JPS574376A - Cementation method of glass - Google Patents

Cementation method of glass

Info

Publication number
JPS574376A
JPS574376A JP7715780A JP7715780A JPS574376A JP S574376 A JPS574376 A JP S574376A JP 7715780 A JP7715780 A JP 7715780A JP 7715780 A JP7715780 A JP 7715780A JP S574376 A JPS574376 A JP S574376A
Authority
JP
Japan
Prior art keywords
glass
braze
joint
parts
cementing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP7715780A
Other languages
Japanese (ja)
Other versions
JPS63148B2 (en
Inventor
Eizo Goto
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toshiba Corp
Original Assignee
Toshiba Corp
Tokyo Shibaura Electric Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toshiba Corp, Tokyo Shibaura Electric Co Ltd filed Critical Toshiba Corp
Priority to JP7715780A priority Critical patent/JPS574376A/en
Publication of JPS574376A publication Critical patent/JPS574376A/en
Publication of JPS63148B2 publication Critical patent/JPS63148B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE: To achieve firm and highly airtight cementation so as to permit substantial reduction in the thickness of glass braze layers by making combination use of an annular joint consisting of an easy-to-melt metal and glass braze and melting these on the surfaces intended for cementing.
CONSTITUTION: Pastelike glass braze 4 is coated on the intended cementing parts 1a, 2a of members 1, 2 to be cemented, and these parts are inserted to an annular joint 3 consisting of Al from both ends. If the joint 3 is heated with burners 5, the org. materials of the glass braze 4 are removed, and the braze 4 and the joint 3 melt. Then, the Al of the joint 3 is a thick film shape, and remains on the molten glass. The molten glass is an extremely laminar shape, and sticks by melting on the surfaces of the parts 1a, 2a. The excess glass braze runs off. Thereupon, when these are cooled, the Al and the glass braze solidify, and the Al is reformed to a new annular joint 6. The glass braze 4 forms a thin glass layer 7 between the parts 1a and 2a. Further, in the process of cooling down to ordinary temp., strong tightening stress is generated in the glass layer 7 by the shrinkage of the joint 6, whereby the cementing is strain-intensified.
COPYRIGHT: (C)1982,JPO&Japio
JP7715780A 1980-06-10 1980-06-10 Cementation method of glass Granted JPS574376A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP7715780A JPS574376A (en) 1980-06-10 1980-06-10 Cementation method of glass

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP7715780A JPS574376A (en) 1980-06-10 1980-06-10 Cementation method of glass

Publications (2)

Publication Number Publication Date
JPS574376A true JPS574376A (en) 1982-01-09
JPS63148B2 JPS63148B2 (en) 1988-01-05

Family

ID=13625951

Family Applications (1)

Application Number Title Priority Date Filing Date
JP7715780A Granted JPS574376A (en) 1980-06-10 1980-06-10 Cementation method of glass

Country Status (1)

Country Link
JP (1) JPS574376A (en)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5954539U (en) * 1982-09-30 1984-04-10 京セラ株式会社 Assembly structure of ceramic parts and metal parts
JPS6068154A (en) * 1983-09-26 1985-04-18 Toshiba Corp Binding method of al member
JPS61164235U (en) * 1985-04-01 1986-10-11

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5954539U (en) * 1982-09-30 1984-04-10 京セラ株式会社 Assembly structure of ceramic parts and metal parts
JPS6068154A (en) * 1983-09-26 1985-04-18 Toshiba Corp Binding method of al member
JPS61164235U (en) * 1985-04-01 1986-10-11

Also Published As

Publication number Publication date
JPS63148B2 (en) 1988-01-05

Similar Documents

Publication Publication Date Title
ES8605870A1 (en) Composite metal articles.
JPS574376A (en) Cementation method of glass
DE3172416D1 (en) Metal, carbon, carbide and other compositions thereof, alloys and methods for preparing same
JPS5428744A (en) Process for joining aluminum, aluminum alloy and steel
JPS57131357A (en) Local surface hardening method for ferrous parts
JPS6417876A (en) Production of metallic pipe coated with tin or tin-base alloy on inside surface
JPS5536020A (en) Brazing method and joint
JPS5711761A (en) Composite casting and production thereof
JPS58104076A (en) Manufacture of reinforced refractories
JPS5540087A (en) Metallic pattern bridge welding process of pipe shaped structure
JP2706934B2 (en) Surface coating method
JPS5722852A (en) Treatment of surface for mold copper plate of continuous casting installation
JPS6428356A (en) Production of joined metal of nickel-based metal and aluminum-based metal
JPH0744363Y2 (en) Inner coating injection pipe for tundish
JPS5727180A (en) Method for covering aluminium plated steel with resin
Nazarenko et al. Eliminatino of Cracks in Shell-Mould Castings of 35 KhGSL Steel
JPS60118366A (en) Production of joined body between oxide ceramics and copper or alloy thereof
JPS641115A (en) Manufacture of magnetic head
JPS56122662A (en) Preventing method of casting crack of antiferromagnetic chromium invar alloy ingot
JPS5727181A (en) Method for covering aluminium plated steel with resin
JPS57134235A (en) Production of polycrystalline silicon semiconductor
Zheng Skin Effect of Hafnium-Rich Melts in Hafnium-Bearing Cast Nickel Base Superalloys
JPS5686676A (en) Gas welding method of cast iron
JPS5728665A (en) Method for forming wearproof coating
JPS55130360A (en) Coat coating structure of mold preventing burning-on