JPS55148799A - Electrolytic chromic-acid-treated steel sheet having low deterioration on standing of adhesive strength and its manufacture - Google Patents
Electrolytic chromic-acid-treated steel sheet having low deterioration on standing of adhesive strength and its manufactureInfo
- Publication number
- JPS55148799A JPS55148799A JP5403679A JP5403679A JPS55148799A JP S55148799 A JPS55148799 A JP S55148799A JP 5403679 A JP5403679 A JP 5403679A JP 5403679 A JP5403679 A JP 5403679A JP S55148799 A JPS55148799 A JP S55148799A
- Authority
- JP
- Japan
- Prior art keywords
- chromate coating
- steel sheet
- standing
- acid
- adhesive strength
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: The above mentioned steel sheet having the minimum deterioration on standing of adhesive strength at the time of using for adhesion can, made by specifying the atomic ratio of S/O in chromate coating and oxo forming degree of outermost surface of chromate coating.
CONSTITUTION: Amount of chromate coating is adjusted so as 5W50mg/m2 of it calculated in terms of Cr to remain, after metallic Cr and chromate coating, are electrodeposited on the steel sheet. Next, cathode electrolytic treatment is carried out at 50°C or more, especially 60°C or more, in the aqueous solution in which 204 2-/Cr6+ is smaller than 1/75, in case of using the chromate coating as it is or washing in water again. That is, oxo forming degree of the chromate coating is improve by liquating anion, especially SO4 2-, contained in the chromate coating and also, liquating Cr6+. Then, the above mentioned electrolytic chromic-acid-treated steel sheet is obtained by treating the chromate coating after carrying out the above cathode treatment moreover at 65W 100°C for 0.3W10sec by a high temperature water having pH of 4 or more. S/O (atomic ratio) in the chromate coating layer of the steel sheet, is 0.2 or less and also, the oxo forming degree in the chromate coating is 0.90 or more.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP54054036A JPS5927399B2 (en) | 1979-05-04 | 1979-05-04 | Method for manufacturing electrolytic chromic acid treated steel sheet with minimal deterioration of adhesive strength over time |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP54054036A JPS5927399B2 (en) | 1979-05-04 | 1979-05-04 | Method for manufacturing electrolytic chromic acid treated steel sheet with minimal deterioration of adhesive strength over time |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS55148799A true JPS55148799A (en) | 1980-11-19 |
JPS5927399B2 JPS5927399B2 (en) | 1984-07-05 |
Family
ID=12959354
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP54054036A Expired JPS5927399B2 (en) | 1979-05-04 | 1979-05-04 | Method for manufacturing electrolytic chromic acid treated steel sheet with minimal deterioration of adhesive strength over time |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5927399B2 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN113864833A (en) * | 2014-02-28 | 2021-12-31 | Seb公司 | Communication induction cooking table and searching and monitoring method of communication cooking equipment on table |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61146669U (en) * | 1985-03-04 | 1986-09-10 |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5235618A (en) * | 1975-09-16 | 1977-03-18 | Yogo Ito | Method and device for tuning five-holed bamboo |
-
1979
- 1979-05-04 JP JP54054036A patent/JPS5927399B2/en not_active Expired
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5235618A (en) * | 1975-09-16 | 1977-03-18 | Yogo Ito | Method and device for tuning five-holed bamboo |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN113864833A (en) * | 2014-02-28 | 2021-12-31 | Seb公司 | Communication induction cooking table and searching and monitoring method of communication cooking equipment on table |
CN113864833B (en) * | 2014-02-28 | 2024-02-27 | Seb公司 | Communication induction cooking station and method for searching and monitoring communication cooking devices on said station |
Also Published As
Publication number | Publication date |
---|---|
JPS5927399B2 (en) | 1984-07-05 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5698480A (en) | Rust preventive treatment of galvanized steel material | |
JPS55145180A (en) | Phosphate-treating method of metal surface for cationic electrocoating | |
JPS5770291A (en) | Highly corrosion resistant surface treated steel and preparation thereof | |
JPS569386A (en) | Production of electro-zinc plated steel plate | |
JPS55148799A (en) | Electrolytic chromic-acid-treated steel sheet having low deterioration on standing of adhesive strength and its manufacture | |
JPS5489946A (en) | Manufacture of steel sheet with little deterioration in bonding strength on standing treated with chromic acid by electrolysis | |
JPS57185997A (en) | After-treatment of very thinly tinned steel plate | |
JPS57177998A (en) | Production of tin-free steel plate | |
ES419556A2 (en) | Method of increasing the hardness of a film formed on the surface of an alloy. (Machine-translation by Google Translate, not legally binding) | |
JPS55107798A (en) | Preparation of electrolytic chromate treated steel sheet | |
JPS57192295A (en) | Surface treated steel sheet of excellent painting property | |
JPS5495941A (en) | After-treating method for steel sheet with superior corrosion resistance and coating adherence treated with chromic acid by electrolysis | |
JPS5669377A (en) | Surface treatment method of zinc | |
JPS5616697A (en) | Preparation of chromic acid treaded steel sheet having low deterioration on standing of adhesive strength | |
JPS57114695A (en) | Production of zinc plated steeel plate of superior blackening resistance and intergranular corrosion resistance | |
JPS5534643A (en) | Manufacture of very thin steel sheet coated with iron- tin alloy | |
JPS5629680A (en) | Surface treatment in annealing line | |
JPS5521533A (en) | Producing method of cold rolled steel plate with superior intermediate rustproofness | |
JPS57192293A (en) | Manufacture of surface treated steel sheet of excellent paint adherence | |
JPS5562198A (en) | Chromium-chromate steel plate of high adhesiveness | |
JPS5616698A (en) | Preparation of electrolytic chromate treated steel sheet having superior wet adhesive property | |
JPS5579891A (en) | Preparation of tin plated steel sheet | |
JPS5735698A (en) | Production of chromate film steel plate for vessel of superior weldability and corrosion resistance after painting | |
JPS55115992A (en) | Production of tin-free steel | |
JPS55145194A (en) | Manufacture of material for vessel |