JPS57199173A - Manufacturing method of silver (2) oxide cell - Google Patents
Manufacturing method of silver (2) oxide cellInfo
- Publication number
- JPS57199173A JPS57199173A JP8323381A JP8323381A JPS57199173A JP S57199173 A JPS57199173 A JP S57199173A JP 8323381 A JP8323381 A JP 8323381A JP 8323381 A JP8323381 A JP 8323381A JP S57199173 A JPS57199173 A JP S57199173A
- Authority
- JP
- Japan
- Prior art keywords
- positive electrode
- layer
- silver
- lead
- aqueous solution
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To control the increase of internal resistance during storage by impregnating an alkaline aqueous solution in the surface layer of a two-layer positive electrode consisting of silver (II) oxide and silver (I) oxide layers, depositing lead hydroxide, incorporating it in a cell, oxidizing lead hydroxide in the cell during storage, and forming a lead dioxide layer on the surface of the positive electrode. CONSTITUTION:A two-layer positive electrode in which a silver (I) oxide layer 3 is formed around a silver (II) oxide layer 2 by reducing the surface layer of the press molding substance consisting of silver (II) oxide is immersed in alkaline aqueous solution and the alkaline aqueous solution is impregnated on its surface layer. Then the positive electrode is immersed in a nitrate aqueous solution and lead hydrooxide is deposited on its surface. As described above, when the positive electrode 1 which impregnates the alkaline aqueous solution is immersed in the nitrate aqueous solution, lead hydroxide is deposited on the surface of the positive electrode 1. Besides, when the positive electrode 1 in which this lead hydroxide is deposited is incorporated in a cell, lead hydroxide is oxidized during storage and becomes lead dioxide. Since this lead dioxide is in the highest oxidation state, it is excellent in oxidation resistance. When a lead dioxide layer is formed on the surface of the positive electrode 1, this cell has small internal resistance and prevents the internal resistance from being increased during storage.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8323381A JPS57199173A (en) | 1981-05-31 | 1981-05-31 | Manufacturing method of silver (2) oxide cell |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8323381A JPS57199173A (en) | 1981-05-31 | 1981-05-31 | Manufacturing method of silver (2) oxide cell |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS57199173A true JPS57199173A (en) | 1982-12-07 |
Family
ID=13796601
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP8323381A Pending JPS57199173A (en) | 1981-05-31 | 1981-05-31 | Manufacturing method of silver (2) oxide cell |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57199173A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US11021192B2 (en) | 2016-07-11 | 2021-06-01 | Honda Motor Co., Ltd. | Underbody structure |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5588265A (en) * | 1978-12-25 | 1980-07-03 | Hitachi Maxell Ltd | Argentic oxide battery |
-
1981
- 1981-05-31 JP JP8323381A patent/JPS57199173A/en active Pending
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5588265A (en) * | 1978-12-25 | 1980-07-03 | Hitachi Maxell Ltd | Argentic oxide battery |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US11021192B2 (en) | 2016-07-11 | 2021-06-01 | Honda Motor Co., Ltd. | Underbody structure |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS51145390A (en) | Manufacturing method of a coated layer of oxygen senser | |
GB1505979A (en) | Manufacture of primary alkaline cells | |
JPS5734662A (en) | Manufacture of silver oxide battery | |
JPS57199173A (en) | Manufacturing method of silver (2) oxide cell | |
DE1291139B (en) | GLASS ELECTRODE | |
JPS5734661A (en) | Manufacture of silver oxide battery | |
KR870003526A (en) | Solid Electrolytic Capacitors and Manufacturing Method Thereof | |
GB1044444A (en) | Improvements relating to capacitors | |
KR920020555A (en) | Joining Cathode Manufacturing Method | |
US3415685A (en) | Gas-depolarizable galvanic cell | |
JP2657932B2 (en) | Method for manufacturing solid electrolytic capacitor | |
KR890004455A (en) | Manufacturing method of superconducting ceramic wire | |
ES426538A2 (en) | Process of producing solderable composites containing AgCdO | |
DE1671745C3 (en) | Galvanic element and process for its production | |
JPS5693842A (en) | Composite electric contact material | |
JPS5630442A (en) | Composite permeable membrane | |
JPS56118266A (en) | Manufacture of silvic-oxide battery | |
KR910019263A (en) | Manufacturing method of multilayer ceramic capacitor by injection electrode method | |
JPS5645571A (en) | Battery | |
KR0163860B1 (en) | Carbon and argentum pasting method in tantalum electrolytic condenser | |
JPS56123389A (en) | Insoluble anode | |
JPS5734654A (en) | Silver oxide battery and its manufacture | |
JPS57139249A (en) | Solar heat adsorbing member | |
JPS556741A (en) | Manufacturing method of sealing plate for battery | |
JPH08115852A (en) | Method for manufacturing capacitor element in solid electrolytic capacitor |