JPS57112905A - Cold rolling method by high screw down - Google Patents
Cold rolling method by high screw downInfo
- Publication number
- JPS57112905A JPS57112905A JP18764580A JP18764580A JPS57112905A JP S57112905 A JPS57112905 A JP S57112905A JP 18764580 A JP18764580 A JP 18764580A JP 18764580 A JP18764580 A JP 18764580A JP S57112905 A JPS57112905 A JP S57112905A
- Authority
- JP
- Japan
- Prior art keywords
- rolling
- steel plate
- phosphate
- film
- cold rolling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To perform stable rolling of a high draft of ≥50% per pass in cold rolling using rolling oil or the like by forming a chemical conversion film such as phosphate beforehand on the surfaces of a steel plate.
CONSTITUTION: After a hot-rolled steel plate is pickled and descaled, it is subjected to a chemical conversion treatment quickly by a dipping method or the like to form a film of phosphate or oxalate on the surfaces of the steel plate. The coating weight of the film is 0.1W10g/m2. Rolling oil of mineral or fat type of ≤15cSt viscosity at 40°C is used by a direct system or recirculation system in the rolling. In lieu of the rolling oil, water soluble rolling fluid consisting essentially of alkylalcohol polyethylene phosphate or the like may be used. If the peripheral speed ratio of the work rolls of rolling is set at a different peripheral roll of ≤1.0/1.5, the stable cold rolling of a draft attaining ≥50% and up to 70% per pass or per stand is made possible, the surface flaws of products are eliminated and the abrasion of the rolls is minimized.
COPYRIGHT: (C)1982,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP18764580A JPS57112905A (en) | 1980-12-29 | 1980-12-29 | Cold rolling method by high screw down |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP18764580A JPS57112905A (en) | 1980-12-29 | 1980-12-29 | Cold rolling method by high screw down |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57112905A true JPS57112905A (en) | 1982-07-14 |
JPS6341646B2 JPS6341646B2 (en) | 1988-08-18 |
Family
ID=16209733
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP18764580A Granted JPS57112905A (en) | 1980-12-29 | 1980-12-29 | Cold rolling method by high screw down |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57112905A (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58202905A (en) * | 1982-05-21 | 1983-11-26 | Nippon Steel Corp | Cold rolling method |
JPS61209786A (en) * | 1985-03-14 | 1986-09-18 | Ishikawajima Harima Heavy Ind Co Ltd | Method and apparatus for rolling clad plate |
AU688222B2 (en) * | 1995-08-15 | 1998-03-05 | Sumitomo Metal Industries Ltd. | Method and roll for hot rolling a steel material |
JP2018172717A (en) * | 2017-03-31 | 2018-11-08 | Jx金属株式会社 | Plate strip and traverse coil of copper or copper alloy, and production method thereof |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5220967A (en) * | 1975-08-12 | 1977-02-17 | Nippon Shii Bii Kemikaru Kk | Composite lubrication coating for steel or alloy steel |
JPS52111843A (en) * | 1976-03-17 | 1977-09-19 | Sumitomo Metal Ind | Chemical conversion treatment for forming lubricaing coating on steel member for cold working |
-
1980
- 1980-12-29 JP JP18764580A patent/JPS57112905A/en active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5220967A (en) * | 1975-08-12 | 1977-02-17 | Nippon Shii Bii Kemikaru Kk | Composite lubrication coating for steel or alloy steel |
JPS52111843A (en) * | 1976-03-17 | 1977-09-19 | Sumitomo Metal Ind | Chemical conversion treatment for forming lubricaing coating on steel member for cold working |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58202905A (en) * | 1982-05-21 | 1983-11-26 | Nippon Steel Corp | Cold rolling method |
JPS61209786A (en) * | 1985-03-14 | 1986-09-18 | Ishikawajima Harima Heavy Ind Co Ltd | Method and apparatus for rolling clad plate |
AU688222B2 (en) * | 1995-08-15 | 1998-03-05 | Sumitomo Metal Industries Ltd. | Method and roll for hot rolling a steel material |
US5928441A (en) * | 1995-08-15 | 1999-07-27 | Sumitomo Metal Industries, Ltd. | Hot rolling method of steel products and hot rolling roll for steel products |
JP2018172717A (en) * | 2017-03-31 | 2018-11-08 | Jx金属株式会社 | Plate strip and traverse coil of copper or copper alloy, and production method thereof |
Also Published As
Publication number | Publication date |
---|---|
JPS6341646B2 (en) | 1988-08-18 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5620170A (en) | Purifying treatment of steel sheet | |
JPS57188619A (en) | Manufacturing facilities for seamless steel pipe | |
CA2006101A1 (en) | Method and apparatus for pre-processing stainless steel strip intended to be cold-rolled | |
JPS57112905A (en) | Cold rolling method by high screw down | |
JPS56127777A (en) | Descaling method for steel member | |
JPS5747519A (en) | Descaling method for hot rolled steel sheet | |
JPS5741801A (en) | Manufacture of stainless steel sheet prevented from generating gold-dust flaw | |
JPS5765796A (en) | Cold rolling method of steel sheet | |
JPS571515A (en) | Descaling method and apparatus | |
JPS5592203A (en) | Skin pass rolling method of cold rolled steel plate | |
JPS5636313A (en) | Method and apparatus for cooling rolled material in continuous hot finishing line | |
JPS55133802A (en) | Cold rolling mill | |
JPS5530363A (en) | Descaling method of hot rolled steel plate | |
JPS5542147A (en) | Cold rolled steel plate | |
JPS5519483A (en) | Production of cold rolled steel plate | |
JPS57106407A (en) | Bright rolling method | |
JPS57161036A (en) | Production of clean cold rolled steel strip | |
JPS57115901A (en) | Hot rolling method for steel material | |
JPS54160546A (en) | Manufacture of cold rolled steel plate | |
EP0628359A4 (en) | Method of manufacturing hot rolled silicon steel sheets of excellent surface properties. | |
JPS5686996A (en) | Hot rolling process using graphite lubricant | |
EP0075322A3 (en) | Method for surface treating of a roll used for s skin pass of thin sheet | |
RU1814569C (en) | Method of cleaning strip surface at cold rolling | |
JPS5736011A (en) | Cold rolling method for steel strip | |
JPS5689302A (en) | Preventing method for steel strip from heat scratch due to cold rolling work |