JPS54139846A - Composite welding method for thick steel materials - Google Patents

Composite welding method for thick steel materials

Info

Publication number
JPS54139846A
JPS54139846A JP4851778A JP4851778A JPS54139846A JP S54139846 A JPS54139846 A JP S54139846A JP 4851778 A JP4851778 A JP 4851778A JP 4851778 A JP4851778 A JP 4851778A JP S54139846 A JPS54139846 A JP S54139846A
Authority
JP
Japan
Prior art keywords
welding
thick steel
face
energy density
high energy
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP4851778A
Other languages
Japanese (ja)
Inventor
Hiroshi Yada
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP4851778A priority Critical patent/JPS54139846A/en
Publication of JPS54139846A publication Critical patent/JPS54139846A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To eliminate complicated after-treatment by usual method and to obtain good weld zone, by applying high energy density welding and arc welding on the groove having 10W30mm of root face at the same time and softening in a specific extent, on occasion of carrying out composite welding of thick steel materials.
CONSTITUTION: At the time of carrying out seam welding of butt part carried out UO press processing, using steel material having more than 40Kg of hardness, hardening by high energy density welding, the groove shape is made (A)W(F) and for example, on occasion of the shape (D), the depth root face x is made 10W30 mm (a fixed softening is difficult at more than 30mm and merit of this invention is not exhibited at less than 10mm) and groove depth y1, y2 is made about 30mm. At first, the high energy density welding is carried out against x face and next, arc welding is carried out against y1, y2 faces by annexed list condition and then, weld zone of the above hardened x face is softened at Hv≤300. Thus, complicated after-treatment by usual method is made unnecessary and good weld zone suitable for high pressure thick steel tube, is obtained.
COPYRIGHT: (C)1979,JPO&Japio
JP4851778A 1978-04-24 1978-04-24 Composite welding method for thick steel materials Pending JPS54139846A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP4851778A JPS54139846A (en) 1978-04-24 1978-04-24 Composite welding method for thick steel materials

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP4851778A JPS54139846A (en) 1978-04-24 1978-04-24 Composite welding method for thick steel materials

Publications (1)

Publication Number Publication Date
JPS54139846A true JPS54139846A (en) 1979-10-30

Family

ID=12805549

Family Applications (1)

Application Number Title Priority Date Filing Date
JP4851778A Pending JPS54139846A (en) 1978-04-24 1978-04-24 Composite welding method for thick steel materials

Country Status (1)

Country Link
JP (1) JPS54139846A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4560855A (en) * 1982-09-08 1985-12-24 Nippon Steel Corporation Method for joining of articles by energy beam and apparatus for controlling said method
CN104858555A (en) * 2015-06-10 2015-08-26 江苏力沛电力工程技术服务有限公司 Pressure pipeline welding process

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4560855A (en) * 1982-09-08 1985-12-24 Nippon Steel Corporation Method for joining of articles by energy beam and apparatus for controlling said method
CN104858555A (en) * 2015-06-10 2015-08-26 江苏力沛电力工程技术服务有限公司 Pressure pipeline welding process

Similar Documents

Publication Publication Date Title
JPS56114590A (en) Joining method of material
JPS54139846A (en) Composite welding method for thick steel materials
JPS53130241A (en) Welding method for manufacture of thick walled steel pipe
JPS53130242A (en) Welding method for manufacture of thick-walled large diameter welded steel pipe
JPS53104531A (en) Surface processing method decreasing stress corrosion cracking
JPS571572A (en) Arc welding method of thick steel plate
JPS53106352A (en) Forming method for reverse strain in welding steel plate
JPS53120647A (en) Welding method for electron beam of high carbon steel material
JPS5431068A (en) Continuous hot rolling method for steel material
JPS5650797A (en) Increasing method for weld-part fatigue strength of high-tension steel
JPS54159355A (en) Electron beam welding method
JPS57168791A (en) Production of clad steel stock
JPS578028A (en) Manufacturing of saw blade
JPS5415455A (en) Method of producing drum having guide groove
JPS5797889A (en) Welding method for plate material
JPS5717377A (en) Method for build-up welding of surface
JPS5413433A (en) Welding method for stainless steel
JPS5536091A (en) Seaming method of billet and pipe sleeve
JPS53140245A (en) Improving method for fatiuge strength of fillet welded joint
JPS56156634A (en) Manufacture of magnetron anode
JPS53119241A (en) Welding method for slightly weldable materials and dehydrogenation apparatus welding
JPS57134289A (en) Metallic parts for laser beam welding
JPS5423047A (en) Welding method
JPS53125954A (en) Method of producing thick pipes
JPS5736080A (en) Electron beam welding method