ja) | 1983-03-07 | 1983-03-07 | 酸化鉄皮膜の除去方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3707883A JPS59162496A (ja) | 1983-03-07 | 1983-03-07 | 酸化鉄皮膜の除去方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS59162496A true JPS59162496A (ja) | 1984-09-13 |
JPH0459599B2 JPH0459599B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1992-09-22 |
Family
ID=12487511
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP3707883A Granted JPS59162496A (ja) | 1983-03-07 | 1983-03-07 | 酸化鉄皮膜の除去方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS59162496A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH02103496A (ja) * | 1988-10-12 | 1990-04-16 | Power Reactor & Nuclear Fuel Dev Corp | 超音波を利用した使用済み核燃料等の溶解方法 |
JP2006320805A (ja) * | 2005-05-18 | 2006-11-30 | Hideo Yoshida | 六価クロムの抽出方法 |
CN105684091A (zh) * | 2013-10-29 | 2016-06-15 | 西屋电气有限责任公司 | 通过组合的溶解与机械的目标换热器沉积物去除 |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5515009A (en) * | 1978-07-19 | 1980-02-01 | Hitachi Ltd | Method of removing radioactive clad |
-
1983
- 1983-03-07 JP JP3707883A patent/JPS59162496A/ja active Granted
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5515009A (en) * | 1978-07-19 | 1980-02-01 | Hitachi Ltd | Method of removing radioactive clad |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH02103496A (ja) * | 1988-10-12 | 1990-04-16 | Power Reactor & Nuclear Fuel Dev Corp | 超音波を利用した使用済み核燃料等の溶解方法 |
JP2006320805A (ja) * | 2005-05-18 | 2006-11-30 | Hideo Yoshida | 六価クロムの抽出方法 |
CN105684091A (zh) * | 2013-10-29 | 2016-06-15 | 西屋电气有限责任公司 | 通过组合的溶解与机械的目标换热器沉积物去除 |
US20160201214A1 (en) * | 2013-10-29 | 2016-07-14 | Westinghouse Electric Company Llc | Targeted heat exchanger deposit removal by combined dissolution and mechanical removal |
EP3063769A4 (en) * | 2013-10-29 | 2017-03-29 | Westinghouse Electric Company Llc | Targeted heat exchanger deposit removal by combined dissolution and mechanical removal |
US10309032B2 (en) | 2013-10-29 | 2019-06-04 | Westinghouse Electric Company Llc | Targeted heat exchanger deposit removal by combined dissolution and mechanical removal |
Also Published As
Publication number | Publication date |
---|---|
JPH0459599B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1992-09-22 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPH0445594B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
US11728054B2 (en) | Ambient temperature decontamination of nuclear power plant component surfaces containing radionuclides in a metal oxide | |
JP2022518072A (ja) | 放射能除染のための電解処理 | |
JPS59162496A (ja) | 酸化鉄皮膜の除去方法 | |
JPS62238B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
JPS58210200A (ja) | 鉄酸化物皮膜の溶解法 | |
JPS5983800A (ja) | 表面付着鉄酸化物の溶解法 | |
Al-Mobarak | Effect of oxalic acid on the dissolution of magnetite coupled with iron of various surface area | |
JPS60234998A (ja) | 金属材表面の除染清浄化方法 | |
JPS6193999A (ja) | 原子力プラントの部品除染法 | |
JPS6286200A (ja) | 還元除染における溶解速度調整法 | |
JPS61118700A (ja) | 酸化被膜の除却方法およびその装置 | |
JPH03158800A (ja) | 放射性金属廃棄物の電解除染方法 | |
JPH0672954B2 (ja) | 酸化物の溶解法 | |
JPH055079B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
JPS603598A (ja) | 酸化鉄皮膜の除染システム | |
JPH02171696A (ja) | 放射性金属廃棄物の除染装置 | |
JPS6057299A (ja) | 汚染された金属材料の洗浄方法 | |
JPH0222597A (ja) | 放射性金属廃棄物の化学除染方法 | |
JP2005140761A (ja) | 遮蔽用鉛材の電解除染方法 | |
JPS6244699A (ja) | 二価クロムイオン還元再生液を用いる除染方法 | |
WO2006080948A2 (en) | Corrosion resistance of storage containers for nuclear waste | |
JPS6267200A (ja) | 金属酸化物除去方法 | |
CN110306232A (zh) | 去污方法 | |
JPS58120786A (ja) | 酸化スケ−ルの除去方法 |