JPS5861993A - 低温鋼用溶接心線 - Google Patents

低温鋼用溶接心線

Info

Publication number
JPS5861993A
JPS5861993A JP16121381A JP16121381A JPS5861993A JP S5861993 A JPS5861993 A JP S5861993A JP 16121381 A JP16121381 A JP 16121381A JP 16121381 A JP16121381 A JP 16121381A JP S5861993 A JPS5861993 A JP S5861993A
Authority
JP
Japan
Prior art keywords
welding
core wire
wire
low
low temperature
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP16121381A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0152118B2 (enrdf_load_stackoverflow
Inventor
Osamu Tanaka
治 田中
Yutaka Nishikawa
裕 西川
Masato Konishi
正人 小西
Tatsuhiko Shigematsu
重松 辰彦
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kobe Steel Ltd
Original Assignee
Kobe Steel Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kobe Steel Ltd filed Critical Kobe Steel Ltd
Priority to JP16121381A priority Critical patent/JPS5861993A/ja
Publication of JPS5861993A publication Critical patent/JPS5861993A/ja
Publication of JPH0152118B2 publication Critical patent/JPH0152118B2/ja
Granted legal-status Critical Current

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B23MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
    • B23KSOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
    • B23K35/00Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
    • B23K35/22Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
    • B23K35/24Selection of soldering or welding materials proper
    • B23K35/30Selection of soldering or welding materials proper with the principal constituent melting at less than 1550 degrees C
    • B23K35/3033Ni as the principal constituent

Landscapes

  • Engineering & Computer Science (AREA)
  • Mechanical Engineering (AREA)
  • Nonmetallic Welding Materials (AREA)
  • Heat Treatment Of Steel (AREA)
  • Heat Treatment Of Strip Materials And Filament Materials (AREA)
JP16121381A 1981-10-09 1981-10-09 低温鋼用溶接心線 Granted JPS5861993A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP16121381A JPS5861993A (ja) 1981-10-09 1981-10-09 低温鋼用溶接心線

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP16121381A JPS5861993A (ja) 1981-10-09 1981-10-09 低温鋼用溶接心線

Publications (2)

Publication Number Publication Date
JPS5861993A true JPS5861993A (ja) 1983-04-13
JPH0152118B2 JPH0152118B2 (enrdf_load_stackoverflow) 1989-11-07

Family

ID=15730754

Family Applications (1)

Application Number Title Priority Date Filing Date
JP16121381A Granted JPS5861993A (ja) 1981-10-09 1981-10-09 低温鋼用溶接心線

Country Status (1)

Country Link
JP (1) JPS5861993A (enrdf_load_stackoverflow)

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS60247493A (ja) * 1984-05-22 1985-12-07 Nippon Steel Corp 低温用鋼の溶接用心線
JPS6199598A (ja) * 1984-10-22 1986-05-17 Nippon Steel Corp 低温用鋼の溶接用心線
US5482086A (en) * 1994-07-18 1996-01-09 Toyoda Gosei Co., Ltd. Hose with intermediate coupling
JP2007203350A (ja) * 2006-02-02 2007-08-16 Kobe Steel Ltd Ni基合金フラックス入りワイヤ
CN103480983A (zh) * 2013-09-18 2014-01-01 张盘 一种9Ni钢的高强高韧气保焊缝金属
JP5876563B1 (ja) * 2014-11-28 2016-03-02 中国電力株式会社 鋳鋼部材の溶接材料
EP3778108A4 (en) * 2018-03-27 2021-11-24 Nippon Steel Corporation Ni BASED ALLOY CORE FOR COATED ARC WELDING ROD, COATED ARC WELDING ROD AND COATED ARC WELDING ROD MANUFACTURING PROCESS

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS60247493A (ja) * 1984-05-22 1985-12-07 Nippon Steel Corp 低温用鋼の溶接用心線
JPS6199598A (ja) * 1984-10-22 1986-05-17 Nippon Steel Corp 低温用鋼の溶接用心線
US5482086A (en) * 1994-07-18 1996-01-09 Toyoda Gosei Co., Ltd. Hose with intermediate coupling
JP2007203350A (ja) * 2006-02-02 2007-08-16 Kobe Steel Ltd Ni基合金フラックス入りワイヤ
CN103480983A (zh) * 2013-09-18 2014-01-01 张盘 一种9Ni钢的高强高韧气保焊缝金属
JP5876563B1 (ja) * 2014-11-28 2016-03-02 中国電力株式会社 鋳鋼部材の溶接材料
EP3778108A4 (en) * 2018-03-27 2021-11-24 Nippon Steel Corporation Ni BASED ALLOY CORE FOR COATED ARC WELDING ROD, COATED ARC WELDING ROD AND COATED ARC WELDING ROD MANUFACTURING PROCESS

Also Published As

Publication number Publication date
JPH0152118B2 (enrdf_load_stackoverflow) 1989-11-07

Similar Documents

Publication Publication Date Title
KR102511652B1 (ko) 가스 메탈 아크 용접용 솔리드 와이어
JP2002511023A (ja) ガスフローシールド溶接用のフラックスコアワイヤ
JP2017131900A (ja) ステンレス鋼フラックス入りワイヤ
CN116137872A (zh) 气体保护金属极电弧焊用实芯焊丝
US4017711A (en) Welding material for low temperature steels
JPS5861993A (ja) 低温鋼用溶接心線
JP7276597B2 (ja) サブマージアーク溶接用ワイヤおよびそれを用いた溶接継手部の製造方法
US2985530A (en) Metallurgy
JPS60261679A (ja) 窒素含有合金の溶接方法
JPS5950437B2 (ja) Cr−Mo系低合金鋼用被覆ア−ク溶接棒
KR960705070A (ko) 용접 변형이 적고 선상(線狀)가열에 의한 구부림 가공성이 좋은 강판 및 그 제조방법과 용접재료 및 그 용접방법(steel plate having low welding strain and good bending workability by linear heating and method for producing the same, and welding material and method for producing the same)
US2784125A (en) Wrought stainless steel
US2891859A (en) Alloy steel
JPS6046896A (ja) 低温用鋼溶接用のΝi基複合ワイヤ
JPH03204196A (ja) 耐濃硫酸腐食性に優れた二相ステンレス鋼溶接用ワイヤ
JPS59226151A (ja) 溶接性と熱間加工性に優れた高合金オ−ステナイト系ステンレス鋼
JPH07100688A (ja) 高強度Cr−Mo鋼用TIG溶接ワイヤ
JPS5947071A (ja) CrーMo鋼溶接用ソリッドワイヤ
US4131781A (en) Submerged arc welding process for nickel containing steel
JPH01215491A (ja) Cr−Mo系低合金鋼用被覆アーク溶接棒
JPH0796390A (ja) 9Cr−1Mo鋼溶接用ワイヤ
JPS60261690A (ja) Cr−Mo系低合金鋼用被覆ア−ク溶接棒
CN115803144B (zh) 药芯焊丝
JPS6114100A (ja) Ni基被覆ア−ク溶接棒
JPS596756B2 (ja) 超低温用鋼の潜弧溶接法