JPS5826091A - コンクリ−トブロツク製品の紛体塗装による表面美装方法 - Google Patents
コンクリ−トブロツク製品の紛体塗装による表面美装方法Info
- Publication number
- JPS5826091A JPS5826091A JP12322481A JP12322481A JPS5826091A JP S5826091 A JPS5826091 A JP S5826091A JP 12322481 A JP12322481 A JP 12322481A JP 12322481 A JP12322481 A JP 12322481A JP S5826091 A JPS5826091 A JP S5826091A
- Authority
- JP
- Japan
- Prior art keywords
- powder paint
- concrete block
- dressing method
- surface dressing
- block products
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。
め要約のデータは記録されません。
Description
【発明の詳細な説明】
本発BAはコンクリートブロックに遠赤外線を用いて粉
体塗料を焼付塗装する方法に関するものである。
体塗料を焼付塗装する方法に関するものである。
コンクリートブロックに粉体塗料を塗布したのち全体を
熱風炉にて強制加熱し塗膜を形成すると、ブロック表面
に開口していた気口内の水分及びガス体が膨張吐出によ
りその塗膜にピンホール等が発生したり塗膜の剥離を生
じて製品に不良品が沢山できる。又コンクリートブロッ
クを絶乾状態圧して粉体塗料を塗布するのは比熱の大き
いコンクリートブロックではエネルギーを多大に要しl
&済的に大きな損失である等の欠点に鑑み、本発明は上
記の欠点を解消して良質の塗膜を形成する美麗な製品を
珈価に提供しようとする目的である。
熱風炉にて強制加熱し塗膜を形成すると、ブロック表面
に開口していた気口内の水分及びガス体が膨張吐出によ
りその塗膜にピンホール等が発生したり塗膜の剥離を生
じて製品に不良品が沢山できる。又コンクリートブロッ
クを絶乾状態圧して粉体塗料を塗布するのは比熱の大き
いコンクリートブロックではエネルギーを多大に要しl
&済的に大きな損失である等の欠点に鑑み、本発明は上
記の欠点を解消して良質の塗膜を形成する美麗な製品を
珈価に提供しようとする目的である。
Claims (1)
- 表面乾燥状態のコンクリートブロックに粉体塗料を電着
させ、遠赤外線にて粉体塗料を焼付温度200変前后で
約2分間焼付て塗料を半硬化如しさらにその上に粉体塗
料を電着させて所建の厚さを作り、遠赤外線にて200
変前后で約20分間本焼付てml11Iを形成硬化せし
める方法。