JPS5564371A - Manufacturing method of sintered negative plate for alkaline storage battery - Google Patents
Manufacturing method of sintered negative plate for alkaline storage batteryInfo
- Publication number
- JPS5564371A JPS5564371A JP13742078A JP13742078A JPS5564371A JP S5564371 A JPS5564371 A JP S5564371A JP 13742078 A JP13742078 A JP 13742078A JP 13742078 A JP13742078 A JP 13742078A JP S5564371 A JPS5564371 A JP S5564371A
- Authority
- JP
- Japan
- Prior art keywords
- active agent
- surface active
- instance
- solution
- manufacturing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To suppress a dissolution of nickel in a process of imprognation of the active material to provide a less dispersion of capacity, and to make the promotion of improvement of highly efficient discharge performance, by processing to immerse a sintered nickel substrate in the solution that includes a surface active agent.
CONSTITUTION: A sintered nickel substrate of porosity, for instance, 80%, after being immersed in the solution that includes a surface active agent, for instance, sodium octyl sulfate, sodium dodecyl sulfate of anion surface active agent, and decyl amin, diethanolamide, cetyltrimethylammonium chloride of cation surface active agent, is processed a drying. Subsequently, for instance, after a processing of reduced pressure impregnation by an impregnating liquid of cadmium nitrate, an operation of treating and drying while being immersed in the alkaline water solution is repeated to construct the plate.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13742078A JPS5564371A (en) | 1978-11-07 | 1978-11-07 | Manufacturing method of sintered negative plate for alkaline storage battery |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13742078A JPS5564371A (en) | 1978-11-07 | 1978-11-07 | Manufacturing method of sintered negative plate for alkaline storage battery |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5564371A true JPS5564371A (en) | 1980-05-15 |
Family
ID=15198206
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP13742078A Pending JPS5564371A (en) | 1978-11-07 | 1978-11-07 | Manufacturing method of sintered negative plate for alkaline storage battery |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5564371A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN100459271C (en) * | 2005-12-06 | 2009-02-04 | 比亚迪股份有限公司 | Method for making alkali secondary cell |
-
1978
- 1978-11-07 JP JP13742078A patent/JPS5564371A/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN100459271C (en) * | 2005-12-06 | 2009-02-04 | 比亚迪股份有限公司 | Method for making alkali secondary cell |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB1505979A (en) | Manufacture of primary alkaline cells | |
JPS5564371A (en) | Manufacturing method of sintered negative plate for alkaline storage battery | |
US2931846A (en) | Electric battery plate | |
JPS5564372A (en) | Manufacturing method of sintered negative plate for alkaline storage battery | |
JPS5564374A (en) | Manufacturing method of sintered plate for alkaline storage battery | |
JPS532381A (en) | Making harmless method for incinerated ash containing heavy metals | |
JPS5576570A (en) | Manufacturing method for alkali battery plate | |
JPS5636863A (en) | Lead storage battery | |
JPS55109371A (en) | Method of producing cadmium negative electrode for alkaline battery | |
JPS5525913A (en) | Packing method of paste for storage battery base plate | |
JPS64648A (en) | Manufacture of sintered electrode for alkaline storage battery | |
JPS5560271A (en) | Manufacturing method of plate for nickel cadmium storage battery | |
JPS5564373A (en) | Manufacturing method of sintered negative plate for alkaline storage battery | |
JPS5550626A (en) | Surface treatment of thin plate | |
JPS5487695A (en) | Preparation of two valency silver oxide | |
JPS56126257A (en) | Method of preparing silver (2) oxide battery | |
JPS5560272A (en) | Manufacturing method of sintered substrate for alkaline storage battery | |
JPS5663774A (en) | Manufacture of plate for alkaline storage battery | |
JPS54130672A (en) | Vacuum impregnation of varnish | |
JPS5622048A (en) | Manufacturing process of pasted plate for lead battery | |
JPS57170458A (en) | Manufacture of cadmium negative electrode for battery | |
JPS5894759A (en) | Manufacture of storage battery | |
JPS5335676A (en) | Rapid treating method for dust | |
JPS5328072A (en) | Treating method for liquid | |
JPS54142182A (en) | Oxidizing agent production |