JPS5492513A - Metal mold for centrifugal casting of cast iron pipe - Google Patents

Metal mold for centrifugal casting of cast iron pipe

Info

Publication number
JPS5492513A
JPS5492513A JP16064977A JP16064977A JPS5492513A JP S5492513 A JPS5492513 A JP S5492513A JP 16064977 A JP16064977 A JP 16064977A JP 16064977 A JP16064977 A JP 16064977A JP S5492513 A JPS5492513 A JP S5492513A
Authority
JP
Japan
Prior art keywords
cast iron
centrifugal casting
mold
metal mold
occurrence
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP16064977A
Other languages
Japanese (ja)
Other versions
JPS5631866B2 (en
Inventor
Toshiaki Morichika
Yoshiro Murase
Akio Tanaka
Yoshinobu Ohashi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kubota Corp
Original Assignee
Kubota Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kubota Corp filed Critical Kubota Corp
Priority to JP16064977A priority Critical patent/JPS5492513A/en
Publication of JPS5492513A publication Critical patent/JPS5492513A/en
Publication of JPS5631866B2 publication Critical patent/JPS5631866B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE: To prevent occurrence of brittle rupture in a metal mold for centrifugal casting of cast iron pipes due to occurrence of heat cracks by making the mold of cast steel of a specific compsn. followed by hardening and tempering.
CONSTITUTION: A metal mold for centrifugal casting of cast iron pipes is made of steel contg. C; 0.05W0.22%, Si; 0.2W0.8%, Mn; 0.5W1.5%, P<0.04%, S< 0.03%, Ni 0.5W1.5% and V; 0.03W0.12%, By hardening and tempering the mold, occurrence of shattered cracks due to repeated thermal impacts is prevented. Accordingly, occurrence of brittle rupture due to propagation of the cracks is also prevented, and hence the endurance life of the mold is elongated.
COPYRIGHT: (C)1979,JPO&Japio
JP16064977A 1977-12-29 1977-12-29 Metal mold for centrifugal casting of cast iron pipe Granted JPS5492513A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP16064977A JPS5492513A (en) 1977-12-29 1977-12-29 Metal mold for centrifugal casting of cast iron pipe

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP16064977A JPS5492513A (en) 1977-12-29 1977-12-29 Metal mold for centrifugal casting of cast iron pipe

Publications (2)

Publication Number Publication Date
JPS5492513A true JPS5492513A (en) 1979-07-21
JPS5631866B2 JPS5631866B2 (en) 1981-07-24

Family

ID=15719489

Family Applications (1)

Application Number Title Priority Date Filing Date
JP16064977A Granted JPS5492513A (en) 1977-12-29 1977-12-29 Metal mold for centrifugal casting of cast iron pipe

Country Status (1)

Country Link
JP (1) JPS5492513A (en)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR102576735B1 (en) * 2018-12-18 2023-09-07 주식회사 엘지화학 Method of preparation for super absorbent polymer
KR102567563B1 (en) * 2018-12-03 2023-08-14 주식회사 엘지화학 Method of preparation for super absorbent polymer
KR102566284B1 (en) * 2018-11-14 2023-08-10 주식회사 엘지화학 Method of preparation for super absorbent polymer

Also Published As

Publication number Publication date
JPS5631866B2 (en) 1981-07-24

Similar Documents

Publication Publication Date Title
JPS5492513A (en) Metal mold for centrifugal casting of cast iron pipe
JPS5492512A (en) Metal mold for centrifugal casting of cast iron pipe
JPS5496418A (en) Heat resistant cast steel
JPS54110119A (en) Manufacture of line pipe steel with superior hydrogen induced cracking resistance
JPS56163244A (en) Heat resistant austenite steel with superior hot workability and oxidation resistance
JPS5550451A (en) Aluminum alloy for high strength die cast
JPS52144306A (en) Water cooled skid for heating furnace
JPS54120220A (en) Cast iron inoculating method and inoculant
JPS5585655A (en) Steel for plastic molding metal mold
JPS5741350A (en) Alloy with high strength, high ductility and low thermal expansibility and its manufacture
JPS5739128A (en) Preparation of heat resistant cutter bit for dental die
JPS5413414A (en) Medium cr low ni stainless cast steel of high corrosion resistance and high strength
JPS5573480A (en) Sheet iron shell crack propagation preventive method
JPS5465116A (en) Wear resistant cast iron
JPS53146213A (en) Improving method for graphite structure of cast iron
JPS5433204A (en) Cooling plate forming inner wall of high temperature furnace such as arc furnace, etc.
JPS558414A (en) Damping alloy
JPS54118323A (en) Heat crack resistant steel for use as metal mold
JPS5723051A (en) Cavitation and erosion resistant martensite type stainless cast steel
JPS5792162A (en) Thick cast steel for low temperature use
JPS5268019A (en) Roller conveying steel plate
JPS566758A (en) Steel for mold and its production
JPS53119254A (en) Repairing method for nodular graphite cast steel roll
JPS54103721A (en) Inoculation method in core casting for compound roll
JPS5651552A (en) Cast steel for low temperature member