JPS5741801A - Manufacture of stainless steel sheet prevented from generating gold-dust flaw - Google Patents
Manufacture of stainless steel sheet prevented from generating gold-dust flawInfo
- Publication number
- JPS5741801A JPS5741801A JP11649080A JP11649080A JPS5741801A JP S5741801 A JPS5741801 A JP S5741801A JP 11649080 A JP11649080 A JP 11649080A JP 11649080 A JP11649080 A JP 11649080A JP S5741801 A JPS5741801 A JP S5741801A
- Authority
- JP
- Japan
- Prior art keywords
- max
- surface roughness
- roll
- final pass
- sheet
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To prevent the generation of a gold-dust flaw, and to make a dividing process and a grinding process unnecessary, by employing a roll having a limited surface roughness prescribed with an upper limit and a lower limit of Hmax for rolling a blank material having a ≤30μ surface roughness as Hmax.
CONSTITUTION: For the purpose of reducing the roll marks in the surface of a rolled sheet to ≤6μ as Hmax, a roll having a surface roughness ≥0.5μ and ≤6μ as Hmax is employed in a cold rolling pass except its final pass, for reducing a blank material having a ≤30μ surface roughness as Hmax. Then, a roll having ≤6μ surface roughness as Hmax is employed in the final pass for reducing a sheet finished to a ≥0.5μ surface roughness as Hmax just before the final pass. Accordingly, even if the surface roughness of the roll to work in the final pass is made ≤0.5μ as Hmax, the sheet surface can retain the lubricant oil, so that the heat scratches do not generate in the sheet surface.
COPYRIGHT: (C)1982,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11649080A JPS5741801A (en) | 1980-08-26 | 1980-08-26 | Manufacture of stainless steel sheet prevented from generating gold-dust flaw |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11649080A JPS5741801A (en) | 1980-08-26 | 1980-08-26 | Manufacture of stainless steel sheet prevented from generating gold-dust flaw |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5741801A true JPS5741801A (en) | 1982-03-09 |
Family
ID=14688408
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11649080A Pending JPS5741801A (en) | 1980-08-26 | 1980-08-26 | Manufacture of stainless steel sheet prevented from generating gold-dust flaw |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5741801A (en) |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS59232607A (en) * | 1983-06-16 | 1984-12-27 | Toyo Kohan Co Ltd | Manufacture of metallic plate for shadow mask |
JPS60227904A (en) * | 1984-04-27 | 1985-11-13 | Nippon Steel Corp | Production of cold rolled stainless steel strip having excellent surface characteristic |
JPS61249603A (en) * | 1985-04-26 | 1986-11-06 | Nippon Steel Corp | Production of thin austenitic stainless steel sheet having excellent surface characteristic |
JPS61249602A (en) * | 1985-04-26 | 1986-11-06 | Nippon Steel Corp | Production of thin ferritic stainless steel sheet having excellent surface characteristic |
EP0375384A2 (en) * | 1988-12-23 | 1990-06-27 | Kawasaki Steel Corporation | Method and apparatus for pre-processing stainless steel strip intended to be cold-rolled |
US5105638A (en) * | 1990-07-12 | 1992-04-21 | Mitsubishi Jukogyo Kabushiki Kaisha | Method and machine for rolling a metal workpiece at a reduced rolling load |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS53106365A (en) * | 1977-02-28 | 1978-09-16 | Kawasaki Steel Co | Cold rolling method of stainless steel band |
-
1980
- 1980-08-26 JP JP11649080A patent/JPS5741801A/en active Pending
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS53106365A (en) * | 1977-02-28 | 1978-09-16 | Kawasaki Steel Co | Cold rolling method of stainless steel band |
Cited By (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS59232607A (en) * | 1983-06-16 | 1984-12-27 | Toyo Kohan Co Ltd | Manufacture of metallic plate for shadow mask |
JPH0344842B2 (en) * | 1983-06-16 | 1991-07-09 | Toyo Kohan Co Ltd | |
JPS60227904A (en) * | 1984-04-27 | 1985-11-13 | Nippon Steel Corp | Production of cold rolled stainless steel strip having excellent surface characteristic |
JPS61249603A (en) * | 1985-04-26 | 1986-11-06 | Nippon Steel Corp | Production of thin austenitic stainless steel sheet having excellent surface characteristic |
JPS61249602A (en) * | 1985-04-26 | 1986-11-06 | Nippon Steel Corp | Production of thin ferritic stainless steel sheet having excellent surface characteristic |
JPH0347928B2 (en) * | 1985-04-26 | 1991-07-22 | Nippon Steel Corp | |
JPH0347927B2 (en) * | 1985-04-26 | 1991-07-22 | Nippon Steel Corp | |
EP0375384A2 (en) * | 1988-12-23 | 1990-06-27 | Kawasaki Steel Corporation | Method and apparatus for pre-processing stainless steel strip intended to be cold-rolled |
EP0375384A3 (en) * | 1988-12-23 | 1992-01-15 | Kawasaki Steel Corporation | Method and apparatus for pre-processing stainless steel strip intended to be cold-rolled |
US5105638A (en) * | 1990-07-12 | 1992-04-21 | Mitsubishi Jukogyo Kabushiki Kaisha | Method and machine for rolling a metal workpiece at a reduced rolling load |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
KR880014119A (en) | Pretreatment method and apparatus for cold rolling stainless steel | |
JPS5741801A (en) | Manufacture of stainless steel sheet prevented from generating gold-dust flaw | |
JPS56165502A (en) | Manufacture of cold rolled titanium sheet | |
JPS56111501A (en) | Manufacture of h-beam | |
JPS5641032A (en) | Hemming method of aluminum or aluminum alloy plate | |
JPS5425214A (en) | Method of producing hot-rolled soft steel plate | |
JPS5592203A (en) | Skin pass rolling method of cold rolled steel plate | |
JPS5689302A (en) | Preventing method for steel strip from heat scratch due to cold rolling work | |
JPS6466003A (en) | Production of high brightness cold-rolled steel sheet | |
JPS5689329A (en) | High speed tension leveler | |
JPS5533870A (en) | Temper rolling method of mirror surface material on surface of tinplate | |
JPS56131002A (en) | Changing method for roll crown | |
JPS5695402A (en) | Manufacture of rough shaped billet for h-beam | |
JPS5719325A (en) | Production of steel product | |
JPS5597804A (en) | Temper rolling roll for galvanized steel sheet | |
JPS5514172A (en) | Skin-pass rolling method of original tin plate | |
JPS57106407A (en) | Bright rolling method | |
JPS5516769A (en) | Manufacturing steel sheet of high shaping property for drawing and squeezing | |
JPS5736011A (en) | Cold rolling method for steel strip | |
JPS5415458A (en) | Method of producing cold rolled steel plate | |
JPS55165203A (en) | Manufacture of thin steel sheet | |
JPS56160805A (en) | Manufacture of cold rolled steel sheet | |
JPS5672124A (en) | Manufacture of case hardening steel | |
JPS5750204A (en) | Rolling mill | |
JPS57103732A (en) | Al slag material for impact excellent in lubrication |