JPS5514866A - Heat treating method for joining steel sheet of soft steel and thermal refining high tensile steel - Google Patents
Heat treating method for joining steel sheet of soft steel and thermal refining high tensile steelInfo
- Publication number
- JPS5514866A JPS5514866A JP8749578A JP8749578A JPS5514866A JP S5514866 A JPS5514866 A JP S5514866A JP 8749578 A JP8749578 A JP 8749578A JP 8749578 A JP8749578 A JP 8749578A JP S5514866 A JPS5514866 A JP S5514866A
- Authority
- JP
- Japan
- Prior art keywords
- steel
- high tensile
- thermal refining
- refining high
- soft
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To prevent the production of strain at hardening time, by cooling rapidly after heating at the temperature between Ac3 point of soft iron and Ac3 point of thermal refining high tensile steel, at the time of hardening joining steel sheet of soft steel and thermal refining high tensile steel. CONSTITUTION:Clad steel sheet is formed by soft steel contining 0.05% of C and thermal refining high tensile steel containing 0.12% of C and the above formed sheet is hardened. On this occasion, the above sheet is heated at the middle temperature of 897 deg.C of Ac3 transformation point of soft iron and 837 deg.C of Ac3 transformation point of thermal refining high tensile steel and is tempered at 620 deg.C after carrying out water hardening. By the above method, deformation on the basis of transformation expansion at the time of transforming from austenite to ferrite, is prevented.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8749578A JPS5514866A (en) | 1978-07-17 | 1978-07-17 | Heat treating method for joining steel sheet of soft steel and thermal refining high tensile steel |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8749578A JPS5514866A (en) | 1978-07-17 | 1978-07-17 | Heat treating method for joining steel sheet of soft steel and thermal refining high tensile steel |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5514866A true JPS5514866A (en) | 1980-02-01 |
Family
ID=13916536
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP8749578A Pending JPS5514866A (en) | 1978-07-17 | 1978-07-17 | Heat treating method for joining steel sheet of soft steel and thermal refining high tensile steel |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5514866A (en) |
-
1978
- 1978-07-17 JP JP8749578A patent/JPS5514866A/en active Pending
Similar Documents
Publication | Publication Date | Title |
---|---|---|
SE9903880L (en) | Method for heat treatment of structural parts of steel or cast iron | |
JPS5576020A (en) | Production of steel plate stable in strength and toughness by direct hardening and tempering | |
BR8902345A (en) | PROCESS FOR THERMAL TREATMENT OF CORROSION RESISTANT STEEL BODIES | |
JPS5723026A (en) | Spheroidization treatment for bar steel material | |
JPS5514866A (en) | Heat treating method for joining steel sheet of soft steel and thermal refining high tensile steel | |
JPS5514833A (en) | Heat-treating method | |
JPS5741322A (en) | Spheroidizing method for carbide in steel | |
ES8207226A1 (en) | Method for producing high-strength deep-drawable dual-phase steel sheets. | |
FR2300810A1 (en) | Device for patenting steel wire - which partially quenches it followed by temp. homogenisation and isothermal transformation | |
JPS55134126A (en) | Production of high-strength cold rolled steel plate of superior press formability | |
JPS56102519A (en) | Cold rolling method for stainless steel of high strength | |
SU749914A1 (en) | Method of thermal treatment of high-streength corrosion-resistant martensite steels | |
SU1749256A1 (en) | Method of thermally treating cold-deformed workpieces | |
JPS56150127A (en) | Direct normalizing method | |
SU726191A1 (en) | Method of thermal processing of bimetallic rods | |
JPS5719327A (en) | Heat treatment device for link chain | |
JPS5635722A (en) | Production of thick-walled high tensile large-diameter steel pipe | |
GB782356A (en) | Improvements in or relating to the manufacture of steel bars | |
SU789606A1 (en) | Method of thermal treatment of chrome-nickel austenite-martensite steels | |
JPS5589420A (en) | Linear heating method of tempered high tensile steel | |
JPS5658926A (en) | Production of hot-rolled steel plate of superior ductility | |
JPS5585624A (en) | Continuous over-aging method for continuously hot-zinc dipped steel sheet | |
SU378419A1 (en) | METHOD FOR TREATING CARBON AND ALLOYED STEELS | |
JPS5485116A (en) | Heat treating method for large-sized steel pipe | |
JPS57114610A (en) | Hardening and tempering method for steel material |