JPS5597804A - Temper rolling roll for galvanized steel sheet - Google Patents
Temper rolling roll for galvanized steel sheetInfo
- Publication number
- JPS5597804A JPS5597804A JP401079A JP401079A JPS5597804A JP S5597804 A JPS5597804 A JP S5597804A JP 401079 A JP401079 A JP 401079A JP 401079 A JP401079 A JP 401079A JP S5597804 A JPS5597804 A JP S5597804A
- Authority
- JP
- Japan
- Prior art keywords
- roll
- steel sheet
- galvanized steel
- surface roughness
- ppi
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To prevent the dross involvement, and to extend the roll life, by prescribing the surface characteristics of the reducing roll for the galvanized steel sheet with the surface roughness 2.5W5.0μRa, the cutoff level 1.2W1.3μ, and PPI 150 or more.
CONSTITUTION: This roll is a temper rolling roll possessing the dull roll surface roughness 2.5W5.0μRa, the cutoff level 1.2W1.3μ, and PPI (number of peak per inch) 150 or more. If the surface roughness as the mean roughness on the center line is less than 2.5μRa, the dull profile can not be satisfactorily transferred to the galvanized steel sheet, and the roll life is shortened. Besides, if above roughness exceeds 5.0μRa, the surface roughness becomes coarse and the appearance is deteriorated. The cutoff level 1.2W1.3μ is in the range permissible to exactly count the number of peak for bringing about the effect. If the value of PPI is smaller, the sectional area of a peak becomes large, the wear of the roll surface becomes irregular, and the amount of dross involvement increases.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP401079A JPS5947608B2 (en) | 1979-01-19 | 1979-01-19 | Temper rolling roll of plated steel plate |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP401079A JPS5947608B2 (en) | 1979-01-19 | 1979-01-19 | Temper rolling roll of plated steel plate |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5597804A true JPS5597804A (en) | 1980-07-25 |
JPS5947608B2 JPS5947608B2 (en) | 1984-11-20 |
Family
ID=11572994
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP401079A Expired JPS5947608B2 (en) | 1979-01-19 | 1979-01-19 | Temper rolling roll of plated steel plate |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5947608B2 (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61162306U (en) * | 1985-03-29 | 1986-10-08 | ||
JPH02175007A (en) * | 1988-12-27 | 1990-07-06 | Kawasaki Steel Corp | Manufacture of surface treated steel sheet having good image clarity |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63183210U (en) * | 1987-05-14 | 1988-11-25 |
-
1979
- 1979-01-19 JP JP401079A patent/JPS5947608B2/en not_active Expired
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61162306U (en) * | 1985-03-29 | 1986-10-08 | ||
JPH02175007A (en) * | 1988-12-27 | 1990-07-06 | Kawasaki Steel Corp | Manufacture of surface treated steel sheet having good image clarity |
Also Published As
Publication number | Publication date |
---|---|
JPS5947608B2 (en) | 1984-11-20 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS56146678A (en) | Cutting blade | |
JPS5597804A (en) | Temper rolling roll for galvanized steel sheet | |
JPS53146954A (en) | Rolling mill | |
JPS56165502A (en) | Manufacture of cold rolled titanium sheet | |
JPS5741801A (en) | Manufacture of stainless steel sheet prevented from generating gold-dust flaw | |
Imai | Study on a Jumping Phenomenon in Wet Temper Rolling of Annealed Tinplates With Light Reduction | |
JPS56131002A (en) | Changing method for roll crown | |
JPS5548405A (en) | Rolling method of metallic plate | |
JPS5785989A (en) | Zinc electroplated steel plate forming star mark hardly during press working | |
JPS56116855A (en) | A -killed steel plate for can by continuous casting | |
JPS53146217A (en) | Work roll for cold rolling | |
JPS5689329A (en) | High speed tension leveler | |
JPS5510341A (en) | Rolling mill | |
JPS5577901A (en) | Preventing method for surface cracking of billet in hot rolling pass | |
Dubinskii et al. | Preventing the" Catching" of Cold Rolling Mill Rolls When in Contact With Etched Strip | |
Maeda et al. | Slip behaviour of material on top surface of die in circular blanking | |
Kitagawa et al. | Electric Discharge Method for Work Roll of Cold Rolling Mill | |
JPS5575808A (en) | Cold rolling mill | |
JPS53118221A (en) | Method of manufacturing non-pretempered high-tensile steel | |
JPS5592203A (en) | Skin pass rolling method of cold rolled steel plate | |
JPS5514172A (en) | Skin-pass rolling method of original tin plate | |
JPS57146453A (en) | Rolling roll | |
JPS5689302A (en) | Preventing method for steel strip from heat scratch due to cold rolling work | |
JPS55128308A (en) | Rolling mill | |
Trishevskii et al. | The Effect of Chemical Composition and Rolling Conditions on the Uniform Elongation of Carbon-Steel Plate |