JPS5365212A - Ingot case additive for continuous casting of steel - Google Patents

Ingot case additive for continuous casting of steel

Info

Publication number
JPS5365212A
JPS5365212A JP14022776A JP14022776A JPS5365212A JP S5365212 A JPS5365212 A JP S5365212A JP 14022776 A JP14022776 A JP 14022776A JP 14022776 A JP14022776 A JP 14022776A JP S5365212 A JPS5365212 A JP S5365212A
Authority
JP
Japan
Prior art keywords
steel
continuous casting
ingot case
additive
case additive
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP14022776A
Other languages
Japanese (ja)
Inventor
Moriyuki Ishiguro
Mikio Suzuki
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Engineering Corp
Original Assignee
NKK Corp
Nippon Kokan Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NKK Corp, Nippon Kokan Ltd filed Critical NKK Corp
Priority to JP14022776A priority Critical patent/JPS5365212A/en
Publication of JPS5365212A publication Critical patent/JPS5365212A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To provide the title additive which can prevent solidification of the surface of molten steel, form a slag film, and give a good ingot by blending slag of a specified compsn. contg. CaO, SiO2, MgO and Al2O3 with regulators for m.p., viscosity and melting speed.
COPYRIGHT: (C)1978,JPO&Japio
JP14022776A 1976-11-24 1976-11-24 Ingot case additive for continuous casting of steel Pending JPS5365212A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP14022776A JPS5365212A (en) 1976-11-24 1976-11-24 Ingot case additive for continuous casting of steel

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP14022776A JPS5365212A (en) 1976-11-24 1976-11-24 Ingot case additive for continuous casting of steel

Publications (1)

Publication Number Publication Date
JPS5365212A true JPS5365212A (en) 1978-06-10

Family

ID=15263853

Family Applications (1)

Application Number Title Priority Date Filing Date
JP14022776A Pending JPS5365212A (en) 1976-11-24 1976-11-24 Ingot case additive for continuous casting of steel

Country Status (1)

Country Link
JP (1) JPS5365212A (en)

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5927759A (en) * 1982-08-10 1984-02-14 Nippon Steel Metal Prod Co Ltd Mold additive for continuous casting of steel
JPS59209465A (en) * 1983-05-12 1984-11-28 Nippon Steel Corp Protective agent for molten metal surface for continuous casting of steel having less surface defect
JPS60141355A (en) * 1983-12-29 1985-07-26 Nippon Steel Corp Protective agent for molten metal surface for continuous casting
CN103170591A (en) * 2013-03-05 2013-06-26 新疆八一钢铁股份有限公司 Production technology for steel ladle and molten steel covering agent
CN103443298A (en) * 2011-03-31 2013-12-11 新日铁住金株式会社 Environmentally friendly flux for desulfurization of molten steel
CN108284207A (en) * 2017-06-27 2018-07-17 胡毅婧 A kind of special Power Plant Ash of austenite antimicrobial stainless steel crystallizer protecting residue
CN111604484A (en) * 2020-04-23 2020-09-01 华北理工大学 Super high drawing speed thin slab continuous casting covering slag for low carbon steel

Cited By (10)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5927759A (en) * 1982-08-10 1984-02-14 Nippon Steel Metal Prod Co Ltd Mold additive for continuous casting of steel
JPH0211346B2 (en) * 1982-08-10 1990-03-13 Nippon Steel Metal Prod
JPS59209465A (en) * 1983-05-12 1984-11-28 Nippon Steel Corp Protective agent for molten metal surface for continuous casting of steel having less surface defect
JPS60141355A (en) * 1983-12-29 1985-07-26 Nippon Steel Corp Protective agent for molten metal surface for continuous casting
CN103443298A (en) * 2011-03-31 2013-12-11 新日铁住金株式会社 Environmentally friendly flux for desulfurization of molten steel
US9127327B2 (en) 2011-03-31 2015-09-08 Nippon Steel & Sumitomo Metal Corporation Environmentally friendly flux for molten steel desulfurization
CN103170591A (en) * 2013-03-05 2013-06-26 新疆八一钢铁股份有限公司 Production technology for steel ladle and molten steel covering agent
CN103170591B (en) * 2013-03-05 2015-08-26 新疆八一钢铁股份有限公司 A kind of production technology of ladle molten steel coverture
CN108284207A (en) * 2017-06-27 2018-07-17 胡毅婧 A kind of special Power Plant Ash of austenite antimicrobial stainless steel crystallizer protecting residue
CN111604484A (en) * 2020-04-23 2020-09-01 华北理工大学 Super high drawing speed thin slab continuous casting covering slag for low carbon steel

Similar Documents

Publication Publication Date Title
JPS5714496A (en) Molten type flux for submerged arc welding
JPS5365212A (en) Ingot case additive for continuous casting of steel
GB1271022A (en) Improved process for the continuous casting of steel
KR870011257A (en) Steelmaking flux
ES440730A1 (en) Process of ingot casting
JPS54104415A (en) Slag cut material for discharge of steel
GB1449234A (en) Controlled flux addition fo minimizing surface defects on continuously cast steel
JPS5325210A (en) Steel refining method
JPS5531148A (en) Manufacture of clean cast steel product
JPS5554520A (en) Continuous-casting method for oriented electrical steel
JPS5589412A (en) Preventing method of collapse of converter slag and electric furnace slag
JPS5536042A (en) Casting method for low-carbon ferrochrome ingot
JPS5326204A (en) Method for prevention of solidification of melt at taphole of cupola furnace
AU507154B2 (en) Continuous casting by atomising molten metal
JPS53142305A (en) Preventing method for burning-out of refractories in ladle
GB1504280A (en) Methods of reducing inclusions in castings
JPS57130754A (en) Formation of special chill of gray cast iron
SU442889A1 (en) Slag-forming material
JPS53114716A (en) Improving method for properties of nodular graphite cast iron tube
JPS5719142A (en) Manufacture of continuous ingot superior in surface characteristic
SE7712586L (en) PROCEDURES AND DEVICES FOR THE MANUFACTURE OF BLOCKS
JPS55128526A (en) Casting mold additive for continuously casting steel
JPS52149204A (en) Vibration casting of refractory material in vessel of molten metal
JPS53133543A (en) Flux for submerged arc welding
JPS5458613A (en) Steel refining flux