JPS5725260A - Endless track type horizontal continuous casting installation - Google Patents
Endless track type horizontal continuous casting installationInfo
- Publication number
- JPS5725260A JPS5725260A JP9961480A JP9961480A JPS5725260A JP S5725260 A JPS5725260 A JP S5725260A JP 9961480 A JP9961480 A JP 9961480A JP 9961480 A JP9961480 A JP 9961480A JP S5725260 A JPS5725260 A JP S5725260A
- Authority
- JP
- Japan
- Prior art keywords
- slag
- molten slag
- layer
- solidified
- molten
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To prevent the occurrence of breaking lines on the outside circumferential surface of an ingot by forming the head part of a pouring nozzle into a truncated cone, and opening a supply hole for molten slag on the way of the cone. CONSTITUTION:Upon starting of casting work, the molten slag 13 in a airtight tank is supplied into a mold through a supply hole 15 opened on the slope S of the head part 4' of a pouring nozzle 4. The molten slag 13 in the clearance C between the tread surface of an endless track and the flat part T of the nozzle 4, and the part near the same forms a solidified layer U of a wedge shape in section stuck on the slope s, thereby preventing the slag 13 from leaking to the outside through the clearance C. The slag layer carried along with the shifting of the tread surface is broken at the leading end part V of the solidified layer U, and the molten slag 13 in a well W immediately infiltrates the broken part of the slag layer and is carried without disconnection while reproducing fresh solidified shells. On the other hand, the molten steel 1 in the mold is cooled while forming one partition wall of the well W of the molten slag 13, thereby successively and continuously forming solidified shells 6. Hence, inscribing of breaking lines does not occur.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9961480A JPS5725260A (en) | 1980-07-21 | 1980-07-21 | Endless track type horizontal continuous casting installation |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9961480A JPS5725260A (en) | 1980-07-21 | 1980-07-21 | Endless track type horizontal continuous casting installation |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5725260A true JPS5725260A (en) | 1982-02-10 |
Family
ID=14251965
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP9961480A Pending JPS5725260A (en) | 1980-07-21 | 1980-07-21 | Endless track type horizontal continuous casting installation |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5725260A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6027448A (en) * | 1983-07-26 | 1985-02-12 | Ishikawajima Harima Heavy Ind Co Ltd | Continuous casting method of steel plate |
US4589472A (en) * | 1983-06-01 | 1986-05-20 | Swiss Aluminium Ltd. | Process for preventing metal penetrating between a mold wall and a nozzle |
-
1980
- 1980-07-21 JP JP9961480A patent/JPS5725260A/en active Pending
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4589472A (en) * | 1983-06-01 | 1986-05-20 | Swiss Aluminium Ltd. | Process for preventing metal penetrating between a mold wall and a nozzle |
JPS6027448A (en) * | 1983-07-26 | 1985-02-12 | Ishikawajima Harima Heavy Ind Co Ltd | Continuous casting method of steel plate |
JPH0378170B2 (en) * | 1983-07-26 | 1991-12-12 | Ishikawajima Harima Heavy Ind |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB1467024A (en) | Method of continuously casting silicon-and/or aluminium-killed steels | |
KR920000407A (en) | Method and apparatus for flowing molten metal during continuous strip casting | |
JPS5725260A (en) | Endless track type horizontal continuous casting installation | |
GB1251875A (en) | ||
US4531567A (en) | Injection and feeder pipe for apparatus for continuous casting of steel | |
ES476101A1 (en) | Device for continuous horizontal casting | |
JPS55139148A (en) | Ultrasonic wave casting method for steel ingot excellent in inner quality | |
JPS5731453A (en) | Continuous casting method for steel | |
JPS5785652A (en) | Continuous casting method for hollow blank material for pipe making | |
JPS5788952A (en) | Sealing method for hot-water feed nozzle in endless track type horizontal continuous casting machine | |
JPS5781944A (en) | Continuous casting device | |
JPS6466061A (en) | Production of ingot having double layers | |
JPS56154260A (en) | Method for preventing wear of mold for continuous casting | |
JPS5752553A (en) | Nozzle for casting of molten metal | |
JPS613657A (en) | Bottom pouring ladle | |
JPS645641A (en) | Lost foam pattern | |
JPS6317571Y2 (en) | ||
GB1217787A (en) | Method and apparatus for degassing iron-base melts | |
JPS6466055A (en) | Continuous casting method | |
JPS5510312A (en) | Continuous casting method of steel | |
Duchateau et al. | Continuous Casting Device | |
JPS56165544A (en) | Method for continuous casting of steel | |
JPS55144362A (en) | Continuous casting start method | |
JPS56154265A (en) | Endless track type horizontal continuous casting device | |
JPS5533875A (en) | Deoxidation method of molten steel inside mold at start of continuous casting |